Influence of Phase Transformations on the Residual Stress Evolution and Cracking Tendency in CM247LC Nickel-base Superalloy
… melting at the grain boundary as well as constitutional liquation of the MC carbide particles is identified as a source of cracking. Thiscracking tendency is correlated to the crystallographic misorientation between adjacent grains. It is found that cracking only occurs at grain boundaries …
-
Characterisation of mechanical responses of nickel based superalloys to deformation at high strain rates and high temperatures
… of strengthening γ' precipitates, but also from constitutional liquation of the remaining γ' precipitates. As the deformation continues, dynamic recrystallisation of grains occurs in the microstructure, which softens the material. This process occurs at a critical strain, which decreases with …
-
Evaluation of the Potential for Weld-Related Cracking in Cast 20Cr-32Ni-1Nb Heat-Resistant Stainless Steel
… exposure this alloy exhibits problems with liquation cracking in the base metal heat-affected zone (HAZ) during repair welding. In the work presented herein, two heats of material from centrifugally-cast manifold components were evaluated to quantify the potential susceptibility to HAZ …
-
Evaluation of the hot cracking sensitivity of 316 NG, 347 and 304 stainless steels using the hot ductility test and the modified subscale varestraint test
… at the ZDT is related to the grain boundary liquation, there are two types of secondary cracks; first one is along the grain boundary which is roughly parallel to the fracture surface, second one is along the preferentially melted segregation bands. In AISI 347, the second type of secondary …
-
Heat Affected Zone Cracking of Allvac 718Plus Superalloy during High Power Beam Welding and Post-weld Heat Treatment
… superalloy was associated with grain boundary liquation. However, despite a more extensive liquation of grain boundaries and grain interior in the HAZ of high heat input welds, no cracking occurred. This was attributed to the combination of lower welding stresses generated during cooling, and …