Results 1 to 14 of 14 for “"Chromia scale"”

  1. Effect of SO2 on corrosion behaviour of Fe-Cr-(Mn, Si) and Fe-Cr-Ni-(Mn, Si) alloys in CO2-H2O gases at high temperatures

    … Fe-Cr alloys, which however, form a protective chromia scale in air/O2 gas. In coal combustion process, sulphur is unavoidable which could affect the corrosion behaviour of material in CO2-rich gas atmosphere. However, the kinetics and mechanism of sulphur on CO2 corrosion is still unknown. This …

    unsw Repository record for Effect of SO2 on corrosion behaviour of Fe-Cr-(Mn, Si) and Fe-Cr-Ni-(Mn, Si) alloys in CO2-H2O gases at high temperatures (opens in a new tab)

  2. Kinetics of carbide dissolution in chromium + molybdenum steels during oxidation

    … then pre-oxidised in H2+10%H2O to grow a purely chromia scale. In this low oxygen partial pressure environment, carbides in the alloy's sub-surface dissolved and formed a ferritic precipitate-free zone. The precipitate dissolution model developed by previous investigators was then tested and …

    unsw Repository record for Kinetics of carbide dissolution in chromium + molybdenum steels during oxidation (opens in a new tab)

  3. Effect of Sulphate and Coal Ash on High-Temperature Corrosion of Chromia-forming Alloys in Wet CO2 Gas

    … of sulphate salt on the corrosion behaviour of chromia forming alloys (Fe- and Ni-based alloys) was determined at 650 and 750 °C in a gas Ar-60CO2-20H2O simulating oxyfuel combustion atmosphere. Then, the effect of ash particles was further investigated by adding different contents of ash (10, …

    unsw Repository record for Effect of Sulphate and Coal Ash on High-Temperature Corrosion of Chromia-forming Alloys in Wet CO2 Gas (opens in a new tab)

  4. Corrosion behaviour of Ni-Cr-(Fe) alloys in dry and wet CO2 at high temperatures

    … 650‒800 °C. In dry CO2 gas, multilayered oxide scales were formed on Ni-Cr alloys with low Cr concentrations. Increasing Cr level, the protection of corrosion scales was gradually developed. Elevating temperature accelerated the corrosion kinetics of low Cr alloys, but significantly reduced the …

    unsw Repository record for Corrosion behaviour of Ni-Cr-(Fe) alloys in dry and wet CO2 at high temperatures (opens in a new tab)

  5. Chlorine-induced Corrosion of Chromia-forming Alloys Relevant to Incineration Process

    … Cr2O3 formation, leading a protective chromia scale when Cr concentration reached a critical value. This critical value was found to be increased in the presence of HCl. Increasing temperature enhanced corrosion kinetics. The accelerating effect of HCl was attributed to the metal …

    unsw Repository record for Chlorine-induced Corrosion of Chromia-forming Alloys Relevant to Incineration Process (opens in a new tab)

  6. The oxidation damage of Ni-based superalloy, RR1000, with different surface modifications and the role of oxidation in fatigue crack initiation

    … measurements. The oxide comprises of an external chromia scale with isolated grains of TiO\(_2\) on the outer surface. Sub-surface internal alumina is present, beneath which the presence of TiN occurs (at higher temperatures >800\(^o\)C), all contained within a ɣ' denuded zone. The chromia …

    birmingham Repository record for The oxidation damage of Ni-based superalloy, RR1000, with different surface modifications and the role of oxidation in fatigue crack initiation (opens in a new tab)

  7. Effect of Cyclic Reaction on Corrosion Behaviour of Chromium-Containing Alloys in CO2-rich Gases at 650C

    … conditions by forming a thin protective alumina scale. However, alloys F321, F316L, 800H and 304SS all formed thick multi-layered oxides with external iron-rich oxides and internal spinel oxides in all reaction conditions. Alloys 310SS and 253MA, behaved protective in isothermal reaction …

    unsw Repository record for Effect of Cyclic Reaction on Corrosion Behaviour of Chromium-Containing Alloys in CO2-rich Gases at 650C (opens in a new tab)

  8. Structure and Electrical Conductivity of Mn-based Spinels Used as Solid Oxide Fuel Cell Interconnect Coatings

    … (650<sup>o</sup>C--800<sup>o</sup>C), the chromia scale growth on the interconnect surface and chromium poisoning of cathode can lead to performance degradation of the whole cell. A spinel coating can be effective for blocking chromium outward diffusion to overcome this issue. In this …

    mcmaster Repository record for Structure and Electrical Conductivity of Mn-based Spinels Used as Solid Oxide Fuel Cell Interconnect Coatings (opens in a new tab)

  9. Steam effects on cyclic oxidation of chromia forming alloys

    … In isothermal oxidation at 700°C, a protective chromia layer was formed in dry oxygen for Fe9Cr. Alloys with Cr≥17% formed protective chromia layers in all gas mixtures. In thermal cyclic oxidation, at high Po2, the 9%Cr alloy exhibited breakaway oxidation at an early stage of the reaction at …

    unsw Repository record for Steam effects on cyclic oxidation of chromia forming alloys (opens in a new tab)

  10. Carburisation and metal dusting of nano-crystalline nickel-chromium alloys

    … appeared little attack due to the formation of chromia scales on the surface and along the interfaces among the columns. Both alloys formed other reaction products inside of columnar coating scales, with fine graphite deposits for Ni-10Cr and relatively large Cr7C3 precipitates for Ni-20Cr. For …

    unsw Repository record for Carburisation and metal dusting of nano-crystalline nickel-chromium alloys (opens in a new tab)

  11. Development and breakdown of oxide scales on iron-25 percent chromium-20 percent nickel alloys in atmospheres containing oxygen and sulfur

    … FCC alloy, it takes a long time for a complete chromia layer to become established at 700°C. Even after long exposure times the oxide scale still contains additional Fe-rich oxide phases. A chromia scale forms more rapidly on the Fe-25%Cr-20%Ni alloy at 900°C, although there are still areas …

    ohiolink Repository record for Development and breakdown of oxide scales on iron-25 percent chromium-20 percent nickel alloys in atmospheres containing oxygen and sulfur (opens in a new tab)

  12. Modelling and experiments of metal interconnect degradation in solid oxide fuel cells

    … change over time due to the formation of a chromia scale and subsequent volatilisation of chromium gaseous species. As the operational temperature of SOFC systems is continuously reduced, the present thesis reports research aimed at investigating the behaviour of chromium in stainless …

    birmingham Repository record for Modelling and experiments of metal interconnect degradation in solid oxide fuel cells (opens in a new tab)

  13. EFFECT OF ADVANCED MANUFACTURING PROCESS ON THE HIGH TEMPERATURE OXIDATION BEHAVIOR OF SUPERALLOYS

    … on HTO behavior depends on the type of alloy. Chromia forming superalloy H230 shows improvement in HTO behavior by utilizing the RAA process. However, the alumina forming AFA25’s HTO behavior deteriorates with the RAA process. The RAA process leads to the formation of a three-zone diffusion …

    ohiolink Repository record for EFFECT OF ADVANCED MANUFACTURING PROCESS ON THE HIGH TEMPERATURE OXIDATION BEHAVIOR OF SUPERALLOYS (opens in a new tab)