  1. Temperature and silicon effects on tensile and corrosion behavior of chronium-molybdenum steel

    … specimens tested at 550°C exhibited ductile failures, brittle failures were seen at ambient temperature. However, all activated specimens revealed cleavage facets, indicating predominantly brittle failures.

    unlv Repository record for Temperature and silicon effects on tensile and corrosion behavior of chronium-molybdenum steel (opens in a new tab) Download PDF for Temperature and silicon effects on tensile and corrosion behavior of chronium-molybdenum steel (opens in a new tab)

  2. Stress Corrosion Cracking and Hydrogen Embrittlement of Martensitic Alloy EP-823

    … (SCC), localized corrosion, and hydrogen embrittlement (HE) susceptibility of martensitic Alloy EP-823 in neutral and acidic solutions at ambient and elevated temperatures. While no failures were observed in smooth specimens in the neutral solution, failures were noticed in the 90°C acidic …

    unlv Repository record for Stress Corrosion Cracking and Hydrogen Embrittlement of Martensitic Alloy EP-823 (opens in a new tab) Download PDF for Stress Corrosion Cracking and Hydrogen Embrittlement of Martensitic Alloy EP-823 (opens in a new tab)

  3. Stress corrosion cracking and hydrogen embrittlement of martensitic Alloy Ep -823

    … (SCC), localized corrosion, and hydrogen embrittlement (HE) susceptibility of martensitic Alloy EP-823 in neutral and acidic solutions at ambient and elevated temperatures. While no failures were observed in smooth specimens in the neutral solution, failures were noticed in the 90°C …

    unlv Repository record for Stress corrosion cracking and hydrogen embrittlement of martensitic Alloy Ep -823 (opens in a new tab) Download PDF for Stress corrosion cracking and hydrogen embrittlement of martensitic Alloy Ep -823 (opens in a new tab)

  4. Effect of beam size and FRP thickness on interfacial shear stress concentration and failure mode of FRP-strengthened beams

    … of beams using FRP is the potential brittle failures attributed to the interfacial stress concentrations at FRP-cut off points and at flexural cracks along the beam. In the present studies, three series of tests were conducted to investigate the interfacial shear stress concentration …

    nus Repository record for Effect of beam size and FRP thickness on interfacial shear stress concentration and failure mode of FRP-strengthened beams (opens in a new tab) Download file for Effect of beam size and FRP thickness on interfacial shear stress concentration and failure mode of FRP-strengthened beams (opens in a new tab)

  5. Embrittlement and Localized Corrosion in Alloy HT-9

    … of stress corrosion cracking (SCC), hydrogen embrittlement (HE) and localized corrosion susceptibility of Alloy HT -9 in neutral and acidic solutions at 30, 60 and 90°C. Constant-load and slow-strain-rate (SSR) testing techniques were used to evaluate the SCC and HE behavior of this alloy by …

    unlv Repository record for Embrittlement and Localized Corrosion in Alloy HT-9 (opens in a new tab) Download PDF for Embrittlement and Localized Corrosion in Alloy HT-9 (opens in a new tab)

  6. Metallurgical and corrosion characterization of a martensitic stainless steel as a function of silicon content

    … at 550°C, indicating enhanced ductility. No failures were observed in an acidic solution at constant-load irrespective of their Si content. The magnitude of all parameters obtained from the slow-strain-rate testing was gradually reduced with increasing temperature. However, T91 grade steel …

    unlv Repository record for Metallurgical and corrosion characterization of a martensitic stainless steel as a function of silicon content (opens in a new tab) Download PDF for Metallurgical and corrosion characterization of a martensitic stainless steel as a function of silicon content (opens in a new tab)

  7. High-temperature deformation and environment-induced degradation of Waspaloy

    … at 800°C, possibly due to the formation of brittle sigma phase. The cracking susceptibility of Waspaloy in an acidic solution was enhanced at a higher temperature when tested by the slow strain rate (SSR) technique. Slight variations in ductility parameters, true failure stress and time to …

    unlv Repository record for High-temperature deformation and environment-induced degradation of Waspaloy (opens in a new tab) Download PDF for High-temperature deformation and environment-induced degradation of Waspaloy (opens in a new tab)

