Global ETD Search
Search theses and dissertations gathered from participating repositories worldwide. Every result links back to the library that holds it. No account is needed.
Results 1 to 20 of 1,132 for “"700°C"”
-
Sickness, disability, and miracle cures: hagiography in England, c. 700 - c. 1200
<p>This thesis considers how religious literature represented sickness and disability in Anglo- Saxon and post-Conquest England. Based on Gospel accounts of Jesus's healings, narratives of miracle-cures were highly valued within medieval Christian culture. By analysing a selection of miracle-cure …
-
Early Stage Hot Corrosion Behavior of Pt/Cr-Modified ß-NiAl Alloys at 700°C
… sulfate-deposit induced Type II hot corrosion at 700°C was systematically studied using advanced micro-characterization techniques. The model compositions studied in this study are relevant to ß-NiAl coatings used in current technology to protect Ni-based superalloys. In Type II hot corrosion, …
-
An experimental calibration of chlorine isotope fractionation between amphibole and fluid at 700 °C and 0.2 GPa
… amphibole and fluid has been determined at 700 °C and 0.2 GPa. Rates of isotope exchange between pargasite and water at 600-800 °C were slow; therefore synthesis of amphibole in the presence of a fluid was necessary to facilitate the incorporation of Cl into amphibole. Hastingsite was …
-
Etude thermo-chimico-mécanique de l’acier inoxydable AISI 316L oxydé entre 700°C et 900°C sous air humide
… austénitique AISI 316L ont été effectués de 700°C à 900°C sous air contenant différentes humidités (0-8% vol) pendant différentes durées (6-96h). La morphologie de la surface d’oxyde, la microstructure de la section transversale, l’identification de phases d’oxyde, les contraintes de …
-
Corrosion Behaviour of Fe-Cr and Ni-Cr Alloys in O2, H2O and H2O+O2 gases at 700°C
… (0, 5, 10, 20 and 30wt%) alloys were reacted at 700°C in Ar-20%O2, Ar-20%O2-20%H2O and Ar-20%H2O, respectively. For pure iron, the three typical iron oxides formed in all atmospheres with a thick FeO layer surmounted by thin Fe3O4 and Fe2O3 layers. The presence of water vapor changed the oxide …
-
Alternate Novel Thermal Structure Interaction Designs of Molten Salt Shell Structures at High Temperatures Ranging from 565˚C to 700˚C
Excess energy from solar power stations and other baseline power production methods canbe stored in molten salts (MS) in the 565°C range, therefore allowing the use of large containers to store energy for up to a week and generate eight hours of electricity or more to be used during peak demand …
-
Kinetics and Morphological Development of the Sulphide Scale on a Nickel - 20 w/o Chromium Alloy at 700°C and Low Sulphur Potentials
… for sulphidation on a Ni-20 wt. % Cr alloy at 700ºC and sulphur potentials below 10⁻⁹ atmospheres have been studied using a thermogravimetric technique. The morphology of the reaction product was studied using optical microscopy, electron probe microanalysis and X-ray techniques. The kinetics …
-
Synthèse et étude thermodynamique d’alliages Ir-Rh à l’état massif et en films minces pour la réalisation de capteurs SAW fonctionnant à haute température (700°C-1000°C) dans l’air.
