  1. Aqueous corrosion of AA-2024 by zinc coated steel fasteners

    Thesis (M.S.)--Michigan State University. Department of Metallurgy, Mechanics and Materials Science, 1989

    msu Repository record for Aqueous corrosion of AA-2024 by zinc coated steel fasteners (opens in a new tab)

  2. Friction surfacing of aluminum alloy 5083-H112 over AA 2024-T3

    … The present study addresses the deposition of AA5083-H112 coatings over AA2024-T3 substrates, focusing on the influence of the thermo-mechanical process in the mechanical properties and geometry of the deposits. A performance and geometric analysis of the depositions are also presented. Sound …

    brazil-ufscar Repository record for Friction surfacing of aluminum alloy 5083-H112 over AA 2024-T3 (opens in a new tab)

  3. POLYANILINE CLAY - POLYIMIDE HYBRID NANOCOMPOSITE COATINGS FOR CORROSION PROTECTION OF AA 2024

    … PI) hybrid nanocomposite coatings were cast onto AA 2024 to give corrosion resistant coatings. The PACN powders were prepared from different formulations containing varying concentrations of the dopant and clay. The powders were characterized by using various analytical techniques including the …

    ohiolink Repository record for POLYANILINE CLAY - POLYIMIDE HYBRID NANOCOMPOSITE COATINGS FOR CORROSION PROTECTION OF AA 2024 (opens in a new tab)

  4. Conducting Polymers / Polyimide-Clay Nanocomposite Coatings for Corrosion Protection of AA-2024 Alloy

    … was solution cast as the barrier layer on AA-2024 alloy. This study will provide a better understanding of the corrosion protection mechanism of the conducting polymer coating. Various characterization techniques such as infrared spectroscopy, cyclic voltammetry and scanning electron …

    ohiolink Repository record for Conducting Polymers / Polyimide-Clay Nanocomposite Coatings for Corrosion Protection of AA-2024 Alloy (opens in a new tab)

  5. Effects of ultrasonic impact treatment on fatigue life of pre-exfoliated AA-2024-t351.

    … Impact Treatment (UIT) on pre-exfoliated AA 2024 T351. Electrochemical tests were conducted to determine any changes in electrochemical behaviour of the alloys due to UIT condition. Uniaxial monotonic, cyclic and fatigue crack propagation (FCG) tests were conducted on material in …

    sheffield-hallam Repository record for Effects of ultrasonic impact treatment on fatigue life of pre-exfoliated AA-2024-t351. (opens in a new tab)

  6. Low velocity impact characterization of monolithic and laminated AA 2024 plates by drop weight test

    … plates were investigated. Tested material was AA 2024, heat treatable aluminum alloy, which was artificially aged to obtain a wide range of mechanical properties. In the second stage of the study, the relationship between the low velocity impact behavior of laminated plates was compared with …

    metu Repository record for Low velocity impact characterization of monolithic and laminated AA 2024 plates by drop weight test (opens in a new tab)

  7. Aa 2024-T3 alüminyum alaşımının sürtünme karıştırma kaynağında işlem parametrelerinin mikroyapı ve mekanik özelliklere etkileri

    AA2024-T3 ALÜM NYUM ALAŞIMININ SÜRTÜNME KARIŞTIRMAKAYNAĞINDA ŞLEM PARAMETRELER N N M KROYAPI ve MEKAN KÖZELL KLERE ETK LERALANUR B NALÖZETBu çalışmada sürtünme karıştırma kaynak yöntemi ile birleştirilen AA2024-T3alüminyum levhaların mikro yapı ve mekanik özellikleri işlem parametrelerine …

    ogu-tr Repository record for Aa 2024-T3 alüminyum alaşımının sürtünme karıştırma kaynağında işlem parametrelerinin mikroyapı ve mekanik özelliklere etkileri (opens in a new tab)

  8. Damage Evolution of Magnesium Rich Primer Applied over AA 2024 T-3 Alloy Exposed to Aggressive Environments

    Al 2024 T-3 is a commonly used alloy in the aircraft industry which is highly susceptible to localized corrosion when subjected to corrosive environments. Of the many corrosion protection systems, applying a coating is one of the most cost effective methods. The classical physical barrier …

    ohiolink Repository record for Damage Evolution of Magnesium Rich Primer Applied over AA 2024 T-3 Alloy Exposed to Aggressive Environments (opens in a new tab)

  9. Korozní ochrana slitin hliníku

    … inhibitorů. Následuje charakterizace slitiny AA 2024. Předmětem hlavní části je mechanismus tvorby směsného ceritého konverzního povlaku na slitině AA 2024. V posledním oddílu jsou poté komentovány faktory ovlivňují charakter a kvalitu vzniklých povlaků. V experimentální části byl sledován …

    brno-tech Repository record for Korozní ochrana slitin hliníku (opens in a new tab)

  10. Simulation of hard projectile impact on friction stir welded plate

    … specimen. Then the impact on an Aluminium Alloy 2024 (AA 2024) plate without FSW was modelled. The minimum thickness of a homogeneous AA 2024 plate which could withstand the impact from engine debris is 3 mm. Finally the impact on 3 mm thick AA 2024 FSW plate was simulated. The welding induced …

    cranfield Repository record for Simulation of hard projectile impact on friction stir welded plate (opens in a new tab)

  11. Embedded Reference Electrodes for Corrosion Potential Monitoring, Electrochemical Characterization, and Controlled-Potential Cathodic Protection

