Global ETD Search
Search theses and dissertations gathered from participating repositories worldwide. Every result links back to the library that holds it. No account is needed.
Results 1 to 11 of 11 for “"Cr7C3"”
-
Electronic and Magnetic Properties of MAX Phase (Cr1-xGdx)2AlC and Er3AlC Alloy
… parent compound Cr2AlC exhibits a side phase of Cr7C3. The substituted samples were found to have secondary phases of Cr7C3 and GdCr3.5Al8.5 which slightly increase on increasing substitution of Cr3+ by Gd3+. The change of the concentration of Gadolinium does not have any real effect on the …
-
Lazer kaplama yöntemi kullanılarak üretilen Mo katkılı stellite 21 alaşımı kaplamaların aşınma ve oksidasyon davranışlarının incelenmesi
… artığı görülmüştür. Ayrıca Mo ilavesinin Cr7C3 ve Cr23C6 gibi karbür fazlarının oluşumuna da katkı sağladığı görülmüştür. Mekanik karakterizasyon çalışmaları sonucunda alaşımların sertliklerinin %Mo ilavesi ile orantılı olarak artığı ve bu durumun oda sıcaklığındaki aşınma dayanımını …
-
Microstructure evolution and optimization of the tempering heat treatment of a medium-carbon low-alloy steel
… carbides tend to be rich in chromium and mostly Cr7C3 and Cr23C6 carbides were identified. Hardness increase was observed during carbides precipitation, while it decreased when carbide coarsening started.
-
Etude de l’élaboration de revêtements autocicatrisants pour le développement de matériaux robustes en condition nucléaire
… une couche intermédiaire résiduelle de carbure Cr7C3 servant de réservoir de Cr jusqu'à complète oxydation. Ces résultats ont également montré la perte d'une partie du réservoir d'Al par diffusion dans les alliages Zr. Une architecture multicouche a été développée pour limiter cette diffusion et …
-
Recubrimientos de carburos ternarios depositados con la técnica TRD
… (NbC), de vanadio (V8C7) y de Cromo (Cr23C6, Cr7C3) sobre dos aceros para herramientas: AISI D2 y AISI H13, utilizando el proceso de deposición por difusión termorreactiva (TRD). El tratamiento fue realizado en baños de sales compuestos por bórax fundido, aluminio y las respectivas …
-
Carburisation and metal dusting of nano-crystalline nickel-chromium alloys
… deposits for Ni-10Cr and relatively large Cr7C3 precipitates for Ni-20Cr. For electroplated samples, the rates of weight gain performed a slow increase first, followed by an accelerated increase. Pre-oxidation before dusting significantly improved the resistance of alloy against …
-
Caracterización, evolución de microestructura y propiedades mecánicas de aceros austeníticos resistentes a altas temperaturas
… una red de carburos primarios de tipo NbC y Cr7C3 en el caso de la ET45 micro, y de tipo NbC y Cr23C6 en el caso de la aleación HP40-Nb. En ambas aleaciones, se observa una zona de deplexión libre de precipitados secundarios adyacente a la red de carburos eutécticos primarios y que presenta …
-
ALUMINA-FORMING NANOLAMINATED CARBIDES AND BORIDES
… