Showing 1 to 20 of 60 for “"5AL"”.
-
Ultrasonic characterization of Ti-5Al-5Mo-5V-3Cr
Metastable β titanium alloys such as Ti-5Al-5Mo-5V-3Cr are of increasing interest due to their excellent corrosion resistance, high strength, and in particular, the ability to manipulate microstructure to a high degree to control the mechanical properties of the material. It is therefore important …
-
Mechanical Characterization and Evaluation of Additively Manufactured Titanium 5V-5Mo-5Al-3Cr Alloy
Ti-5V-5Mo-5Al-3Cr (Ti-5553) is a near beta titanium alloy commonly used in aerospace applications. It is currently being explored for additive manufacturing (AM), but the fatigue behavior of this AM alloy needs to be well-understood for adoption in aerospace applications. The present work examines …
-
Implementation of FAST-forge for Ti-5Al-5Mo-5V-3Cr and Ti-Ti composites
… steps for a metastable β titanium alloy, Ti-5Al-5Mo-5V-3Cr (Ti-5553), used in landing gear. The alternative process consists of: using field-assisted sintering technology (FAST) to heat and consolidate powder into a solid billet, by the application of direct current; forging the billet in …
-
Understanding the relationship between microstructure and mechanical properties in HIPped Ti-5Al-5Mo-5V-3Cr
Ti-5Al-5Mo-5V-3Cr (Ti-5553), a relatively new generation beta titanium alloy has the advantage of high strength. It is a current generation alloy used in landing gear. Currently, landing gear components are large scale and processed through forging, followed by complex heat treatments. HIPping (hot …
-
Laser Powder Bed Fusion Additive Manufacturing and Post Processing of Ti-5Al-5Mo-5V-3Cr Alloy
Metastable β titanium alloys like Ti-5Al-5Mo-5V-3Cr (Ti-5553) are highly valued in the aerospace industry due to exceptional specific strength and fatigue crack growth resistance [1]. Particularly, Ti-5553 is ideal for structural and additive manufacturing applications, maintaining a near-beta …
-
Microstructure Evolution and Phase Transformation of Welded Metastable Beta-titanium Alloy (Ti-5Al-5V-5Mo-3Cr)
Ti-5Al-5V-5Mo-3Cr (Ti5553, in wt%) is a recently developed metastable β titanium alloy, specifically designed to replace Ti-10V-2Fe-3Al (VT22) in the manufacture of large airplane components. The studies of Ti5553 have drawn the attention of many researchers. Ti5553 shows reasonable weldability and …
-
Micromechanics of Polycrystalline TI-5AL-2.5SN Using Differential Aperture X-ray Microscopy and Crystal Plasticity Simulation
… surface plastic deformation processes of a Ti-5Al-2.5Sn sample deformed under uniaxial tension at ambient temperature were analyzed using differential aperture X-ray microscopy (DAXM) and computational models based on crystal plasticity theory. A series of crystal plasticity simulations were …
-
Microstructural Engineering and Deformation Mechanisms in an Additively Manufactured Metastable Beta Ti-5Al-5Mo-5V-3Cr Alloy
Metastable β titanium alloys serve as critical structural materials in the aerospace industry for improved fuel efficiency and reduced CO2 emissions due to their high specific strength, excellent fracture toughness, and deep hardenability. However, the high production cost and the lack of …
-
Analysis of slip transfer in TI-5AL-2.5SN (WT. %) at two temperatures in comparison to pure aluminum
… will aid in improving modeling methods. Ti-5Al-2.5Sn samples were tensile tested at 296K and 728K, and slip behavior was assessed near grain boundaries. From the EBSD measurements of grain orientations, various metrics related to the slip systems, traces, residual Burgers vectors, and grain …
-
Understanding the effect of surface generation rates for finish milling of Ti-5Al-5Mo-5V-3Cr aero-structural components