La technologie des capteurs à ondes élastiques de surface, appelés SAW pour Surface acoustic waves, existe depuis une cinquantaine d’années. Cette technologie est largement utilisée dans l’industrie des télécommunications et en perpétuelle évolution pour la réalisation de microcapteurs dans des …
-
Development and breakdown of oxide scales on iron-25 percent chromium-20 percent nickel alloys in atmospheres containing oxygen and sulfur
… sulfur. Pure oxidation has been carried out at 700°C and 900°C in 1 atm O<sub>2</sub> as well as in H<sub>2</sub>-H<sub>2</sub>O atmospheres of low oxygen partial pressures (at 700°C in a range of 10<sup>-31</sup> to 10<sup>-20</sup> atm and at 900°C in a range of 10<sup>-24</sup> to …
-
Étude de matériaux composites à base de nanosiliciures de métaux de transition pour la thermoélectricité
… est performant à haute température (à partir de 700 °C), c'est pourquoi il trouve également un fort intérêt dans l'industrie automobile. De nombreuses recherches dans ce secteur s'orientent vers la thermoélectricité, notamment vers des modules fonctionnant à haute température pour permettre la …
-
Studies on Particle-Wall Interactions in Particle-based High Temperature Concentrating Solar Thermal Systems
… medium to reach operating temperatures above 700 °C, but the continuous contact between flowing particles and component surfaces drives severe material degradation through the coupled action of high-temperature oxidation and abrasion. This thesis examines particle–wall interactions in …
-
Evaluación radiográfica de la anchura coronal y la distancia cabeza-primera espira de los implantes dentales para su identificación morfológica tras el sometimiento a diferentes temperaturas y tiempos
… C durante 15 minutos, 500° C durante 30 minutos, 700° C durante 15 minutos, 800° C durante 15 minutos, 800° C durante 45 minutos, 500° C durante 15 minutos y 700° C durante otros 15 minutos y finalmente a 1000° C durante 2 horas. Material y método Implantes dentales de diversas empresas …
-
Studium intermetalických fází v lité duplexní oceli
… v důsledku izotermického žíhání na teplotě 700 °C a 595 °C. Doba izotermického žíhání při teplotě 700 °C se pohybovala od 1 do 160 hodin a při teplotě 595 °C od 24 do 245 hodin. Studium mikrostruktury po žíhání na teplotě 700 °C prokázalo vyloučení -fáze, Lavesovy fáze, karbidů chromu a …
-
Pile à combustible à céramique conductrice protonique : élaboration et caractérisations physico-chimiques et électrochimiques des matériaux et optimisation de la mise en forme par le procédé de densification à basse température CSP
… opérant dans le domaine de température 400-700°C. L’électrolyte est BaCe0.8Zr0.1Y0.1O3-δ (BCZY), l'anode est le cermet Ni-BCZY et la cathode est Pr2NiO4+δ. Des poudres pures de ces composés ont été synthétisées par auto combustion selon le procédé glycine-nitrate et leur microstructure a été …
-
Rational design of nickel-based perovskite-type cathode for improved performance of protonic ceramic fuel cells
… PCFCs operate at a temperature range 550-700 °C. However, PCFCs face numerous challenges. One of the most significant challenges is the slow oxygen reduction reaction (ORR) kinetics. Additionally, protons react with oxygen to produce water at the cathode. Thus, proton transfer is also …
-
Low pressure chemical vapor deposition of silicon dioxide and phosphosilicate glass thin films
… were processed at different temperatures between 700 C and 850 C at a constant pressure, and at different flow ratios of the precursors. The films deposited were uniform, amorphous and the composition of the films varied with deposition temperature and precursor flow ratios. The deposition rate …
-
High Manganese Press Hardenable Steel for Automotive Safety Applications
… function of the DHPF temperatures of 550 – 700 °C. The substrate predominantly consisted of martensite with small amounts of ferrite and the coating consisted of α-Fe(Zn) and ≥ 15 vol.% Γ-Fe3Zn10. Based on the fraction of Γ-Fe3Zn10 and the coating thickness, robust cathodic corrosion …
-
Influence de la microstructure sur les micromécanismes de déformation en fluage dans le superalliage AD730TM
… qui contrôlent la déformation en fluage à 700°C, dans le superalliage AD730(tm) développé par Aubert & Duval pour la fabrication des disques de turbines des futurs turboréacteurs pour application civile. Les différents éléments de la microstructure (taille, distribution et composition …
-
Compósito de zircônia comercial com hidroxiapatita pura produzida via método sol gel para aplicações biomédicas
… calcination times (500°C/2h, 500°C/4h, 500°C/6h; 700°C/1h, 700°C/2h, 700°C/4h; 900°C/4h). The samples showed commercial yttria doped zirconia layer followed by composite material layer produced with commercial zirconia and hydroxyapatite calcined at 700°C/4h in the following proportions YSZ/HA …
Page 1 of 57