  1. Hot deformation processing and microstructural evolution of alloy 617

    Includes bibliographical references (pages 130-133).

    colo-mines Repository record for Hot deformation processing and microstructural evolution of alloy 617 (opens in a new tab)

  2. Tensile deformation, toughness and crack propagation studies of alloy 617

    Austenitic nickel-base Alloy 617 has been tested under tensile loading at temperatures relevant to both the Nuclear Hydrogen Initiative and the Next Generation Nuclear Plant programs of the U.S. Department of Energy. Two important metallurgical phenomena, namely dynamic strain aging (DSA) and yield …

    unlv Repository record for Tensile deformation, toughness and crack propagation studies of alloy 617 (opens in a new tab)

  3. High temperature creep-fatigue behavior of alloy 617 and alloy 230

    … applications. Currently, Ni-based superalloy alloy 617 (Inconel 617) and alloy 230 (Haynes 230) are considered as the leading metallic candidate materials for applications in the VHTR because of their favorable mechanical properties at elevated temperatures. The major damage mechanism …

    uiuc Repository record for High temperature creep-fatigue behavior of alloy 617 and alloy 230 (opens in a new tab)

  4. Mechanical and electrochemical properties of inconel alloy 617 after refurbishment through heat treatment

    … turbine nozzles. These pieces are made from an alloy that resist high temperature and thermal loading and being considerably expensive. The high operating temperature and thermal fatigue limit the lifetime of such component Consequently, the life extension of the alloy through sound …

    dcu

  5. High temperature aging study on long-term aged Alloy 617 and Alloy 230

    Alloy 617 and Alloy 230 are lead structural materials for next generation nuclear power plant (NGNP). Both alloys possess good corrosion resistance and exceptional high-temperature strength. In order to gain a better understanding of the high-temperature degradation process of these materials, …

    uiuc Repository record for High temperature aging study on long-term aged Alloy 617 and Alloy 230 (opens in a new tab)

  6. Time-dependent crack growth behavior of alloy 617 and alloy 230 at elevated temperatures

    Two Ni-base solid-solution-strengthened superalloys: INCONEL 617 and HAYNES 230 were studied to check sustained loading crack growth (SLCG) behavior at elevated temperatures appropriate for Next Generation Nuclear Plant (NGNP) applictaions with constant stress intensity factor (K max = 27.75 …

    unlv Repository record for Time-dependent crack growth behavior of alloy 617 and alloy 230 at elevated temperatures (opens in a new tab)

  7. Kinetic Property and SS 316/Alloy 617 Corrosion Study in Molten Chloride and Fluoride Salts

    … studies of structural materials (SS 316H and Alloy 617), including static corrosion and galvanic corrosion, in molten MgCl2-NaCl-KCl and/or NaF-KF-UF4-UF3 salts in a temperature range of 600 to 800C. The study applied the semi-differential (SD) analysis method and innovative fitting method …

    vt Repository record for Kinetic Property and SS 316/Alloy 617 Corrosion Study in Molten Chloride and Fluoride Salts (opens in a new tab)

  8. Effects of mechanical and metallurgical variables on creep, fracture toughness and crack growth behavior of Alloy 617

    Nickel base Alloy 617 has been identified to be a suitable structural material for heat exchanger applications in both hydrogen and electricity generation using nuclear heat. A maximum operating temperature of 950°C has been specified by department of energy (DOE) for both applications to achieve a …

    unlv Repository record for Effects of mechanical and metallurgical variables on creep, fracture toughness and crack growth behavior of Alloy 617 (opens in a new tab)

  9. Total hemispherical emissivity of very high temperature reactor (VHTR) candidate materials : Hastelloy X, Haynes 230, and Alloy 617

    … (from 0.178 at 600 K to 0.235 at 1375 K), and Alloy 617 (about 0.2 at 600 K to about 0.35 at 1275 K). Oxidation was found to increase emissivity, but as there is some oxidation of these materials used in the construction of VHTRs, this represents an essentially neutral finding in terms of the …

    missouri Repository record for Total hemispherical emissivity of very high temperature reactor (VHTR) candidate materials : Hastelloy X, Haynes 230, and Alloy 617 (opens in a new tab)

