Global ETD Search

Search theses and dissertations gathered from participating repositories worldwide. Every result links back to the library that holds it. No account is needed.

Results

Showing 1 to 20 of 45 for “"Adhesive Wear"”.

  1. The adhesive wear of modern and traditional engineering coatings

    The adhesive wear and frictional characteristics of modern and traditional engineering coatings have been investigated under conditions of constant load and sliding speed. The wear tests were carried out under dry sliding contact using the standard pin-on-disc wear testing equipment. The …

    aston Repository record for The adhesive wear of modern and traditional engineering coatings (opens in a new tab) Download PDF for The adhesive wear of modern and traditional engineering coatings (opens in a new tab)

  2. Adhesive Wear Phenomena in High Performance Polyaryletherketones (PAEK) Polymers

    Adhesive wear is one of the most difficult types to study and is especially challenging for polymers. Such wear processes involve the mutual sticking of surface asperities followed by removal of debris from the bulk. This differs from abrasive wear in which debris is formed due to the penetration …

    tamu Repository record for Adhesive Wear Phenomena in High Performance Polyaryletherketones (PAEK) Polymers (opens in a new tab)

  3. On developing a graphitic white iron for metal-to-metal wear systems

    … addressed heat dissipation issues related to the adhesive wear observed in metal-to-metal wear systems, by developing a graphitic white iron to increase thermal diffusivity of the wear components. One of the premium materials commonly used in current metal-to-metal wear systems is Fe15Mo18Cr and …

    must-thes Repository record for On developing a graphitic white iron for metal-to-metal wear systems (opens in a new tab)

  4. Tribological characteristics of coatings on aluminium and its alloys

    … to improve the resistance of the otherwise poor wear characteristics of aluminium. In recent years there has been an increasing interest in other treatments and coatings, on both aluminium and other base metals. The aim of this investigation is to explain the tribological performance and wear …

    brunel Repository record for Tribological characteristics of coatings on aluminium and its alloys (opens in a new tab)

  5. MACHINING WEAR OF CEMENTED CARBIDE INSERTS

    The present work investigates the machining wear of a mixed-carbide (A30; Sumitomo Electric) and a tungsten-carbide (F-grade; Toshiba Tungaloy) cemented carbide inserts when machining medium-carbon steel under different cutting conditions (cutting speed =50-300 m/min, feed rate =0.1-0.3 mm/rev ). …

    nus Repository record for MACHINING WEAR OF CEMENTED CARBIDE INSERTS (opens in a new tab) Download file for MACHINING WEAR OF CEMENTED CARBIDE INSERTS (opens in a new tab)

  6. Computational generation of wear maps for H13 tool steel in open die hot forging

    … productivity. The literature suggests that wear is responsible for 70%of failures in hot forging with abrasive and adhesive wear being the main failure modes in open die forging.Understanding the modes and mechanisms with which wear occurs on worn surfaces and contact faces is essential to …

    strathclyde Repository record for Computational generation of wear maps for H13 tool steel in open die hot forging (opens in a new tab)

  7. TRIBOLOGICAL AND WEAR PERFORMANCE OF PVD COATINGS FOR MACHINING SAF 2507 (UNS S32750) SUPER DUPLEX STAINLESS STEEL

    … strain hardening of the workpiece, intense adhesive wear and elevated temperatures within the cutting zone leading to rapid tool wear and poor machined surface integrity. This research pertains to the application of commercially available PVD coatings to minimize the detrimental effects when …

    mcmaster Repository record for TRIBOLOGICAL AND WEAR PERFORMANCE OF PVD COATINGS FOR MACHINING SAF 2507 (UNS S32750) SUPER DUPLEX STAINLESS STEEL (opens in a new tab)

  8. Mechanisms of Formation and Effects of Transition Metal Oxides in Silicon Nitride on Steel Dry Sliding Contacts

    … self-mated pairs, however the friction and wear behavior at high sliding speeds (>1 m/s) is not well understood. Previous studies at low sliding speeds (< 1 m/s) have found that the wear mechanisms change as a function of the operating parameters, e.g. atmosphere, sliding speed, load, and …

    unt Repository record for Mechanisms of Formation and Effects of Transition Metal Oxides in Silicon Nitride on Steel Dry Sliding Contacts (opens in a new tab)

  9. A novel method of detecting galling and other forms of catastrophic adhesion in tribotests

    … of a tribotest provides better detection of adhesive wear than the coefficient of friction alone. In this investigation an industrial tribotester (the Twist Compression Test) was instrumented with a variety of sensors to record: vibrations along two axes, acoustic emissions, electrical …

    laurentian Repository record for A novel method of detecting galling and other forms of catastrophic adhesion in tribotests (opens in a new tab)

