The effects of machining on the flexural strength of CAD-CAM materials
… machining modes on the flexural strength CAD-CAM restorative materials. MATERIALS AND METHODS: Four different CAD-CAM materials were used: VITA MARKII, VITA Enamic (VITA Zahnfabrik), Empress CAD, and e.max CAD (Ivoclar Vivadent). Rectangular bars for each material (except e.max CAD) were …
-
In- vitro Wear of Four CAD-CAM Materials in the UAB Wear Simulating Device
In- vitro Wear of Four CAD- CAM Materials in the UAB Wear Simulating Device RITIKA BANSAL MS IN CLINICAL DENTISTRY ABSTRACT Hybrid ceramic/polymer blocks represent a new category of CAD/CAM materials that do not require heat treatment following milled fabrication and limited clinically relevant …
-
CAD/CAM veneers: effect of material and thickness on color masking, bond strength and marginal fit
New CAD/CAM materials are becoming more accepted in veneer restoration. The objective is to investigate the margin integrity of CAD/CAM veneer, their color masking over dark backgrounds and shear bond strength (SBS) to resin cements. Materials and Methods: Four types of CAD/CAM materials shaded A2: …
-
Bond strength between veneer porcelains and CAD/CAM ceramic to CP titanium and evaluation of fracture load and effect of aging on low fusing porcelain fired over CP TI and CAD / CAM materials cemented onto CP TI
… porcelains fired over CP Titanium and a CAD/CAM ceramic cemented to CP Titanium. METHODS: Sixty-four bars of CP Titanium grade II (25±1x 3±0.5x 0.5±0.05 mm) were divided randomly into four groups: Group 1: Titankeramik (Vita Zahnfabrik), Group 2: Triceram (Dentaurum), Group 3: Initial Ti …
-
Mechanical properties of interim restorative materials: conventional vs. CAD/CAM
… and flexural modulus of conventional and CAD/CAM provisional crown and bridge restorative materials. Six provisional crown and bridge materials were selected for this study. Three conventional resins: Jet Set 4 (Lang), Luxatemp (DMG), and Protemp Plus (3M ESPE); and three CAD/CAM …
-
Influence of adhesive technique and thermomechanical fatigue on the fracture strength of minimally invasive CAD/CAM occlusal veneers
With the development of new CAD/CAM restorative dental materials, limited data regarding their survival rate and fracture strength are available when they are used as occlusal veneers. Therfore, These materials could be evaluated under conditions similar to those of the oral environment before …
-
Adhesion and Microleakage of CAD/CAM Crowns Using Self-adhesive Resin Cements
Ceramic and composite resin CAD/CAM restorations were introduced as indirect restorative materials that combine high esthetics and superior mechanical properties. However, an important requirement for successful function of these restorations is adequate adhesion between the restoration and tooth …
-
Static and cyclic loading effects on fracture toughness of contemporary CAD/CAM restorative materials
… (K1C) and microhardness of dental restorative CAD/CAM materials. MATERIAL AND METHODS: Five commercially available CAD/CAM restorative materials were included in this study: Lava™ Ultimate Restorative (3M ESPE), IPS Empress® CAD (Ivoclar Vivadent), Enamic® (VITA), IPS e.max® CAD (Ivoclar …
-
Μελέτη μηχανικών, οπτικών και επιφανειακών ιδιοτήτων πολυμερών υλικών για προσθετικές αποκαταστάσεις ψηφιακής σχεδίασης και κατασκευής (CAD/CAM)
… and mechanical characterization of contemporary CAD/CAM resin-based composite (RBC) materials used for prosthetic restorations and the assessment of the effect of aging procedures on color, gloss and surface roughness of these materials. Materials and Methods: Six CAD/CAM RBC materials [Brilliant …
-
In vitro Investigation of Mechanical Properties of Latest-Generation CAD-CAM Composites
… Design/Computer-Aided Manufacturing (CAD-CAM) materials for dental prostheses: fractures and debonding from titanium implant abutment (Ti-base). Specifically, the work focused on evaluating the mechanical performance of latest generation CAD-CAM composites compared to established …
-
Evaluation of the fracture resistance of posterior monolithic CAD/CAM crowns restoring custom-made implant abutments after artificial aging
… effect of using different commercially available CAD/CAM materials for fabrication of molar crowns on the fracture strength of custom-made abutments after dynamic loading and thermal cycling. A total of 88 identical custom-made CAD/CAM abutments milled out of titanium, zirconia, lithium disilicate …
-
Properties and Applications of Polymer-Infiltrated Ceramic Network Materials
Computer-aided design and manufacturing (CAD-CAM) materials are gaining popularity in the field of restorative dentistry. Among recently developed materials are polymerinfiltrated ceramic network (PICN) materials, a sub-class of CAD-CAM composites, comprised of 75 vol% sintered glass-ceramic …
-
Analysis of machining damage to CAD/CAM block materials characterized by changes in surface roughness, edge chipping, and flexural strength
… roughness, the edge chipping of different CAD/CAM bur milled dental materials (bar and crown design of 1.0mm and 1.5mm thickness), correlate the effect of machining damage on the material strength, compare the flexural strength of bur milled versus sectioned CAD/CAM blocks and evaluate the …
-
Experimental 4-step braided glass fiber reinforced composite for dental CAD/CAM applications
… has lead to rapid expansion of new dental materials. A new product from Shofu (Shofu, Japan), TRINIA CAD/CAM blocks and pucks, offers an alternative to the existing resin composite CAD/CAM materials. The claimed mechanical properties of TRINA provide merit to further research and …
-
Comparison of adherence of self-cured adhesive resin cement to lithium disilicate ceramics and ceramic resin composites using fracture mechanics
… Ultimate, 3M ESPE) and recently introduced CAD/CAM materials : two ceramic resin composites (Lava Ultimate – 3M ESPE and Enamic – Vita-Zahnfabrik) and a ceramic (IPS e.max – Ivoclar-Vivadent). Materials and Methods : Sixty specimens were prepared from each e.max and Enamic, and 120 specimens …
-
Edge Chipping Resistance and Flexural Strength of Polymer Infiltrated Ceramic Network and Resin Nano Ceramic Materials
… and a resin nano ceramic (RNC) restorative materials for Computer Aided Design/Computer Aided Manufacturing (CAD/CAM) applications recently became commercially available. Little independent evidence regarding their mechanical properties exists to facilitate material selection process. The …
-
Biomechanical considerations for endocrowns in restoring endodontically treated teeth
… to evaluate the effect of using different dental CAD/CAM materials on the biomechanical behaviour of endodontically treated teeth restored with a new technique named endocrown. Methodology: In this study, a thorough comparison of endocrown restorations fabricated from new types of all-ceramic, …
-
Fatigue behaviour and failure modes of monolithic CAD/CAM hybrid-ceramic and all-ceramic posterior crown restorations
… behaviour and failure modes of a novel CAD/CAM experimental hybrid-ceramic material and to compare it with two monolithic all-ceramic CAD/CAM materials (Vita Mark II and IPS e.max CAD) in a standardized molar crown model. The correlation between fracture load, cement thickness, crack …
-
Evaluation of certai influence the durab n factors that ility of CAD/CAM restorations
… of the factors that influence the failure CAD/CAM ceramic dental restorations. Objectives: To analyse the failure of CAD/CAM ceramic crowns the following investigations were carried out: (1) micro-CT analysis of the tooth-crown marginal gaps on extracted teeth; (2) evaluation of the failure …