  1. Influence of Cleaning Methods on Resin Bonding to Contaminated Translucent 3Y-TZP ceramic

    … resin bond strength to contaminated translucent 3Y-TZP ceramic. Materials and Methods: A total of 133 airborne-particle abraded zirconia specimens (0.1 MPa) were divided into 7 groups. Uncontaminated zirconia specimens were either not cleaned (UN) or cleaned with cleaning paste (Ivoclean) (UP1). …

    cau-kiel Repository record for Influence of Cleaning Methods on Resin Bonding to Contaminated Translucent 3Y-TZP ceramic (opens in a new tab)

  2. Development and CAD/CAM production of ultra-thin, high translucent 3Y-TZP zirconia veneers

    … tetragonal estabilizada com 3 mol% de ítria (3Y-TZP). Estas restaurações visam aliar elevada translucência, excelente resistência mecânica com o intuito de se promover as restaurações minimamente invasivas, respondendo assim às exigências clínicas atuais. Foi desenvolvido um programa …

    minho-thes Repository record for Development and CAD/CAM production of ultra-thin, high translucent 3Y-TZP zirconia veneers (opens in a new tab)

  3. Processing, microstructure and mechanical properties of alumina platelet reinforced 3Y-TZP and mullite composites

    … matrix composites consisting of mullite and 3Y-TZP containing alumina platelet reinforcements were fabricated by suspension processing and pressureless sintered. The effect of the matrix on the microstructural development in the presence of alumina platelets were characterized. A systematic …

    uiuc Repository record for Processing, microstructure and mechanical properties of alumina platelet reinforced 3Y-TZP and mullite composites (opens in a new tab)

  4. Effect of Different Supporting Die Materials and Crown Thicknesses on the Fracture Load of Monolithic 3Y-TZP Zirconia and Lithium Disilicate Crowns

    … tetragonal zirconia polycrystals (3Y-TZP). Furthermore, we seek to investigate the fracture resistance of different thicknesses of 3Y-TZP and lithium disilicate crowns using different luting cements. Methods: A standardized premolar crown preparation was performed on a typo-dont …

    uab Repository record for Effect of Different Supporting Die Materials and Crown Thicknesses on the Fracture Load of Monolithic 3Y-TZP Zirconia and Lithium Disilicate Crowns (opens in a new tab)

  5. Influence of human osteoblasts on biological and mechanical properties of zirconia implant materials

    … tetragonal zirconia polycrystal (3Y-TZP) and alumina-toughened zirconia (ATZ) implant materials with respect to normal human osteoblastic cell activity and biaxial flexural strength. Disc-shaped specimens were fabricated from 3Y-TZP and ATZ powders, sintered according to …

    bu Repository record for Influence of human osteoblasts on biological and mechanical properties of zirconia implant materials (opens in a new tab)

  6. Diamond Bur Cutting Efficiency of Dental Zirconia

    … cut sintered Yttria Stabilized Zirconia blocks (3Y-TZP) at a constant 0.9N force for five minutes. The distance traveled was measured by a Linear Variable Differential Transformer (LVDT) and recorded per time by a data acquisition device. Time was divided into 100-second intervals for comparison. …

    wvu Repository record for Diamond Bur Cutting Efficiency of Dental Zirconia (opens in a new tab)

  7. A Thermodynamic Study of 3 Mole Percent Yttria Stabilized Zirconia

    … This discovery led to the special interest in 3Y-TZP(3 m/o Y2O3-ZrO2) which contains primarily the tetragonal structure. Along with its ultra-high strength, its excellent thermal shock resistance provides another stimulus for investigating the electrical behavior of 3Y-TZP. 3Y-TZP also has a …

    marquette Repository record for A Thermodynamic Study of 3 Mole Percent Yttria Stabilized Zirconia (opens in a new tab)

