This thesis, which comprises of a theoretical and a practical part, deals with possible means of increasing ceramic body frost resistance. The current state of research in the field of ceramic body frost resistance is summarized in the theoretical part. The practical part is divided into two sections. In the first section, the influence of firing temperature (820 °C and 1020 °C) and duration (2, 4 and 6 hours) on frost resistance and several other parameters is assessed by means of experiment, using a specimen of brick body made of mixes currently used in roof tile production by TONDACH Šlapanice and TONDACH Dolní Jirčany factories. In the second section of the practical part, two modifications are introduced of the mixture currently used in roof tile production in the TONDACH Šlapanice factory – GE clay and zeolite supplements were added, the effects of which are verified by means of experiment using specimens fired in a kiln designated for ceramic masonry blocks and alternatively in a kiln used for firing TONDACH Šlapanice roof tiles.
Identifer | oai:union.ndltd.org:nusl.cz/oai:invenio.nusl.cz:226720 |
Date | January 2014 |
Creators | Keršner, Štěpán |
Contributors | Šveda,, Mikuláš, Sokolář, Radomír |
Publisher | Vysoké učení technické v Brně. Fakulta stavební |
Source Sets | Czech ETDs |
Language | Czech |
Detected Language | English |
Type | info:eu-repo/semantics/masterThesis |
Rights | info:eu-repo/semantics/restrictedAccess |
Page generated in 0.002 seconds