Global ETD Search
Search theses and dissertations gathered from participating repositories worldwide. Every result links back to the library that holds it. No account is needed.
Results
Showing 1 to 7 of 7 for “"Ball Bonding"”.
-
Mechanical and Tribological Aspects of Microelectronic Wire Bonding
… tribological mechanisms in microelectronic wire bonding. In particular, it focusses on the development and application of quantitative models of ultrasonic (US) friction and interfacial wear in wire bonding. Another objective of the thesis is to develop a low-stress Cu ball bonding process that …
-
Thermo-mechanical Simulation and Experimental Characterization of Power Semiconductor Devices' Packaging Processes
… di stress-deformazione durante il processo di ball-bonding. A tale scopo, è stato sviluppato un modello predittivo agli elementi finiti e sono state effettuate delle prove sperimentali per caratterizzare il processo di ball-bonding e validare il modello di calcolo. Un altro tema discusso è …
-
A Study of the Electrical Flame Off Process During Thermosonic Wire Bonding with Novel Wire Materials
Thermosonic ball bonding is the most popular method used to create electrical interconnects between integrated circuits (ICs) and substrates in the microelectronics industry. Traditionally gold (Au) wire is used, however with industry demands for lower costs and higher performance, novel wire …
-
Study of Au Ball Bond Mechanism and Reliability on Pd/Ni/Cu Substrate
Microelectronic wire bonding is a manufacturing process used to electrically connect integrated circuits with circuit boards or other substrates. Conventionally, balls are molten at the end of a Au bonding wire and subsequently bonded on Al metallization of a integrated circuit. However, Pd/Ni …
-
A Study on the Effect of Bond Stress and Process Temperature on Palladium Coated Silver Wire Bonds on Aluminum Metallization
… increasing price of gold has motivated the wire bonding industry to look for alternative bonding wire materials in the field of microelectronics packaging. A new candidate wire to replace gold is palladium coated silver wire. In this thesis, the effect of the two specific process parameters “bond …
-
A Surface Acoustic Wave Microsensor System for Thermogravimetric Measurements of Thin Polymer Films
… bond copper substrate operated to 425 °C. Gold ball bonding provided electrical connections to the SAW sensor that were used up to 400 °C. The system developed in this work was capable of measuring the mass loss due to water outgassing during cure thin polymer films to 2 % of total polymer mass …
-
Real-Time Interfacial FTIR-Electrochemical Investigation of Smart Passivating Film for Extended Lifetime of Copper Containing Microelectronic Devices
… Additionally, during the SnAgCu (SAC) solder ball bonding on the Cu wafer by mass reflow process, solder flux is used to reduce the native oxides on Cu and SAC solder ball. Post cleaning, residual amount of the solder flux corrodes the Cu wafer. Passivation coating is used as an organic solder …