Global ETD Search

Search theses and dissertations gathered from participating repositories worldwide. Every result links back to the library that holds it. No account is needed.

Results

Showing 1 to 12 of 12 for “"Adhesion wear"”.

  1. Sustainable manufacturing metal cutting fluid – from mineral oil to vegetable oil

    … (FCS). The work is primarily focused on the tool wear, the surface roughness of the machined components, and the microstructure of the raw materials. The results show no significant difference between the wear mechanisms of the tools, predominant being the adhesion wear. The minimum tool wear on …

    chalmers Repository record for Sustainable manufacturing metal cutting fluid – from mineral oil to vegetable oil (opens in a new tab)

  2. Electrodeposited Metal Matrix Composites for Enhanced Corrosion Protection and Mechanical Properties

    … Ni and Cu-Ni matrix, an increase in strength, adhesion, wear and fracture toughness of the coating occurs, which leads to an increase corrosion resistance and longevity of the coating. These coatings were evaluated for composition and corrosion using many different types of instrumental and …

    unt Repository record for Electrodeposited Metal Matrix Composites for Enhanced Corrosion Protection and Mechanical Properties (opens in a new tab)

  3. Investigation on Improved Tapping Life in Automotive Die Cast Aluminum-Silicon Alloy Applications

    … alloy is challenging due to severe abrasion and adhesion wear of the tools. Form tapping is a common method for generating internal threads in engine blocks. It is usually a finishing process on a production line. An unexpected tap failure may lead to significant scrap and high rework costs. The …

    mcmaster Repository record for Investigation on Improved Tapping Life in Automotive Die Cast Aluminum-Silicon Alloy Applications (opens in a new tab)

  4. Development of TiAlN PVD Coating Systems for Machining of Compacted Graphite Iron (CGI)

    … which results in built-up edge formation and adhesion wear. This research attempts to address challenges associated with CGI turning by developing a TiAlN coating with a focus on thickness and low residual stress. The mentioned coating was developed using a new technology called super fine …

    mcmaster Repository record for Development of TiAlN PVD Coating Systems for Machining of Compacted Graphite Iron (CGI) (opens in a new tab)

  5. Wheel/Rail Contact Tribology: Characterising Low Adhesion Mechanisms and Friction Management Products

    Friction management and control of adhesion at the wheel/rail interface is vital for an efficient and cost effective railway network. The understanding of how the friction management products (grease and friction modifiers) work and effectively test these products is necessary to improve the …

    whiterose Download PDF for Wheel/Rail Contact Tribology: Characterising Low Adhesion Mechanisms and Friction Management Products (opens in a new tab)

  6. Modelling and simulation in tribology of complex interfaces

    … scales. Therefore, friction, lubrication and wear of materials are intrinsically highly multiphysics and multiscale phenomena. Several modelling and simulation tools have been developed in the last decades, always requiring a trade-off between the available computational power and the accurate …

    trento Repository record for Modelling and simulation in tribology of complex interfaces (opens in a new tab)

  7. ULTRATHIN CARBON-BASED OVERCOATS FOR EXTREMELY HIGH DENSITY MAGNETIC RECORDING

    … SPACING, WHEREAS IN TAPE DRIVES, ABRASIVE WEAR OF THE HEAD SENSORS LEADS TO HIGHER SPACING. THIS NECESSITATES THE USE OF ULTRATHIN OVERCOATS WHICH CAN MAINTAIN CORROSION AND TRIBOLOGICAL PROTECTION AT THE HEAD-MEDIA INTERFACE, AND IDEALLY POSSESS GOOD THERMAL STABILITY FOR HEAT-ASSISTED …

    nus Repository record for ULTRATHIN CARBON-BASED OVERCOATS FOR EXTREMELY HIGH DENSITY MAGNETIC RECORDING (opens in a new tab) Download file for ULTRATHIN CARBON-BASED OVERCOATS FOR EXTREMELY HIGH DENSITY MAGNETIC RECORDING (opens in a new tab)

  8. Hodnocení mechanismů opotřebení vstřikovacího ústrojí

    Bakalářská práce se zabývá popisem adhezního opotřebení na kontaktní ploše mezi Common railem a komponentou a vlivy, které ovlivňují vznik tohoto opotřebení. Cílem práce je seznámení se a pochopení fyzikálních principů adhezního opotřebení. Teoretická část práce se zabývá popisem vstřikovacího …

    brno-tech Repository record for Hodnocení mechanismů opotřebení vstřikovacího ústrojí (opens in a new tab)

  9. The development of a wear resistance aluminium bronzes (Cu-Al-Fe) coating

    … with Al > 14 wt. % are known to have high wear resistance and low friction coefficient against ferrous metals thus making it an ideal material for forming dies application. However, the use of these alloys has been restricted by the high cooling rate required to prevent embrittlement of the …

    soton Download PDF for The development of a wear resistance aluminium bronzes (Cu-Al-Fe) coating (opens in a new tab)

  10. An investigation on the mechanics of nanometric cutting for hard-brittle materials at elevated temperatures

    … on the cutting edge of the diamond tool, tool wear, defect-mediated plasticity and amorphization processes were calculated and analysed to quantify the differences in the cutting behaviour at different temperatures. Furthermore, In-situ high temperature nanoscratching (~500°C) of silicon wafer …

    strathclyde Repository record for An investigation on the mechanics of nanometric cutting for hard-brittle materials at elevated temperatures (opens in a new tab)

  11. Režimy opotřebení hliníkových slitin

    Tato práce se zabývá zkoumáním režimů opotřebení vybrané hliníkové slitiny za podmínek suchého tření. Cílem práce bylo vyhodnotit míru abrazivního a adhezivního opotřebení této slitiny z experimentů provedených na základě poznatků z rešeršní studie. Z výsledků měření byly sestaveny závislosti …

    brno-tech Repository record for Režimy opotřebení hliníkových slitin (opens in a new tab)

  12. Klasifikace a hodnocení opotřebení kolejnic

    Předložená bakalářská práce je zaměřena na opotřebení kolejnic. V práci se čtenář nejprve seznámí se základními pojmy kolejové dopravy jako je názvosloví kola a kolejnice, adheze, součinitel adheze, kontaktní plocha, skluz, trakční křivka a opotřebení. Následně jsou v práci popsány základní typy …

    brno-tech Repository record for Klasifikace a hodnocení opotřebení kolejnic (opens in a new tab)