  8. Ground control support consideration for pre-driven longwall recovery rooms.

    … result in excessive recovery room closures or brittle failures of the concrete crib systems. Three-Dimensional finite element models, combined with an underground test area, provided the critical components and design principles evaluated in a parametric study. The design methodology was …

    wvu Repository record for Ground control support consideration for pre-driven longwall recovery rooms. (opens in a new tab)

  9. Metallic Coatings as Peripheral Barriers to Diminish the Adverse Effects of Cathodic Protection on Prestressing Members

    … at extreme negative potentials leading to brittle cracks in high-strength steel wires. Herein is documented a history of the utilization of cathodic protection in reinforced and prestressed concrete. The adverse effects of the impressed current that may cause the failure of those systems …

    tamu Repository record for Metallic Coatings as Peripheral Barriers to Diminish the Adverse Effects of Cathodic Protection on Prestressing Members (opens in a new tab)

  10. Advanced signal processing for micro-seismic signal analysis

    Seismic events are brittle failures mainly attributed to the reduction in effective stress. They are typically nonstationary signals with small moments (known as microseismic events) and are frequently exposed to various types of ambient noise, resulting in low Signal-to-Noise Ratio (SNR) sensor …

    strathclyde Repository record for Advanced signal processing for micro-seismic signal analysis (opens in a new tab)

  11. Investigation of Wide Beam and Interfacial Shear Transfer in Reinforced Concrete Structures

    … loads, which are susceptible to undesirable and brittle failures. While many studies have been conducted to investigate the shear behavior of RC structural members and components to determine the critical design parameters, these tests are typically modeled after basic structural geometry and …

    must-thes Repository record for Investigation of Wide Beam and Interfacial Shear Transfer in Reinforced Concrete Structures (opens in a new tab)

  12. INVESTIGATING THE COMPATIBILITY OF BIODIESEL ON POLYETHYLENE THROUGH NONDESTRUCTIVE AND TRADITIONAL METHODS

    Being the most abundant cause of unexpected brittle failures of polymers, environmental stress cracking (ESC) is a major issue for the plastics industry, accounting for approximately 15-40% of all plastic part failures in service. ESC is an intriguing phenomenon that is not yet well understood, …

    mcmaster Repository record for INVESTIGATING THE COMPATIBILITY OF BIODIESEL ON POLYETHYLENE THROUGH NONDESTRUCTIVE AND TRADITIONAL METHODS (opens in a new tab)

  13. Strength and reliability analyses of glulam beam-column moment resisting connections

    … was developed to simulate both ductile and brittle failures in timber. Reductions in mechanical properties of timber near bolt holes were also accounted for. The numerical results were evaluated against the experimental moment–rotation curves, rotational performance parameters, and observed …

    ubc Repository record for Strength and reliability analyses of glulam beam-column moment resisting connections (opens in a new tab) Download PDF for Strength and reliability analyses of glulam beam-column moment resisting connections (opens in a new tab)

  14. Blast Performance of Reiforced Concrete Beams Constructed with High-Strength Concrete and High-Strength Reinforcement

    … high-strength concrete also shows potential for brittle failures under extreme blast pressures. The static results show that specimens with high-strength steel bars do not increase beam stiffness, but significantly increase peak load carrying capacity when compared to beams with the same ratio of …

    ottawa-retro Repository record for Blast Performance of Reiforced Concrete Beams Constructed with High-Strength Concrete and High-Strength Reinforcement (opens in a new tab)

  15. MECHANISMS OF STRAIN LOCALIZATION IN ULTRAFINE-GRAINED TUNGSTEN

    … experienced during launch generally result in brittle failures, while tungsten actually shows a high degree of plastic stability under the pressures and strain rates of terminal ballistics. By contrast, ultrafine-grained tungsten (100-1000 nm) has shown significant promise for achieving …

    jhu Repository record for MECHANISMS OF STRAIN LOCALIZATION IN ULTRAFINE-GRAINED TUNGSTEN (opens in a new tab)