  10. Oxidation behavior of very high temperature reactor (VHTR) candidate materials: 316l stainless steel, Alloy 617, and Incoloy-800H

    High temperature nuclear reactors require alloys to perform well at temperatures around 1000 to 1400 K. The oxidation behavior of three high temperature reactor candidate materials, 316 L stainless steel, alloy 617, and Incoloy 800-H under different conditions were investigated in the present work. …

    missouri Repository record for Oxidation behavior of very high temperature reactor (VHTR) candidate materials: 316l stainless steel, Alloy 617, and Incoloy-800H (opens in a new tab)

  11. Calibration of empirical, semi-empirical, and physics-based material models for the prediction of creep and tensile behaviour of Alloy 617

    … in predicting the creep and tensile behaviour of Alloy 617 across three studies of increasing model fidelity. The first study calibrates twelve empirical models and applies symbolic regression (SR) to discover constitutive expressions for elevated-temperature creep behaviour. In general, the …

    unsw Repository record for Calibration of empirical, semi-empirical, and physics-based material models for the prediction of creep and tensile behaviour of Alloy 617 (opens in a new tab)

  12. High temperature creep behavior of Inconel 617 and Haynes 230

    … life of 60 years. Currently, Ni-based Inconel 617 (Alloy 617) and Haynes 230 (Alloy 230) are considered to be the leading metallic candidate materials for applications in the HTGR due to their favorable mechanical properties at high temperatures. In the present study, focus is placed on the …

    uiuc Repository record for High temperature creep behavior of Inconel 617 and Haynes 230 (opens in a new tab)

  13. Surface degradation and creep of Inconel 617 and Haynes 230 at high temperatures

    … an environmental degradation of high temperature alloys used for internals and heat exchangers. Depending on the impurity concentration and the temperature, the materials can undergo oxidation, carburization and decarburization, which can be detrimental to the mechanical behavior of the materials. …

    uiuc Repository record for Surface degradation and creep of Inconel 617 and Haynes 230 at high temperatures (opens in a new tab)

  14. Electrochemical studies of Inconel alloys 617 and 625 in molten PbCl2 : KCl mixture

    Behavior of Inconel alloys 617 and 625 in PbCl₂ -KCl molten salt system at three temperatures of 450, 550, and 650°C in air atmosphere and air-15%CO₂ atmosphere were compared using different electrochemical experiments. Electrochemical experiments performed included open circuit potential, …

    ubc Repository record for Electrochemical studies of Inconel alloys 617 and 625 in molten PbCl2 : KCl mixture (opens in a new tab)

  15. Microstructural evolution and mechanical behavior in nickel based alloys for very high temperature reactor

    … resistance. Among candidate materials, Alloy 617 and Alloy 230 are considered the most promising structural materials for the VHTR. In order to gain a better understanding of material performance during a high-temperature and long-term service life, various material tests and experiments …

    uiuc Repository record for Microstructural evolution and mechanical behavior in nickel based alloys for very high temperature reactor (opens in a new tab)

  16. HIGH TEMPERATURE OXIDATION PHENOMENA'S STUDY OF HIGH ALLOYED MATERIALS FOR POWER GENERATION PLANTS

    … some commercial and more recent SS and Ni based alloys for high temperature applications in order to verify their possible use either at operative conditions higher than conventional (temperature up to 900°C) or in different environment (oxygen, air, carburizing atmospheres). During the first …

    milano Repository record for HIGH TEMPERATURE OXIDATION PHENOMENA'S STUDY OF HIGH ALLOYED MATERIALS FOR POWER GENERATION PLANTS (opens in a new tab)

  17. Fatigue Analysis of 3D Printed 15-5 PH Stainless Steel - A Combined Numerical and Experimental Study

    … and the other one is the cyclic behavior of Alloy 617 under multi-amplitude strain loads using the static analysis method. Both validation models show a good correlation with the literature experimental data. Finally, after the validation, the finite element model is applied to the 15-5 PH …

    iupui Repository record for Fatigue Analysis of 3D Printed 15-5 PH Stainless Steel - A Combined Numerical and Experimental Study (opens in a new tab)