Design of an Accelerated Lifetime Tester for Industrial Gas Compressor Poppet Valves
… an analysis of the feasibility and design of a lifetime accelerator for poppet valves used in industrial gas compressors. First, we investigate the most common compressor and valve types. We then compare existing valve accelerators to determine the gap in current research on poppet valve …
-
Improving Reciprocating Compressor Valve Condition Monitoring via an Accelerated Lifetime Tester and Deep Learning
The goal of this research is to improve the current condition monitoring method for diagnosing reciprocating compressor valves. Leakage, seat wear, and spring degradation are three common valve faults that are seeded into all the valves of a Dresser-Rand ESH-1 dual-acting reciprocating compressor. …
-
Effects of accelerated lifetime test parameters and failure mechanisms on the reliability of electronic assemblies
This dissertation presents the results of accelerated reliability assessment methods employed on lead-free component board assemblies. Temperature cycling and mechanical shock tests are commonly used to assess the reliability of portable electronic products. Higher acceleration factors can be …
-
Development of procedures for performance measurements and lifetime testing of thin film photovoltaic devices
… and to find out potential failure mechanisms in accelerated lifetime testing. Thin film modules may increase their share of the market in the future. A-Si modules have been manufactured already for several years and CdTe and CIGS modules are shortly entering the market. However, there is a lack …
-
Characterization and reliability of vertical n-type gallium nitride Schottky contacts
… fabricated and subjected to high-current density accelerated lifetime tests to understand the physics of contact degradation and compare the reliability of different metallization types and process cleans. Tested Schottky metals included molybdenum, molybdenum-gold, and chromium-gold. Process …
-
Optinių medžiagų tarnavimo laiko lazerio spinduliuotės poveikyje vertinimas taikant pagreitinto ilgaamžiškumo testavimą /
The reliability and lifetime of optical materials under high-repetition-rate laser irradiation are critical factors in modern high-power laser systems. Classical Laser-Induced Damage Threshold (LIDT) testing methods, such as S-on-1 tests, are useful for evaluating optical materials under repeated …
-
Stability of thin-film CdTe solar cells with various back contacts
… barrier height as well as how they hold up under accelerated lifetime testing. Various degradation mechanisms, such as diffusion of species, drift within the built-in fields, and formations of various impurities/complexes on the surface and within the bulk were explored. The results of …
-
DEEP SUBMICRON CMOS VLSI CIRCUIT RELIABILITY MODELING, SIMULATION AND DESIGN
… wearout to circuit functionality. A set of accelerated lifetime models and failure equivalent circuit models are proposed for the most common MOSFET intrinsic wearout mechanisms, including Hot Carrier Injection (HCI), Time Dependent Dielectric Breakdown (TDDB), and Negative Bias Temperature …
-
An Investigation on Balance Switching Behavior in Credit Card Market
… distinct responses on the switchers' side. The accelerated lifetime model is adopted to capture the impact of the credit card debt and other relevant factors on the duration spell for holding an initial card. Last, we address the issue of unobserved heterogeneity in a structural Weibull-Gamma …
-
CHARACTERIZATION OF MEDICAL GRADE POLY-DIMETHYLSILOXANE AS ENCAPSULATION MATERIALS FOR IMPLANTABLE MICROELECTROMECHANICAL SYSTEMS
… Packaged interdigitated electrodes subjected to accelerated lifetime tests at 85°C in a saline environment had an average lifetime of 156.6 days, which exceeded the previous average lifetime by 22.3 days and suggests a packaging lifetime in the human body greater than 2 years and perhaps as long …
-
Roller-Cast Poly-Dimethylsiloxane as a Non-Hermetic Encapsulant for MEMS Packaging
… be used as an encapsulant for implantable MEMS. Accelerated lifetime studies were conducted at 40°C and 85°C in saline solution on sixteen samples each containing eight interdigitated electrode arrays and encapsulated with Dow Corning MDX4-4210 Biomedical Grade Elastomer. A custom environmental …
-
Uso de métodos bayesianos em testes de vida acelerados no controle da qualidade de produtos industriais
… level. We assume di¤erent distributions for the lifetimes of the units under a type II censoring mechanism and a general stress-response model that includes the usual accelerated life test models. Using a predictive density of a future observation, we present some criteria to be used by engineers …
-
Characterization, Reliability and Packaging for 300 °C MOSFET
… of SiC MOSFETs at 300 °C is tested with accelerated lifetime bias tests.
-
Defect spectroscopy on Cu(In,Ga)(S,Se) 2 -based heterojunction solar cells: role of the damp-heat treatment
The changes of defect characteristics induced by accelerated lifetime tests on solar cells of the heterostructure ZnO/CdS/Cu(In,Ga)(S,Se)2/Mo are investigated. The fill factor and open-circuit voltage of non-encapsulated test cells are reduced after prolonged damp-heat treatment in the laboratory, …
-
Anion Exchange Membrane Transport and Accelerated Testing Methods for CO2 Electrolyzers with Cu-based Electrocatalyst
… imidazolium-based (Dioxide Materials) membranes. Accelerated lifetime testing of CO2 reduction in MEA cells was conducted using galvanostatic stepping at 6-hour intervals to define a precipitation-free operating window. A “critical current density” was identified based on the cell potential and …
-
ARROW-Based On-Chip Alkali Vapor-Cell Development
… performance of these seals are quantified using accelerated lifetime tests combined with optical spectroscopy. Finally, the successful probing of the rubidium absorption spectrum, electromagnetically induced transparency, and slow light on the ARROW-based vapor-cell platform is reported.
-
Electrochemical Probing of Causes for Variation in Lifetime of Iridium-Tantalum Oxide Electrode Used in Copper Electrowinning
… effect of fluoride and metallic cations on the lifetime of IrO2-Ta2O5 coated Ti electrodes in sulfuric acid solutions has been investigated, and a degradation mechanism for IrO2-Ta2O5 coatings in the presence of fluoride has been proposed. Typical lifetime of the conductive ceramic coated anodes …
-
Reliability studies of ultra-small copper-plated through-package-vias in ultra-thin glass interposers
… models by demonstration of reliability through accelerated lifetime testing. To meet these objectives, this study focusses on four main tasks, a) mechanical modeling and design of TPVs in glass, b) fabrication of test vehicles for reliability characterization, c) reliability characterization of …