Scanning Probe Microscopy and Oxidation of Silicon at Breakdown Voltages
… dot patterns were generated at several selected voltages and exposure times. In order to evaluate current efficiency, current was measured during line production. Oxide growth correlates with voltage until it reaches a saturation potential. This saturation appears to be associated with the onset …
-
Design and fabrication of AlGaN/GaN HEMTs with high breakdown voltages
… maximum potential out of them with regards to breakdown voltage. GaN based devices are able to breakdown at higher voltages compared to Si or GaAs due to its wider band gap (3.4 eV compared to 1.1 eV and 1.4 eV respectively) and although a lot of work has been invested into these devices over …
-
Dependence of Set, Reset and Breakdown Voltages of a MIM Resistive Memory Device on the Input Voltage Waveform
… and repeatedly by application of appropriate voltages. Although, there exists a large body of literature on this topic, many aspects of the CBRAM mechanisms and are still poorly understood. In the next paragraph, the aspects of CBRAM studied in this thesis are spelled out in more detail. CBRAM …
-
Calculating the dielectric strengths of insulating gas mixtures with the use of a multi-term Boltzmann equation method
… values of α_eff/N are applied to the Raether Breakdown Criterion to predict the DC breakdown voltages in these gases for uniform-field gaps between 1 and 100 cm. The use of the multi-term method and the criterion are discussed and justified. The calculations allow the characterization of what …
-
Įvairių metalų oksidų plonų sluoksnių, suformuotų atominių sluoksnių nusodinimo būdu, tyrimas /
… microscopy (AFM), X-ray diffraction (XRD) and breakdown voltages were measured. We investigated the effect of phase transformations induced by thermal annealing on the mechanical properties of our oxides. Oxides were annealed 10 minutes in a rapid thermal annealing (RTA) chamber to 400, 600, …
-
Studies of Electrical Breakdown of High-Pressure Ultra-Zero Air
… There are still uncertainties about the dominant breakdown mechanisms of ultra-zero air in the high-pressure regime. The classical equations for breakdown describing Paschen curves appear to not be valid above 500 psia. In order to better understand gas breakdown in the high-pressure regime, this …
-
SIMULATION OF SHORT CHANNEL AlGaN/GaN HEMTs
… semiconductor devices suffer from relatively low breakdown voltages precluding their operation at very high voltages and high powers. The vacuum tube based devices, however, suffer from the issues of high cost, large size and reliability issues. In recent years AlGaN/GaN HEMTs have demonstrated …
-
A Comprehensive Study of Safe-Operating-Area, Biasing Constraints, and Breakdown in Advanced SiGe HBTs
… thesis presents a comprehensive assessment of breakdown and operational voltage constraints in state-of-the-art silicon-germanium (SiGe) heterojunction bipolar transistor (HBT) BiCMOS technology. Technology scaling of SiGe HBTs for high frequency performance results on lower breakdown voltages, …
-
A Statistical Theory of Avalanche Breakdown in Silicon
A statistical theory of avalanche breakdown in silicon is presented, based on the conventional Boltzmann transport equation. The scattering mechanisms considered are impact ionization (electron-hole pair production), phonon emission and absorption, thermal generation and recombination. The …
-
SIMULATION AND DESIGN OF A SUBMICRON GATE-LENGTH AIGaN/GaN HEMT
… power amplification as the device offers high breakdown voltages (> 200 V) and high frequency operation (> 100 GHz). Recent devices have been able to achieve power densities as high as 10.5 W/mm at 40 GHz, cutoff frequencies (fT) of 163 GHz and maximum oscillation frequencies (fmax) of 230 GHz. …
-
Chemistry of the Trifluoromethoxy Group: From Nucleophilic Transfer Reagents to Fluorinated Sulfur Compounds
… behav-ior. Both compounds exhibit higher breakdown voltages compared to sulfur hexafluoride (SF6), with averaged relative breakdown voltages of 1.3 ± 0.2 for CF3OSO2F and 1.4 ± 0.2 for CF3OSF5, compared to 1.0 for SF6. This makes them promising candidates for dielectric appli-cations where …
-
Vertical gallium nitride schottky diodes for power switching applications.
… to date exhibit an ON-resistance (Ron) versus breakdown voltage much below theoretical predictions. Heteroepitaxial growth of GaN on substrates such as SiC, Si, and sapphire suffer from a high density of threading dislocations defects due to the mismatch in lattice constants and thermal …
-
A computerized system for the acquisition and alaysis of spark gap breakdown voltage data
… was assembled, primarily to deal with self- breakdown voltage data from one of several spark gap switches in the Texas Tech Plasma and Switching Laboratory. The system computer programs digitize the capacitor voltage waveform , find the peaks (which correspond to the self-breakdown voltages), …
-
An investigation of the V-I characteristics of electrical discharges in Argon and their dependence on gap length and pressure
… governing characteristics such as threshold and breakdown voltages, critical field strength and general shape of the voltage vs. current (V-I) curve, of each of the Townsend, coronal and arc phases of the discharge. These relations were fit to experimental data to obtain approximate values for …
-
Gas-solid interfaces stressed with HV impulses : surface flashover behaviour and control
… insulation as well as mechanical support. The breakdown/flashover voltage, at which a discharge process initiates across the gas-solid interface, is important in the design process, as it informs designers of specific threshold ‘failure’ voltages of the insulation system. In this thesis, a …
-
Gas discharges confined by metallic walls
… at one end of a metal segment is equal to the breakdown field. A relationship between the maximum length of a metal segment and the tube radius and pressure has been derived. The form of this relationship agrees qualitatively with experimental results. Measurements of the anode-cathode …
-
Power Module with Series-connected MOSFETs in Flip-chip Configuration
… power module with high efficiency and improved breakdown voltage, this thesis proposes a novel series-connected power MOSFETs module. Three IRF7832 MOSFETs (30 V breakdown voltage) in series are simulated in a chopper circuit. The drain-source voltage sharing in switching off-mode shows that the …
-
Background Reduction for Improved Sensitivity at the Enriched Xenon Observatory through advancements in Barium-Tagging Simulations, Prediction and Prevention of High-Voltage Breakdown in Liquid Xenon Time-Projection Chambers, and Event Classification using Ensemble Methods and Machine Learning
… EXO-200. First, a method for predicting breakdown voltages in dielectrics through pattern recognition is applied to a liquid xenon time projection chamber. A proposed extension to this method, which aims to incorporate the statistical variations of breakdown in liquid dielectrics, is …
-
Fabrication and electrical measurements of gallium nitride high electron mobility transistors
… The current-voltage characteristics and breakdown voltages of the HEMTs have been measured. The design, fabrication, and characterization of different devices were presented, as well as the measurements and discussion of devices under effects of heat treatment. Although the fabrication …
Page 1 of 8