Wet Etching Optical Fibers to Sub-micron Diameters for Sensing Application
… System. Second, we etch the TSMFs with 6:1 buffered HF solution to a controlled sub-micron size. During the etching process we monitor the fiber's progress by measuring the transmittance characteristics. The in situ measurements are made by connecting a laser at one fiber end and using a …
-
Control of stress in silicon nitride thin films
… interferometry measurements. The etch rate in buffered HF for films with refractive index 2.05 was 29A/min; as measured by JR spectroscopy these films had relatively low oxygen and hydrogen content. On increasing the film thickness from 300 A to 1900 A, the stress decreased from 4.45 x 10^9/m^2 …
-
Design and micro-fabrication of tantalum silicide cantilever beam threshold accelerometer
… variation caused by 8% uncertainty in the buffered HF etch rate of tantalum silicide. Some accelerometers were closed and opened 3 times without failure. The accelerometers tended to break after 3 times of operation and this was attributed to the welding of contacts. Centrifuge acceleration …
-
Wavelength Multiplexing of MEMS Pressure and Temperature Sensors Using Fiber Bragg Gratings and Arrayed Waveguide Gratings
… for etching the cavities in the glass wafer with buffered HF. A silicon wafer polished on both sides is then electrostatically bonded to the patterned glass wafer. Bulk etching techniques are used to thin the silicon wafer down to the desired diaphragm thickness, while the other side of the …
-
Mechanisms controlling silicon nitride growth by plasma-enhanced atomic layer deposition
… of 300-500 °C, low etch rates of 2 nm/min in buffered HF can be achieved. It was shown that the limiting factor in material quality is caused by redeposition of reaction products, which result in impurities in the film. This effect can be reduced by decreasing the residence time t of particles …
-
Beiträge zur Technologieentwicklung für die Erzeugung von Airgap - Strukturen in Metallisierungssystemen in integrierten Schaltkreisen
Die Arbeit beschreibt die Entwicklung und Evaluierung zweier neuartiger Technologien (Maske und Spacer) zur Erzeugung von Airgap-Strukturen in Mehrebenenmetallisierungen integrierter Schaltkreise. Ausgangspunkt der Arbeit bildet die Aufarbeitung der Thematik der low-k Materialien sowie der aus der …