Global ETD Search

Search theses and dissertations gathered from participating repositories worldwide. Every result links back to the library that holds it. No account is needed.

Results 1 to 20 of 47 for “"4140 Steel"”

  1. Modeling of austenite decomposition in an AISI 4140 steel

    … and/or non equilibrium phases in a low alloy steel, such as AISI 4140, by performing isothermal transformation experiments is time consuming and hence not cost effective. Further, to generate meaningful and accurate data with respect to the various stages of the progress of the austenite …

    ubc Repository record for Modeling of austenite decomposition in an AISI 4140 steel (opens in a new tab)

  2. Microstructure influence on hydrogen permeation and embrittlement of 4140 steel

    … un acero estructural de media aleación (grado 4140) y se ha analizado primero su influencia en la microestructura y propiedades mecánicas fundamentales. A continuación, se ha estudiado la cinética de la permeación de hidrógeno a través de todas estas microestructuras. Se han determinado con …

    oviedo Repository record for Microstructure influence on hydrogen permeation and embrittlement of 4140 steel (opens in a new tab)

  3. Influence Of Dissolved Hydrogen On The Fatigue Crack Growth Behaviour Of Aisi 4140 Steel

    … to other metallic elements such as Iron in steels, can enter the material and become dissolved in the matrix. It can lodge itself in interstitials locations of the metal atoms, at vacancies or dislocations in the metallic matrix or at grain boundaries or inclusions (impurities) in the alloy. …

    wayne-thes Repository record for Influence Of Dissolved Hydrogen On The Fatigue Crack Growth Behaviour Of Aisi 4140 Steel (opens in a new tab)

  4. Forging effects on manganese sulfide inclusions as fatigue initiation sites in AISI 4140 steel

    … the shape and distribution of MnS inclusions in steel, and their role as fatigue initiation sites. Billets, 5.0 in. in diameter and 9.7 in. high, of three heats of AISI 4140 steel were upset forged at 2200°F to a 50% reduction. The heats were produced by inert-gas-shielded/bottom pouring, and had …

    ohiolink Repository record for Forging effects on manganese sulfide inclusions as fatigue initiation sites in AISI 4140 steel (opens in a new tab)

  5. Application of the Maximum Deformation Theory of Failure to the Torsional Failure Due to Fracture of 4140 Steel

    Forming is the fastest way of changing the shape of a piece of metal. It is the most economical process to use for high-volume mass production when the shape of a part is such that it can be made by one of the forming operations

    byu Repository record for Application of the Maximum Deformation Theory of Failure to the Torsional Failure Due to Fracture of 4140 Steel (opens in a new tab)

  6. Determination of shot peening effect on fatigue behavior of AISI 4140 steel by non-destructive measurement of surface residual stresses

    … peening severity on the fatigue life of AISI 4140 steel. By this way, it might be possible to correlate the MBN measurement results with fatigue life and to verify nondestructively the success of shot-peening process to achieve the desired fatigue life.

    metu Repository record for Determination of shot peening effect on fatigue behavior of AISI 4140 steel by non-destructive measurement of surface residual stresses (opens in a new tab)

  7. Avaliação do efeito de modificações superficiais a plasma no desempenho frente ao desgaste de um aço baixa liga: estudo da correlação entre profundidade de endurecimento e melhoria de desempenho

    … to improve the wear resistance of an AISI 4140 low alloy steel, two surface treatments were applied: plasma nitriding and PAPVD coating. Wear resistance against cavitation erosion and microabrasion of: AISI 4140 steel, 2 and 4 hours nitrided AISI 4140 steel, Cr-Al-N coated AISI 4140 steel …

    brazil-ufmg Repository record for Avaliação do efeito de modificações superficiais a plasma no desempenho frente ao desgaste de um aço baixa liga: estudo da correlação entre profundidade de endurecimento e melhoria de desempenho (opens in a new tab)

  8. High strain rate-induced failure in steels at high shear strains

    … adiabatic shear bands (ASB). In this study, AISI 4140 steel was tested using a torsional split Hopkinson bar at three different strain rates and the impact of strain rate on the material behaviour was examined. The influence of material hardness on failure mechanisms was also investigated by …

    manitoba Repository record for High strain rate-induced failure in steels at high shear strains (opens in a new tab)

  9. Coolant fluid in a turning operation: Soybean coolant fluid in different concentrations versus petroleum coolant fluid

    … point a number of tests were performed turning 4140 steel on a CNC turning center. A number of tests were conducted to provide a comparative study of dry, petroleum based cutting fluid and soybean based cutting fluid at different concentrations. It has been found that the soy based cutting fluid …

    northern-iowa Repository record for Coolant fluid in a turning operation: Soybean coolant fluid in different concentrations versus petroleum coolant fluid (opens in a new tab)

  10. Development of low alloy steel by direct metal laser sintering

    … process parameters for low alloy (4340/4140 steel) for the powder bed fusion process. Low alloy steel is used in parts where high strength and toughness are required. During parameter optimization, several aspects of the process are investigated. Powder size and morphology optimization …

    njit Repository record for Development of low alloy steel by direct metal laser sintering (opens in a new tab)

Page 1 of 3