    … the corrosion potential of Mg primer on AA 2024-T3 for 800 days of constant immersion in dilute Harrison’s solution. Zn primer on steel had low accuracy in comparison. This is in part due to short circuiting by Zn oxidation products, which are much more conductive than Mg corrosion …

    ndsu Repository record for Embedded Reference Electrodes for Corrosion Potential Monitoring, Electrochemical Characterization, and Controlled-Potential Cathodic Protection (opens in a new tab)

  12. CORROSION PROTECTION OF METALS BY SILANE SURFACE TREATMENT

    … (bis-amino silane) were deposited on AA 2024-T3 and were characterized mainly using reflection-absorption Fourier-transform infrared spectroscopy (FTIR-RA) and electrochemical impedance spectroscopy (EIS) techniques. The results showed that further hydrolysis and crosslinking occurs in …

    ohiolink Repository record for CORROSION PROTECTION OF METALS BY SILANE SURFACE TREATMENT (opens in a new tab)

  13. DEFORMATION AND DAMAGE MECHANISMS IN SELECTED 2000 SERIES ALUMINUM ALLOYS UNDER BOTH QUASI-STATIC AND DYNAMIC IMPACT LOADING CONDITIONS

    … on the deformation and damage mechanisms in AA 2017, AA 2024 and AA 2624 aluminum alloys under both quasi-static and dynamic impact loading conditions. Cylindrical specimens of the selected aluminum alloys were investigated under both quasi-static loading at 3.2 x10-3 s-1 using an Instron …

    sask Repository record for DEFORMATION AND DAMAGE MECHANISMS IN SELECTED 2000 SERIES ALUMINUM ALLOYS UNDER BOTH QUASI-STATIC AND DYNAMIC IMPACT LOADING CONDITIONS (opens in a new tab)

  14. Simulation of Microstructural Evolution of Selective Laser Melting of Metal Powders

    … formed during the melting process of a powdered AA-2024 feedstock using the AM process SLM. The presented CA model is coupled with a detailed thermal FE model which computes the heat flow characteristics of the SLM process. The developed model takes into account the powder-to-liquid-to-solid …

    whiterose Repository record for Simulation of Microstructural Evolution of Selective Laser Melting of Metal Powders (opens in a new tab)

  15. Microstructural characterization & viscoelastic properties of AlZnMg & AlCuMg alloys

    … the viscoelastic behaviour of aluminium alloys AA 7075-T6 and AA 2024-T3, and of pure aluminium in the H24 temper. The identification of the mechanical relaxation processes taking place and the relation between the viscoelastic response of AA 7075-T6 and AA 2024-T3 and the fatigue behaviour will …

    barcelona Repository record for Microstructural characterization & viscoelastic properties of AlZnMg & AlCuMg alloys (opens in a new tab)

  16. SYNTHESIS, CHARACTERIZATION AND CORROSION PERFORMANCE OF POLYANILINE-MONTMORILLONITE CLAY NANOCOMPOSITES

    … into coatings for use in the protection of AA 2024-T3. The effect of PACN nanocomposites on the curing of epoxy resin was studied by using FTIR and a significant enhancement in the degree of curing of epoxy was observed. Corrosion performance of the nanocomposite-epoxy coatings on AA 2024 …

    ohiolink Repository record for SYNTHESIS, CHARACTERIZATION AND CORROSION PERFORMANCE OF POLYANILINE-MONTMORILLONITE CLAY NANOCOMPOSITES (opens in a new tab)

  17. In situ stress measurements during anodic dissolution of cold spray AA6061 coating

    In this study, corrosion performance of AA 6061 coating deposited on AA 2024 substrate using the cold spray(CS) deposition technique was investigated.AA 6061 and AA 2024 alloys are used widely in aircraft and marine industries. As received CS coating of 6061 is dense film covered with spherical …

    iastate Repository record for In situ stress measurements during anodic dissolution of cold spray AA6061 coating (opens in a new tab)

  18. Numerical/Experimental Investigation of Plunge Stage and Effect of Donor Material in Friction Stir Welding

    … obtained from literature. Plunge experiments on AA 2024 were also conducted during the course of this research and the axial load and temperature were measured. The ‘donor material’ concept was proposed for the reduction of tool wear at the plunge by providing localized pre-heating at the plunge …

    odu Repository record for Numerical/Experimental Investigation of Plunge Stage and Effect of Donor Material in Friction Stir Welding (opens in a new tab)

  19. Propriedades mecânicas e eletroquímicas de revestimento compósito com incorporação de óxido de grafeno

    … à corrosão e ao desgaste da liga de alumínio AA 2024-T3. A liga de alumínio AA 2024-T3 é um material bastante usado na indústria aeronáutica devido às propriedades mecânicas e à baixa densidade. Contudo, essa liga não oferece a resistência à corrosão e ao desgaste exigidos para aplicação na …

    brazil-ufrgs Repository record for Propriedades mecânicas e eletroquímicas de revestimento compósito com incorporação de óxido de grafeno (opens in a new tab)

  20. ENVIRONMENTALLY-COMPLIANT NOVOLAC SUPERPRIMERS FOR CORROSION PROTECTION OF ALUMINUM ALLOYS

    … coating system for corrosion protection of AA 2024-T3 aerospace alloy. These special coatings which can be applied directly to the metal are termed as ‘superprimers’ and consist of novolac epoxy binder, silanes, polyurethane and non-chromate inhibitors. Coating evaluation tests were employed …

    ohiolink Repository record for ENVIRONMENTALLY-COMPLIANT NOVOLAC SUPERPRIMERS FOR CORROSION PROTECTION OF ALUMINUM ALLOYS (opens in a new tab)