Lap splice in glass fiber reinforced polymer‐reinforced concrete rectangular columns subjected to cyclic‐reversed loads

This study presents the experimental results of nine full-scale lap spliced glass-fiber reinforced polymer (GFRP) reinforced concrete (RC) columns, and one additional reference steel-RC column with lap splices, under axial and cyclic-reversed loads. The test parameters included type of reinforcement, lap splice length of longitudinal reinforcement, transverse reinforcement spacing, and the effect of using steel fiber-reinforced concrete (SFRC). Test results indicated that a splice length of 60 times the diameter of the longitudinal column bar was adequate in transferring the full bond forces along the splice length and were able to maintain the lateral load carrying capacity when subjected to higher levels of axial loads and drift ratios. In addition, lap spliced GFRP-RC columns with closely spaced transverse reinforcement achieved high levels of deformability. Furthermore, the use of SFRC in columns with inadequate splice increased the peak lateral strength and the energy dissipation of the specimens. / February 2017

Identiferoai:union.ndltd.org:MANITOBA/oai:mspace.lib.umanitoba.ca:1993/31906
Date27 October 2016
CreatorsNaqvi, Syed
ContributorsEl-Salakawy, Ehab (Civil Engineering), Wu, Nan (Mechanical Engineering) Cha, Young-Jin (Civil Engineering)
Source SetsUniversity of Manitoba Canada
Detected LanguageEnglish

Page generated in 0.0014 seconds