Development of akaganéite (β-FeOOH, Cl) nanoparticles (Ak NPs), modified polyvinyl alcohol-Ak composites, and chitosan-Lemon Myrtle essential oil conjugates for green antioxidant and antimicrobial food packaging
… investigated the possibility of manufacturing akaganéite (β-FeOOH) nanoparticles (Ak NPs) utilizing extracts from winery wastes. Selected Ak NPs were added into biodegradable poly(vinyl alcohol) (PVA) and modified to improve physical properties. The role of Ak NPs in the films was investigated …
-
The Heat Capacity and Thermodynamic Properties of the Iron Oxides and Their Relation to the Mineral Core of the Iron Storage Protein Ferritin
… hematite (α-Fe2O3), nanocrystalline hematite, akaganéite (β-FeOOH), and lepidocrocite (γ-FeOOH) at temperatures as low as 0.5 K. These measurements were fit to theoretical functions at temperatures lower than 15 K, and the respective thermophysical properties of these materials are discussed. …
-
Mineral Magnetism of Environmental Reference Materials: Iron Oxyhydroxide Nanoparticles
… goethite, lepidocrocite, schwertmannite and akaganéite) are characterized using DC and AC magnetometry (cryogenic, room temperature), along with complementary analyses from Mössbauer spectroscopy (cryogenic, room temperature), powder X-ray diffraction and scanning electron microscopy. It was …
-
Apport de la spectroscopie infra-rouge in situ à l'étude des réactions de complexation à l'interface solide/solution
… et les (hydr)oxydes de fer (hématite, goethite, akaganéite et lépidocrocite). La spectroscopie infrarouge en réflexion totale atténuée (ATR-FTIR) est l’une des rares méthodes à permettre l’analyse in situ et l’observation des phénomènes de sorption en temps réel directement sur les surfaces. Il …
-
Carbon dioxide sequestration by mineral carbonation of iron-bearing minerals
… environment was goethite < lepidocrocite ≤ akaganéite. Overall, the results suggested that the carbonation of lepidocrocite and akaganéite with a CO2 waste stream containing ~1-5% H2S would sequester both the carbon and sulfide efficiently. Hence, it might be possible to develop a process …
-
Experimental and theoretical study of low-dimensional iron oxide nanoparticles and their nanocomposites
… in this thesis, including Goethite (α-FeOOH) and Akaganéite (β-FeOOH) one-dimensional (1-D) nanostructures with various aspect ratios under ambient conditions. These iron oxyhydroxide materials are thermally and chemically unstable, therefore can easily convert into hematite (α-Fe2O3) and …
-
Clay mineral catalysed oxidation of phenols
… chloride activated clay minerals should contain akaganéite (-FeOOH). Both newly prepared nanocomposites showed much greater rate enhancements than the aged (haematite) nanocomposite due to the lower stability and, probably, their higher degree of defects as full Ostwald ripening has not yet …
-
Carbon Isotopes of CO2 From Mineral Catalyzed Organic Oxidation Processes Under Martian Conditions
… hematite (Fe2O3), olivine ([Mg+2, Fe+2]2SiO4.), akaganéite (Fe3+O[OH,Cl]), and goethite (FeO(OH)). Experiments were conducted at 30 o C with carbon isotope measurements taken at reaction times of 1 hour, 4 hours, 24 hours, 72 hours, and 144 hours. The carbon isotope values obtained from the …
-
Templating of Metal Oxide and Oxhydroxides Nanoparticles in Surfactant Media
For industrial objectives, synthesis of akaganéite ffl-FeOOH) and goethite ((X-FeOOH) iron oxyhydroxides with nanometre particle size and acicular morphology was targeted. Both P & a-FeOOH particles were generated via forced hydrolysis of Fe" ions in acidic media. Templated syntheses of these …
-
Déchloruration des objets archéologiques ferreux par le processus de stabilisation subcritique. Caractérisations physico-chimiques des systèmes transformés
… de 150°C et d'hématite au-delà. L'étude de l'akaganéite, au taux de chlore variable, à différentes étapes de sa transformation, montre que le chlore adsorbé et une partie du chlore de structure est tout d'abord retiré. Ce phénomène, ajouté à une déshydroxylation sous l'effet de la température …