Propriedades do limestone como rocha ornamental: terminologia, caracterização e manutenção

Submitted by Rafael Santana (rafael.silvasantana@ufpe.br) on 2018-02-08T18:35:51Z
No. of bitstreams: 2
license_rdf: 811 bytes, checksum: e39d27027a6cc9cb039ad269a5db8e34 (MD5)
DISSERTAÇÃO LARISSA LAPA_FINAL (1).pdf: 9096993 bytes, checksum: 1e3d7aa07e5a6f6af273fbe4e4f8364b (MD5) / Made available in DSpace on 2018-02-08T18:35:51Z (GMT). No. of bitstreams: 2
license_rdf: 811 bytes, checksum: e39d27027a6cc9cb039ad269a5db8e34 (MD5)
DISSERTAÇÃO LARISSA LAPA_FINAL (1).pdf: 9096993 bytes, checksum: 1e3d7aa07e5a6f6af273fbe4e4f8364b (MD5)
Previous issue date: 2016-11-25 / CAPES / O trabalho analisa as propriedades tecnológicas de dois tipos de limestone,
conhecidos comercialmente como Crema Paraná e Crema Brasil, e esclarece dúvidas
quanto à gênese do material, visando contribuir para a especificação desse tipo de
rocha ornamental na Arquitetura. Por se tratar de um material recentemente inserido
no mercado, pouco se sabe sobre o comportamento do limestone, fato que poderá
comprometer o seu desempenho e o aspecto estético das obras nas quais estiver
empregado. O limestone é uma rocha calcária sedimentar de origem aloquímica, com
granulometria fina, composta basicamente por calcita (CaCO3), e que chama a
atenção dos arquitetos, devido, principalmente, à sua coloração clara, e textura fina e
homogênea. O trabalho abrange, portanto, a caracterização química, física e
mecânica dos dois tipos de limestone, a partir das normas vigentes e de ensaios de
alteração acelerada. A composição química e mineralógica foi obtida através da
petrografia e difração de raio x. Os índices físicos analisados foram a densidade,
porosidade aparente e absorção de água. Os ensaios de comportamento mecânico
determinaram as resistências à compressão, à flexão em 4 pontos, ao impacto de
corpo duro e ao desgaste. Os valores obtidos dos índices físicos do Crema Paraná
(3,87% de absorção de água) se adequam àqueles recomendados pela ASTM C568,
indicando baixa capacidade de absorção de líquidos. Já o Crema Brasil apresentou
um percentual de 3,59%, pouco maior do que os parâmetros estabelecidos. Quanto à
resistência à compressão, ambos apresentaram resultados satisfatórios. No teste de
resistência à flexão, apesar da referida norma estabelecer valores apenas para a
flexão em 3 pontos, as rochas analisadas apresentaram o resultado de 9,30MPa
(Crema Paraná) e 7,20MPa (Crema Brasil), na condição saturada - a qual ressalta-se
ser mais desfavorável no que diz respeito à resistência, conferindo valor maior que
aquele recomendado pela ASTM. Quanto à resistência à abrasão, após o percurso de
500m, observou-se a perda total do polimento de ambas as rochas. Trata-se, pois, de
um material de baixa dureza e alta densidade, possuindo aplicações restritas e
devendo ser evitado principalmente em áreas de alto tráfego de pessoas e ambientes
molhados, devido à composição mineralógica de natureza carbonática e textura fina. / This paper analyzes the technological properties of two types of limestone,
commercially known as Crema Paraná and Crema Brasil, and clarifies doubts about
the genesis of the material, to contribute to the specification of this type of dimension
stone in architecture. As a newly entered the market material, little is known about the
behavior of limestone, a fact that may compromise its performance and the aesthetic
aspect of the building in which will be employed. The Limestone is a sedimentary rock
with na allochemic origin, with fine grain and composed mainly of calcite (CaCO3),
which draws the attention of architects, mainly due to its light color and fine and
homogeneous texture. The work thus covers the chemical, physical and mechanical
properties of two types of limestone, from the current regulations, and chemical change
tests. The chemical and mineralogical composition was obtained by petrographic and
x-ray diffraction. The physical indexes analyzed were the density, porosity and water
absorption. The mechanical tests determined the compressive strength and flexural
strength in 4-point, the hard body impact and abrasion. The values of Crema Parana’s
physical indexes (3.87% water absorption) fit those recommended by ASTM C568,
indicating low fluid absorption capacity. Already Crema Brazil presented a percentage
of 3.59%, slightly higher than the established parameters. In regard to compressive
strength both showed satisfactory results. In flexural strength test, in spite of this
standard to establish values only for flexion in 3 points, the rocks analyzed showed the
result of 9,30MPa (Crema Paraná) and 7,20MPa (Crema Brasil) in saturated condition
- which points to be more favorable as regards resistance, giving more value than that
recommended by ASTM. The abrasion resistance after 500m path, presented total loss
of polishing of the both rocks. It is, therefore, a low hardness and high density material,
having restricted applications and should be avoided especially in areas of high foot
traffic and wet environments due to the mineralogical composition of carbonate nature
and fine texture.

Identiferoai:union.ndltd.org:IBICT/oai:repositorio.ufpe.br:123456789/23625
Date25 November 2016
CreatorsBARBOSA, Larissa Lapa Teles
Contributorshttp://lattes.cnpq.br/0610391409027776, OLIVEIRA, Felisbela Maria da Costa, NEVES, Risale
PublisherUniversidade Federal de Pernambuco, Programa de Pos Graduacao em Engenharia Mineral, UFPE, Brasil
Source SetsIBICT Brazilian ETDs
LanguagePortuguese
Detected LanguagePortuguese
Typeinfo:eu-repo/semantics/publishedVersion, info:eu-repo/semantics/masterThesis
Sourcereponame:Repositório Institucional da UFPE, instname:Universidade Federal de Pernambuco, instacron:UFPE
RightsAttribution-NonCommercial-NoDerivs 3.0 Brazil, http://creativecommons.org/licenses/by-nc-nd/3.0/br/, info:eu-repo/semantics/openAccess

Page generated in 0.0025 seconds