Showing 1 to 10 of 10 for “"Celtra Duo"”.
-
Marginal gap and internal fit of CEREC e.max and Celtra Duo crowns
… as well as marginal chipping of e.max (EM) and Celtra Duo (CD) all-ceramic crowns fabricated using chairside economical restoration of esthetic ceramics (CEREC) system. Material and Methods: Tooth # 15 was prepared for an all-ceramic crown on an ivorine typodont. A total of 15 CD and 15 EM …
-
Comparison Of Vickers Hardness Between Dental Ceramics And Hybrid Materials
… CAD), lithium silicate reinforced with zirconia (Celtra Duo CAD), dual polymer hybrid ceramic (Vita Enamic) and resin ceramic hybrid (VarseoSmile Crown Plus). Vickers indenter (Wilson VH3100, Buehler) was used to create 6 pyramid-shaped indentations on each specimen and surface hardness was then …
-
Mechanical and optical properties of machinable and pressable glass ceramic
… investigated; IPS e.max CAD, IPS e.max Press, Celtra Duo, and Celtra Press. For each material 87 disc-shaped specimens, 2 mm in thickness and 12 mm in diameter were fabricated. Specimens were divided into 3 groups (n=29) as no treatment, polishing, and glazing group. Five samples from each …
-
Edge-Chipping and Translucency Comparison Among Lithium Silicate-Based Ceramics
… glass-ceramic materials, Vita Suprinity and Celtra Duo, were prepared and tested (n=20 specimens/group). Specimens (14 x 12 x 1.5 mm) were sectioned from commercially available chairside computer-aided design/computer-aided manufacturing (CAD-CAM) blocks, fired (if indicated), ground, and …
-
In- vitro Wear of Four CAD-CAM Materials in the UAB Wear Simulating Device
… 2 reference glass ceramics (IPS e.max and Celtra Duo), and 1 reference composite material (Paradigm MZ100). Methods: Flexural strength specimens (n=10) (2.5 Ã 2.5 Ã 16 mm) were prepared using a sectioning saw. After 24 hours in aqueous storage (37ºC), the specimens were loaded to failure …
-
Assessment of the bond strength between resin cement and lithium disilicate based glass ceramics with different chemical composition and surface treatments
… four LDGC products (e.max CAD, Vita Suprinity, Celtra Duo, n!ce) were analyzed using X-ray photoelectron spectroscopy (XPS). In addition, scanning electron microscopy (SEM) was used to analyze the microstructure of LDGC. Part II: The effect of different surface treatments on the micromorphology …
-
Cimentação adesiva de cerâmicas vítreas para CAD/CAM: efeito do tipo de sistema adesivo e do envelhecimento em longo prazo na resistência de união ao cimento resinoso
… ceramics to resin cement. Lithium silicate (SL - Celtra Duo, Dentsply Sirona), feldspathic (FD - Vita Mark II, VITA Zahnfabrik) and polymerinfiltrated ceramic (PIC - Vita Enamic, VITA Zahnfabrik) blocks were sectioned (N=96, 10 x 12 x 2 mm), included and randomly divided into 24 groups according …
-
Monolithische CAD/CAM-Glaskeramik: Bruchlastergebnisse glasierter versus polierter Molarenkronen
… 40 identische monolithische ZLS-Kronen (Celtra Duo, Dentsply, Konstanz, D) zur Versorgung eines dentinanalogen Kompositstumpfes in Regio 46 mit Hilfe der CAD/CAM-Technologie (Cerec inLab SW 4.0, Bensheim, D) als Prüfkörper erstellt. Diese wurden in zwei Gruppen aufgeteilt. Eine Gruppe von …
-
The effect of repetitive firing cycles on physical and optical properties of zirconia reinforced lithium silicate ceramics
… Vita Suprinity’s® translucency, but not that of Celtra® Duo, which showed no significant difference. All materials of greater thickness exhibited less translucency, and e.max® CAD had the highest mean light transmission; however, it was not significantly different than Celtra® Duo. Repetitive …
-
Light transmission and wear of translucent zirconia after conventional and fast sintering cycle
… The mean (s.d.) flat surface wear (mm3) of Celtra Duo against conventional and fast sintered Lava Esthetic cusp was 4.01 (0.74) and 3.94 (0.83), respectively. The mean (s.d.) flat surface wear (mm3) of e.max CAD LT against conventional and fast sintered Lava Esthetic cusp was 1.76 (0.23) and …