Showing 1 to 7 of 7 for “"Atomic hydrogen etching"”.
-
Scanning Tunneling Microscopy of Homo-Epitaxial Chemical Vapor Deposited Diamond (100) Films
Atomic resolution images of hot-tungsten filament chemical-vapor-deposition (CVD) grown epitaxial diamond (100) films obtained in ultrahigh vacuum (UHV) with a scanning tunneling microscope (STM) are reported. A (2x1) dimer surface reconstruction and amorphous atomic regions were observed on the …
-
Carbon nanosheets and carbon nanotubes by RF PECVD
… structure, have smooth surface morphologies and atomically thin edges, and are free-standing roughly vertical to substrate surfaces. CNS have a defective graphitic crystalline structure, and contain only C and H elements. Typical CNS growth parameters are 680??C substrate temperature, 40% CH4 in …
-
Comparative studies of 6-hydrogen-silicon carbide surface preparation.
… the goal of this research is the production of atomically flat surfaces having good stoichiometry, Si-C bonding, and crystallography and low oxygen contamination. Terraced 6H-SiC surfaces with 1.5 nm step heights are routinely produced by atmospheric pressure etching of as-received 6H-SiC in a …
-
Reflection High-Energy Electron Diffraction Studies of Indium Phosphide (100) and Growth on Indium and Indium Nitride on Silicon (100)
Study of the effects of atomic hydrogen exposure on structure and morphology of semiconductor surfaces is important for fundamental properties and applications. In this dissertation, the electron yield of a hydrogen-cleaned indium phosphide (InP) surface was measured and correlated to the …
-
GRAPHENE NANOSTUCTURING WITH THE HELIUM ION MICROSCOPE
… SPUTTERING, WE CAN UTILIZE THE DIFFERENTIAL ETCHING OF ATOMIC-HYDROGEN TO SELECTIVELY REMOVE THE DAMAGED AREA TO FABRICATE ARBITRARY NANOSCALE FEATURES ON GRAPHENE, WHILE MITIGATING THE BACKSCATTERED-ION-INDUCED DAMAGE. RAMAN CHARACTERIZATION SHOWS NO DAMAGE IS CAU
-
CHARACTERIZING LOW ENERGY ELECTRON-INDUCED REACTIONS WITH THIN FILMS, ADSORBATES, AND GAS PHASE MOLECULES
… dimensions and structure were induced using atomic hydrogen etching. Both characterization techniques were able to track the conversion of sp2-like carbon back into sp3-like carbon species in addition to providing etching rates for the films. The holy grail of nanoscale film fabrication is …