  8. Assessment of Tapered Diamond Bur Cutting Efficiency of Dental Zirconia

    … and among time periods on cutting efficiency of 3Y-TZP. Coarse 151 microm super coarse 181 microm and DuraCut 151 microm were significantly more efficient in cutting 3Y-TZP in 5 minutes and in the first 100 seconds. Diamond burs with average grit size ≥ 151 demonstrated greater cutting …

    wvu Repository record for Assessment of Tapered Diamond Bur Cutting Efficiency of Dental Zirconia (opens in a new tab)

  9. Grain Coalescence and Modeling of Nanosized Zirconia in Solid-state Sintering

    … 50nm 3 mol % Yttria Stabilized Zirconia powder (3Y-TZP) was selected to demonstrate the potential of injection molding micro features. The produced 3mm micro gear was visually defect-free with well defined gear teeth and achieving high hardness of 3Y-TZP. Sintering behavior of the nanosized …

    nus Repository record for Grain Coalescence and Modeling of Nanosized Zirconia in Solid-state Sintering (opens in a new tab) Download file for Grain Coalescence and Modeling of Nanosized Zirconia in Solid-state Sintering (opens in a new tab)

  10. Bio-inspired nacre-like ceramic/polymer composites for dentistry

    … tetragonal zirconia polycrystal (3Y-TZP)/polymethyl <br/>methacrylate (PMMA), 5 mol% yttria partially stabilised zirconia (5Y-PSZ)/PMMA, <br/>zirconia-toughened alumina (ZTA)/PMMA, and glass flake/PMMA. These composites were <br/>fabricated using bi-directional freeze casting and …

    bristol Repository record for Bio-inspired nacre-like ceramic/polymer composites for dentistry (opens in a new tab) Download PDF for Bio-inspired nacre-like ceramic/polymer composites for dentistry (opens in a new tab)

  11. Fracture Toughness Testing of 3, 4, and 5 mol% Yttria Stabilized Zirconia Ceramics Using the Single Edge V-notch Beam Test

    … of 3, 4, and 5 mol% yttria stabilized zirconia (3Y, 4Y, 5Y-TZP) in comparison to lithium disilicate glass-ceramics using a modified version of SEVNB method by hopefully creating an appropriately sharp starter crack with focused ion beam (FIB) milling technology. 3. MATERIALS & METHODS: Fracture …

    uconn-diss Repository record for Fracture Toughness Testing of 3, 4, and 5 mol% Yttria Stabilized Zirconia Ceramics Using the Single Edge V-notch Beam Test (opens in a new tab)

  12. Assessing the clinical viability of one- and two-piece zirconia implants as alternatives to titanium-based restorations in the anterior mandible

    … zirconia crown (LayZir) transitioning from 3Y-TZP cervically to 5Y-PSZ occlusally. A physiological oblique load of 10.1 N was applied palato-labially. Von Mises stress was evaluated across implant components and surrounding bone. Crown optical behavior was characterized by contrast ratio …

    bu Repository record for Assessing the clinical viability of one- and two-piece zirconia implants as alternatives to titanium-based restorations in the anterior mandible (opens in a new tab)

  13. DUCTILE GRINDING OF DENTAL CERAMICS

    … zirconia with different yttria concentrations (3Y-TZP and 5Y-PSZ) were tested. Micro-scratch tests with a single diamond indenter were conducted under controlled scratching loads. Additionally, grinding using conventional lapping technology was performed by controlling grinding grit sizes. The …

    penn Repository record for DUCTILE GRINDING OF DENTAL CERAMICS (opens in a new tab) Embargoed until 2028-06-04

  14. The Effect of Different Screw Angulations on the Fracture Resistance of Implant Zirconia Single Crowns Made on Two Different Implant Platforms

    … center to fabricate screw-retained monolithic 3Y-TZP single crown restorations. After that, the restorations were bonded to Dynamic TIBASE® abutment and torqued to 25Ncm on implant replicas that were mounted on resin blocks. The universal testing machine was used to test the fracture strength …

    tamu Repository record for The Effect of Different Screw Angulations on the Fracture Resistance of Implant Zirconia Single Crowns Made on Two Different Implant Platforms (opens in a new tab)

