Global ETD Search
Search theses and dissertations gathered from participating repositories worldwide. Every result links back to the library that holds it. No account is needed.
Results
Showing 1 to 7 of 7 for “"AISI 321"”.
-
Dynamic impact response and corrosion behavior of coarse- and ultrafine-grained AISI 321 austenitic stainless steel
The excellent corrosion-resistance of metastable AISI 321 austenitic stainless steel makes it a choice material in the fabrication of nuclear and chemical plants, pressure vessels, automobile and aircraft components, etc. However, AISI 321 is characterized by low-yield strength and poor …
-
Loss of reactive elements during electroslag processing of iron-base alloys
… Remelting have been investigated in the alloys AISI 321 stainless steel and Maraging 300 steel which contain titanium and in 1409 Al steel, containing aluminium. Attention has been devoted to the influence of various melt parameters, i.e., the partial pressure of oxygen in the atmosphere, the …
-
ΜΕΛΕΤΗ ΤΗΣ ΟΞΕΙΔΩΣΗΣ ΜΕΤΑΛΛΙΚΩΝ ΕΠΙΦΑΝΕΙΩΝ ΣΕ ΔΙΑΒΡΩΤΙΚΕΣ ΑΤΜΟΣΦΑΙΡΕΣ ΜΕ ΤΗ ΒΟΗΘΕΙΑ ΠΥΡΗΝΙΚΩΝ ΜΕΘΟΔΩΝ ΕΠΙΦΑΝΕΙΑΚΗΣ ΑΝΑΛΥΣΗΣ
AUSTENITIC STAINLESS STEEL AISI 321 HAS BEEN IMPLANTED WITH AL, MG, AND ZR IONS RESPECTIVELY (IMPLANTATION ENERGY 40 KEV). THE SAMPLES HAVE BEEN OXIDIZED AT TEMPERATURES BETWEEN 450 AND 650 C FOR DIFFERENT PERIODS OF TIME. THE AL-IMPLANTED SAMPLES HAVE ALSO BEEN OXIDIZED IN AGGRESSIVE ENVIROMENT …
-
Oxidational and Tribological Studies of Austenitic Stainless steels under CO2-Based Environments
… is shown that the oxidational behaviour of the AISI 316 and 310 stainless steels follow Wagnerian parabolic kinetics. The behaviour of the AISI 321 stainless steels is shown to be non-parabolic and logarithmic in nature. Such behaviour is shown to be due to the replacement of the Cr203, oxide by …
-
Thermal fatigue of austenitic and duplex stainless steels
Thermal fatigue behavior of AISI 304L, AISI 316, AISI 321, and AISI 347 austenitic stainless steels as well as 3RE60 and ACX-100 duplex stainless steels was studied. Test samples were subjected to cyclic thermal transients in the temperature range 20 - 600°C. The resulting thermal strains were …
-
Stress corrosion crack growth rate measurement in high temperature water using small precracked bend specimens
… displacement. The studied materials were AISI 304 steel in sensitized, mill-annealed and irradiated conditions, AISI 316 in cold-worked condition, Inconel 82 and 182 weld metals in as-welded and thermally aged conditions and ferritic low activation steel F82H in tempered condition. The …
-
Optimalizace výroby volně kovaných výkovků za tepla z korozivzdorné austenitické oceli 08CH18N10T
Práce se zabývá výrobou a vlastnostmi volně kovaných výkovků za tepla z austenitické oceli 08Ch18N10T. Pozornost je věnována zejména vlivu technologie tváření za tepla a tepelného zpracování na výsledné mechanické vlastnosti při pokojové teplotě a teplotě 350 °C. Výsledky práce zahrnují hodnocení …