Mechanical and microstructural characterization of commercial AA5083 aluminum alloys
… strain rates and with lower cost materials. AA5083 superplastic materials hold great promise for high-volume SPF production. However, several technical issues related to the material are still not well understood. The present investigation characterizes the mechanical and microstructural …
-
Friction stir processing of AS-CAST AA5083 Superplastic response
Plates of continuously cast AA5083 were subjected to friction stir processing (FSP) by three overlapping plunge and traverses. The FSP used a threaded pin tool with a pin diameter of 3 mm, pin length of 3 mm and a shoulder diameter of 10 mm. The process was run at constant tool rotation and …
-
Effects of laboratory rolling conditions on continuously cast AA5083
… rolling conditions on continuously cast AA5083 in the hot-band condition in anticipation of QPF. Orientation imaging microscopy, scanning electron microscopy and X-ray analysis were used to analyze roles of the geometric dynamic recrystallization and particle stimulated nucleation of …
-
Grain size control in AA5083: thermomechanical processing and particle stimulated nucelation
Superplastic forming is an emerging industrial technology that allows the production of complex shapes in metallic materials including aluminum. A critical characteristic of materials that are capable of sustaining superplastic forming is a fine grain size. In this study a commercial …
-
The effect of applied tensile stress on localized corrosion in sensitized AA5083
… and degree of localized corrosion for sensitized AA5083 under an applied tensile stress. AA5083 is an aluminum-magnesium alloy that experiences severe intergranular corrosion and intergranular stress corrosion cracking if sensitized. In this research, AA5083-H116 plates were cut into bend-bar …
-
Identification of deformation mechanisms during bi-axial straining of superplastic AA5083 material
… evaluated dome test samples of a superplastic AA5083 aluminum alloy deformed at nominally constant strain rates under biaxial strain conditions. Dome test samples resulted from gas-pressure forming of sheet material; for this study, samples were deformed at strain rates corresponding either to …
-
Mathematical modelling of deformation and microstructure evolution during hot rolling of AA5083 aluminum alloy
… thermal and deformation history of AA5083 aluminum sheet undergoing single-pass and multi-pass hot rolling using the commercial finite element package, ABAQUS. A physically based internal state variable microstructure model was employed to calculate the material stored energy and …
-
Mathematical modelling of the microstructural evolution during the hot rolling of AA5083 aluminum alloys
… applied to two commercially significant alloys, AA5083 and AA5056 aluminum alloys. For the AA5083 aluminum alloy application a microstructure component was added to model the microstructure evolution that occurred in the strip in the time between the roll bite exit and the quench. The deformation …
-
The effect of sensitization on the corrosion susceptibility and tensile properties of AA5083 aluminum
Aluminum-magnesium alloy (AA5083-H116) is primarily designed for marine applications such as in ship hulls and deckhouses. Its excellent combination of physical and mechanical properties makes it useful for other applications such as aircraft construction, military equipment and vehicles and …
-
The Effect of Laser Shock Peening on Dislocation Morphology and Microstructural Evolution of AA5083-H116
The AA5083-H116 aluminum alloys (Al-4.7Mg-0.62Mn-0.29Fe-0.15Si-0.099Cr-0.094Zn-0.036Cu-0.018Ti-0.086Other) are lightweight structural materials for marine applications. Due to the high magnesium content (>3wt.%), the sensitization of Al3Mg2 β-phase and susceptibility for intergranular stress …
-
Surface Orientation Dependent Corrosion Damage and Temperature Dependent Mechanical Property Degradation of Sensitized AA5083-H116 Alloys
This study relates the sensitization process microstructural changes of 5083-H116 to its resulting corrosion resistance and mechanical performance. Alcoa 5083-H116 was sensitized in an environmental chamber at 100°C for up to ~1500 hours and 150°C up to ~2000 hours, revealing different degrees of …
-
The effect of microstructure on cavitation during hot deformation in fine-grained AA5083 aluminum alloy sheet material
… Commercial fine-grained aluminum alloy AA5083 sheet is the most commonly used material in the SPF and QPF forming processes. Hot formability of AA5083 is often limited by material cavitation during forming, which makes understanding and controlling cavitation an issue of primary …
-
Quantification of the Effect of Degassing on the Microstructure, Chemistry and Estimated Strength of Nanocrystalline AA5083 Powder
… to strength. In this study, cryomilled AA5083 (0.4 wt.% Mn; 4.5 wt.% Mg; minor Si, Fe, Cu, Cr, Zn, Ti; balance Al) powders were degassed at 200, 300, 350, 410 and 500°C at a ramp rate of 68.3 °C?hr-1 for a soak time of 8 hours with a vacuum at or below 6.5 x 10-3 Pa. Grain size, …
-
Reparo induzido pela técnica de emissão de pulsos elétricos (electropulsing) na liga AA5083 utilizada da indústria do petróleo
… of electrical pulses on specimens (CP) of the AA5083. These were submitted to tensile tests to evaluate the mechanical behavior and to promote microstructural defects that could be repaired later. The CPs were separated into six groups according to the cross-sectional area (15mm2 and 6mm2 ) and …
-
Deformation and failure mechanisms of a modified commercial aluminum alloy at elevated temperatures
… study investigates the potential for forming AA5083, the most common commercial alloy for SPF operations, at reduced temperatures and increased strain-rates. The deformation and failure mechanisms under these conditions are examined in a modified AA5083 material and are compared with data from …
-
Process-Structure-Property-Performance Relationships of Precipitate- and Strain-Hardened Aluminum Alloys as Processed Through Solid-State Additive Manufacturing Process
… (AA6061-T6) and strain-hardened (AA5083-H131) aluminum alloy as processed through AFSD, were quantified. A standard post deposition heat treatment (PDHT) was applied to AA6061 AFSD material, an Al-Mg-Si alloy. The as-deposited material exhibited a refined grain structure, reduced …
-
Development Of Nitrogen Concentration During Cryomilling Of Aluminum Composites
… was developed consisting of nanocrystalline AA5083, boron carbide and coarser grained AA5083. The microstructure was determined through optical microscopy and transmission electron microscopy. A technique was developed to determine the nitrogen concentration of an AA5083 composite from …
-
The effects of applied stress and sensitization on the passive film stability of AL-MG alloys
… behavior for the aluminum magnesium alloy AA5083 in a comprehensive and systematic manner. This study used cyclic polarization and electrochemical impedance spectroscopy to study passive film stability of AA5083-H116, and sought to understand how applied and residual tensile and compressive …
-
Avaliação das técnicas de soldagem MIG-P CA e MIG-P CC+ aplicadas ao passe de enchimento em liga de alumínio AA5083
… which best suits pass by filling bevel on AA5083 aluminum sheets with 8 and 12 mm thick respectively. Furthermore, two types of wire, ER5087 and ER5183 were evaluated. To evaluate the process and versions of the wires, the high-speed cameras and thermal were used to monitor the metal …
-
Systematic review of ultrasonic impact treatment parameters on residual stresses of welded non-sensitized versus sensitized aluminum-magnesium
… welds in AA5456 after UIT, around welds in AA5083 installed on-board a U.S. naval combatant and in AA5083 after in situ surface preparation. In the AA5456, we examined the importance of UIT parameters such as peening amplitude and pin size. It was found that all combinations of UIT …