… and fatigue performance for finish milling of Ti-5Al-5Mo-5V-3Cr landing gear components. Low cost, small scale testing methodologies have been developed to replicate complex machining strategies employed in aerospace manufacturing, to understand and develop an improved processing window. …
-
Investigation of the High-Speed Finish-Turning of Ti-5Al-5V-5Mo-3Cr Using Novel Mono/Bi-layered PVD-Coated WC Tools
The Ti-5Al-5V-5Mo-3Cr alloy is used in aerospace, biomedical, and military fields due to its outstanding thermomechanical properties. Nevertheless, its higher strength and toughness make it more challenging to machine compared to traditional Ti alloys like Ti-64. Despite increasing demand, there is …
-
MACHINABILITY COMPARISON BETWEEN TWO DIFFERENT GRADES OF TITANIUM ALLOYS UNDER DIVERSE TURNING AND COOLING CONDITIONS: Ti-6Al-4V and Ti-5Al-5V-5Mo-3Cr
… choice until recently, when Ti-555.3 (Ti-5Al-5V-5Mo-3Cr) began to take its place. Ti-555.3 has improved resistance to fatigue and higher mechanical properties compared to Ti-64 and is able to maintain its strength when exposed to high temperatures, which warrants its acceptance for many …
-
Towards an understanding of high strength metastable β titanium alloy machinability
… conducted on the metastable β titanium alloy, Ti-5Al-5Mo-5V-3Cr. The titanium alloys; Ti-6Al-4V, Ti-6Al-2Sn-4Zr-6Mo and Ti-5Al-2Sn-2Zr-4Cr-4Mo were also investigated to provide comparability. Emphasis was placed on; 1) Characterising microstructural deformation in the workpiece. 2) Analysing force …
-
A study of the high temperature oxidation and microstructure of niobium silicide-based alloys with the additions of boron and germanium
… to facilitate comparison, KZ5 (Nb-18Si-24Ti-5Cr-5Al), and three novel boron and germanium containing alloys, JW1 (Nb-18Si-24Ti-5Cr-5Al-5Ge-5B), JW2 (Nb-18Si-24Ti-5Cr-5Al-5Ge-10B) and JW3 (Nb-18Si-24Ti-5Cr-5Al-10Ge-5B). As-cast and heat-treated (1300oC/1500oC) states of each alloy were …
-
In-situ evaluation of the hcp to bcc phase transformation kinetics in commercially pure titanium and Ti-5Al-5Mo-5V-3Cr alloy using laser ultrasonics
This thesis developed and validated laser ultrasonics as an in-situ monitor of phase transformations in commercially pure titanium and Ti - 5 wt.% Al - 5 wt.% Mo - 5 wt.% V - 3 wt.% Cr (Ti-5553). Three studies (Chapters 5, 6 and 7) were performed to achieve this goal. The first study involved using …
-
The Effect of Heat Treatment on the Microstructure Evolution and Mechanical Properties of Ti-5Al-5V-5Mo-3Cr, and Its Potential Application in Landing Gears.
<p>The properties and microstructure of Ti-5Al-5V-5Mo-3Cr were characterized under various stress states after the following heat treatments: 1) annealing above the β transus, followed by cooling at various rates and ageing for different times; 2) solution heat treatment in the α-β range, …
-
The genetics of leaf rust resistance in the durably resistant wheat cultivar ‘Toropi’
… associated with leaf rust resistance (QLr.crc-5AL.1) on chromosome 5AL, which overlapped with a QTL for stripe rust (QStr.crc-5AL.1) in the same population. This gene, designated Trp1, is believed to be one of the two adult plant complementary partial resistance genes. The position of the Trp-2 …
-
Mechanical properties of heat-treated additively manufactured titanium alloys
… AM community, the metastable β titanium alloy Ti-5Al-5V-Mo-3Cr has only recently become a candidate alloy for investigation. In the second part of this work, samples of Ti-5Al-5V-Mo-3Cr manufactured by laser power bed fusion (L-PBF) were subjected to 27 unique heat treatments and subsequently …
Page 1 of 3