Polyacid modified composite resins (PMCR) are designed to combine the aesthetics of composites-resins with the fluoride release of glass-ionomers. Objectives: to compare the relative biostability and fluoride release of PMCR (F2000 [3M]; Dyract eXtra [DENTSPLY]) and a composite-resin (Z250 [3M]). Standardized samples were incubated in either buffer or human saliva derived esterases (HSDE) for up to 14 days. High- performance-liquid-chromatography revealed higher amounts of degradation products for all HSDE incubated groups, as compared with the buffer. Z250 samples released higher amounts of bishydroxypropoxyphenylpropane (Bis-HPPP) and triethylene-glycol-dimethacrylate (TEGDMA) than both PMCR. Dyract eXtra and F2000 samples released unique degradation products, respectively di-ester of 2-hydroxyethyl di-methacrylate with butane tetracarboxylic acid (TCB) and glyceryl dimethacrylate (GDMA). F2000 samples released more fluoride for both incubation periods in the presence of HSDE as compared with Dyract eXtra samples. Scanning electron microscopy analysis confirmed the greater degradation of both PMCR, as compared with Z250.
Identifer | oai:union.ndltd.org:LACETR/oai:collectionscanada.gc.ca:OTU.1807/18268 |
Date | 13 January 2010 |
Creators | Daniel, Iris |
Contributors | Finer, Yoav |
Source Sets | Library and Archives Canada ETDs Repository / Centre d'archives des thèses électroniques de Bibliothèque et Archives Canada |
Language | en_ca |
Detected Language | English |
Type | Thesis |
Page generated in 0.002 seconds