Global ETD Search
Search theses and dissertations gathered from participating repositories worldwide. Every result links back to the library that holds it. No account is needed.
Results 1 to 20 of 35 for “"Bvid"”
-
Damage Control Measures in Composites: Focus on Damage Tolerance of Aerospace Structures
Barely Visible Impact Damage (BVID) in composite materials presents a stealthy yet significant risk to structural integrity, particularly challenging due to its elusive nature. The approach adopted here diverges from traditional methodologies, focusing on the novel application of Digital Image …
-
Residual Compressive Strength Prediction of Carbon/Epoxy Laminates Subjected to Low Velocity Impact Damage
… termed as barely visible impact damage (BVID). Detecting BVID is only possible by implementing nondestructive testing (NDT) techniques. Depending upon the support conditions, material system, laminate thickness, lay-up orientation, and impactor geometry, velocity, and hardness, the types …
-
Oblique angle pulse-echo ultrasound characterization of barely visible impact damage in polymer matrix composites
… meta-analysis of barely visible impact damage (BVID) in composites is conducted using data from the literature to understand the scope of the BVID problem. The analysis performed shows that delamination morphologies that have hidden delaminations (delaminations that are not detectable with …
-
Nondestructive inspection and quantification of carbon fiber laminates for barely visible impact damage and adhesive layer thickness measurements.
… contributions, barely visible impact damage (BVID) and adhesive layer thickness. An in-house drop weight impact device is used to produce BVID. Inherent to carbon fiber laminates, damage may exist beneath the impact surface that is undetectable by basic visual inspection. Traditional …
-
Hybrid composite sensors for improved visual inspection of impact damage
… example of this is barely visible impact damage (BVID) caused by out-of-plane loadings such as indentation and low-velocity impact that can considerably reduce the residual strength. Therefore, developing advanced visual inspection techniques is essential for early detection, localisation, and …
-
Damage Assessment and Strength Predictions in S-Glass/Epoxy Laminates Subjected to Low Energy Impact
… Also known as barely visible impact damage (BVID), this area of concentration focuses on the small-scale damage that may be very difficult to detect yet can be lethal. The primary emphasis of this research is to predict the residual compressive strength of a 16-ply laminate [(0°/±45°/90°)2]s …
-
Apport des méthodes vibro-acoustiques non linéaires à la détection et à la localisation d’endommagements dans les structures aéronautiques en matériaux composites.
… la suite d’impacts générant des défauts appelés BVID (Barely Visible Impact Damage), souvent invisibles en surface, et qui constituent un enjeu majeur. Provoqués par des chocs légers (grêle, débris ou chutes d’outils lors de la maintenance), ils peuvent évoluer vers des états critiques suite à …
-
Analysis and optimisation of postbuckled damage tolerant composite laminates
Barely Visible Impact Damage (BVID) can occur when laminated composite material is subject to impact, i.e. from runway debris or dropped tools, and may result in a significant reduction in the compressive strength of composite structures. A component containing BVID subjected to compression may …
-
Smart composite parts with multifunctional properties ready to fly
… e deteção de dano de impacto pouco visível (BVID) e a (2) capacidade de self-sensing dos CFRP para detetar BVID através de tomografia por impedância elétrica (EIT). Estes estudos foram conduzidos a nível laboratorial, em pequenas amostras de teste. A um segundo nível, este trabalho …
-
The Effects of Adhesive Quantity on Out-of-Plane Behaviour in Aluminum Honeycomb Panels
… the responses to barely-visible-impact-damage (BVID) in aluminum honeycomb sandwich panels in the out-of-plane direction with particular attention to the structural adhesive. The structural adhesive forms a fillet shape between the face-sheet and the aluminum core during the 120oC curing process …
-
Application of fracture mechanics to predict the growth of single and multi-level delaminations and disbonds in composite structures
… subjected to barely visible impact damage (BVID). The advantages of fracture mechanics-based methodologies to predict interlaminar failure in composite structures were identified, from which the crack tip element (CTE) approach and the virtual crack closure technique (VCCT) were selected for …
-
Experimental and numerical investigation of re-infiltration repair and Compression-After-Impact behaviour in thin-walled Carbon-Fibre-Reinforced-Plastic laminates with Barely-Visible-Impact-Damage
… frente a daños por impacto apenas visibles (BVID) y a la dificultad de recuperar el rendimiento estructural tras este tipo de eventos. Las técnicas de reparación tradicionales---como los parches adhesivos o atornillados---suelen ser invasivas, lentas y poco adecuadas para modos de daño …
-
Neural Network Prediction of Ultimate Compression After Impact Loads in Graphite-Epoxy Coupons from Ultrasonic C-Scan Images
… in order to create barely visible impact damage (BVID). The coupons were then scanned with an ultrasonic C-scan system to create an image of the damaged area. Each coupon was then compressed to failure to determine its ultimate compressive load. Numeric values for each pixel were determined from …
-
Impact fatigue damage in CFRP
… that result in barely visible impact damage (BVID) can threaten the laminate structural integrity and are hard to detect. The polymer matrix is also especially susceptible to environmental conditions such as humidity and moisture uptake. To date, no study is currently available on the combined …
-
Simulation and testing of low velocity impact damage and compression after impact for polymer matrix composite laminates.
Barely visible impact damage (BVID) from low-energy impacts may result in severe degradation of strength and stiffness of a polymer matrix composite laminate, yet the mechanisms of damage initiation and propagation are not fully understood. In this research, we propose a three-dimensional finite …
-
Impact Damage Modelling of Composite Laminates Using Statistical Methods to Assess Strength Reduction for Rapid Design
… reduction, barely visible impact damage (BVID) induced by low energyimpacts is a major concern to composite component manufacturers in the aerospace industry.Component testing to address this issue is both costly and time consuming. Thisresults in manufacturers oversizing components, which …
-
Analysis of After Impact Characteristics and Structural Optimization of CFRP Composite Plate
… may cause Barely Visible Impact Damage (BVID), which is one of the most common damage types and may result in a decrease in strength of the composite. The objectives of this research were (a) to identify the characteristics of a carbon/epoxy composite plate after low-velocity impact, (b) …
-
Interfacial Toughening Of Carbon Fiber Reinforced Polymer (CFRP) Matrix Composites Using MWCNTs/Epoxy Nanofiber Scaffolds
… 27%, respectively. Barely visible impact damage (BVID) energy improved considerably by up to 45%. The thermal and electrical conductivities were also increased considerably because of the highly conductive CNT networks present in between the CFRP layers. The newly introduced approach was able to …
-
Fluid-structure interaction of metallic and composite plates subjected to dynamic loading
… In some cases, barely visible impact damage (BVID) may occur, whicheven if detected by visual inspection would give no true indication to the severity of theinternal material degradation. Since many composites are being utilised in highperformance applications, it is important that the …
-
Guided wave propagation and scattering in anisotropic composite structures
… them vulnerable to barely visible impact damage (BVID) caused by low velocity impacts. Composite damage is multi-modal, consisting of fibre breakage, matrix cracking, and delaminations, with delaminations causing the most significant strength reduction. Guided ultrasonic waves, often generated …
Page 1 of 2