  10. Tribo-corrosion maps for steels, titanium and titanium carbide materials

    … of change in sliding speeds and normal loads on wear behaviours were investigated for dry sliding conditions and tribo-corrosion maps were constructed with a tribo-system approach. The work was carried out in the following phases: In phase I, a fundamental study of the wear behaviour of two …

    strathclyde Repository record for Tribo-corrosion maps for steels, titanium and titanium carbide materials (opens in a new tab)

  11. Multiscale Analysis of Contact in Smooth and Rough Surfaces: Contact Characteristics and Tribo-Damage

    … studied is the rolling/sliding contact fatigue wear. In this research, the principles of continuum damage mechanics (CDM) are applied to predict the rolling/sliding contact fatigue crack initiation, and the effect of variable loading on the fatigue behavior of rolling contact with provision for …

    lsu-thes Repository record for Multiscale Analysis of Contact in Smooth and Rough Surfaces: Contact Characteristics and Tribo-Damage (opens in a new tab)

  12. Energy and Thermodynamically Based Approaches for Analysis of Damage in Contact Problems

    … damage are studied, namely crack nucleation and adhesive wear. The proposed methodology is primarily based on the laws of energy and thermodynamics, and as such offers great advantages by unifying the analysis of damage in a variety of contact configurations. Crack nucleation is the first damage …

    lsu-thes Repository record for Energy and Thermodynamically Based Approaches for Analysis of Damage in Contact Problems (opens in a new tab)

  13. Seizure and wear testing methodology

    <p>In this work the seizure as an adhesive wear has been discussed and analyzed The diffusion hypotheses is accepted as the seizure mechanism. It was determined that the surface of machine components, material properties, and contact stresses in sliding and loading zone are responsible for the …

    njit Repository record for Seizure and wear testing methodology (opens in a new tab)

  14. Deposition and comparative wear study of thin film coatings

    … hard but poorly adherent to the steel flats. A wear test rig designed, constructed and commissioned by another research student to carry out impact wear tests was adapted for adhesive wear tests. Progressive wear tests have been done on titanium carbide (5% titanium) coated, titanium nitride …

    dcu Download PDF for Deposition and comparative wear study of thin film coatings (opens in a new tab)

  15. A radio-tracer study of the effect of surface finish on the transfer of polychlorotrifluoroethylene sliding on mild steel

    … um - rms) surfaces was attributed to an abrasive wear mechanism. An apparent translation to adhesive wear was observed during later stages of transfer. This transition occurred much sooner with the polished surface than with the rough surfaces. This work also demonstrated that a radio-tracer …

    vt Repository record for A radio-tracer study of the effect of surface finish on the transfer of polychlorotrifluoroethylene sliding on mild steel (opens in a new tab)

  16. Infrared microscope studies of surface temperatures produced by friction with graphite-epoxy and carbon-PEEK composites

    … was seen to affect coefficient of friction and wear significantly; but surface temperature was very little affected by fiber orientation. In carbon-PEEK, fiber orientation affected the coefficient of friction, wear and surface temperatures significantly. Surface temperatures in both materials …

    vt Repository record for Infrared microscope studies of surface temperatures produced by friction with graphite-epoxy and carbon-PEEK composites (opens in a new tab)

  17. Cutting edge controlled wear of alumina inserts

    … the tool after the machining revealed that the wear mechanisms along the cutting edge and at the flank wear land are distinctively different. The cutting edge wears by plastic rounding, microspallation and sporadic edge chipping, while edge breakage may occur for tools of imperfect …

    nus Repository record for Cutting edge controlled wear of alumina inserts (opens in a new tab) Download file for Cutting edge controlled wear of alumina inserts (opens in a new tab)

  18. Improving the tribological and corrosion properties of Zr702 and Zircaloy-4 alloys by Ceramic Conversion Treatment

    … wide application of zirconium and its alloys, wear and corrosion of zirconium components are major issues for demanding applications. To this end, ceramic conversion (CC) treatments at different temperatures for varying time were therefore carried out on both Zr702 and Zircaloy-4 alloys. In …

    birmingham Download PDF for Improving the tribological and corrosion properties of Zr702 and Zircaloy-4 alloys by Ceramic Conversion Treatment (opens in a new tab)

  19. The development of a new test method for the evaluation of galling in OCTG connections

    Galling is a form of lubricant-related adhesive wear which occurs in threaded connections used in oil wells. The research reported herein involved the design of a test apparatus providing testing conditions and specimens closely simulating field conditions and the development of a new test method …

    ttu Repository record for The development of a new test method for the evaluation of galling in OCTG connections (opens in a new tab)

  20. Cutting mechanics of soft solids

    … to dissipation in the form of adhesion and wear. In the regime dominated by friction, cutting forces have a weaker sensitivity to blade sharpness. But, in the regime dominated by adhesion and shear damage/ wear, we have a linear dependence between cutting force and blade sharpness. By …

    ubc Repository record for Cutting mechanics of soft solids (opens in a new tab) Download PDF for Cutting mechanics of soft solids (opens in a new tab)

Page 1 of 3