  1. Additive Manufacturing of L12 Precipitate Strengthened Nickel and Aluminum Alloys

    Metal Additive Manufacturing (AM) technologies have enabled the manufacturing of parts with complex geometries that were previously not feasible with conventional manufacturing. Unfortunately, many commercial engineering alloys (with the exception of alloys for welding) were designed with …

    epfl Repository record for Additive Manufacturing of L12 Precipitate Strengthened Nickel and Aluminum Alloys (opens in a new tab)