  15. Shear Bond Strength of Different Types of Zirconia Bonded with Self-Adhesive Resin Cement with and Without a Primer Application

    … 3mol% Yttria Tetragonal Zirconia Polycrystals (3Y-TZP, n= 60), 4mol% Yttria Tetragonal Zirconia Polycrystals (4YSZ, n= 60), and 5mol% Yttria Tetragonal Zirconia Polycrystals (5Y-TZP, n=60). All zirconia specimens were sandblasted with a tribochemical surface etch using Rocatec Plus. Zirconia …

    buffalo Repository record for Shear Bond Strength of Different Types of Zirconia Bonded with Self-Adhesive Resin Cement with and Without a Primer Application (opens in a new tab)

  16. Comparing Volumetric Wear of Lithium Disilicate Against Different Ceramics and Enamel Antagonist an In-Vitro Study

    … wheel. For the antagonist, balls made of 3Y-TZP, 5Y-TZP, LDC, and FP were milled at an external laboratory. The ceramic materials, 3Y-TZP, 5Y-TZP, and e.max were polished with ASAP Indirect+ for 20 seconds each. Similarly, porcelain antagonists were polished with Dialite Feather Lite for …

    uab Repository record for Comparing Volumetric Wear of Lithium Disilicate Against Different Ceramics and Enamel Antagonist an In-Vitro Study (opens in a new tab)

  17. Effect of Toothbrushing on a Monolithic Dental Zirconia Submitted to an Accelerated Hydrothermal Aging

    … the biaxial flexural strength of monolithic 3Y-TZP ceramic specimens and (2) to assess their surface roughness after being submitted to accelerated hydrothermal aging (simulation 1-10 years of aging); and simulated toothbrushing (simulation 1-10 years of toothbrushing). Materials/Methods: 84 …

    iupui Repository record for Effect of Toothbrushing on a Monolithic Dental Zirconia Submitted to an Accelerated Hydrothermal Aging (opens in a new tab)

  18. Fracture Load of Cantilever Implant-Supported Zirconia Fixed Partial Dentures: An In Vitro Study

    … high-strength monochromatic composition (3Y-TZP - tetragonal zirconia polycrystal) and high-translucency zirconia with polychromic multilayer and uniform compositions (4Y-PSZ and 5Y-PSZ). The study also aims to examine the impact of varying connector dimensions on the mechanical …

    buffalo Repository record for Fracture Load of Cantilever Implant-Supported Zirconia Fixed Partial Dentures: An In Vitro Study (opens in a new tab)

  19. Validierung von Mindestschichtstärken (okklusal, axial, marginal) der Zirkonoxidkeramik KATANA™ unter Berücksichtigung ihrer Transluzenz für den Einsatz substanzschonender Präparation

    … Bei den drei Keramiken handelt es sich um eine 3Y-TZP (Multi Layer), eine 4Y-TZP (Super Translucent Multi Layer) und eine 5Y-TZP (Ultra Translucent Multi Layer) Keramik. Sie werden in 0,4 mm, 0,8 mm und 1,2 mm [H] x 2,4 mm [B] x 12 mm [L] Prüfkörper (n = 15) gesägt, die einmal quer zur …

    fu-berlin Repository record for Validierung von Mindestschichtstärken (okklusal, axial, marginal) der Zirkonoxidkeramik KATANA™ unter Berücksichtigung ihrer Transluzenz für den Einsatz substanzschonender Präparation (opens in a new tab)

  20. The Influence of Cutback Design on the Fracture Strength of Zirconia Crowns with Minimal Porcelain Veneering

    … is to compare designs of partially veneered 3Y-TZP zirconia crowns, quantify the fracture and ultimate compressive loads and define the failure patterns. A premolar was prepared with a 1mm reduction. The die was duplicated, 30 specimens were fabricated and divided in 3 groups (n=10): Group A …

    umn Repository record for The Influence of Cutback Design on the Fracture Strength of Zirconia Crowns with Minimal Porcelain Veneering (opens in a new tab)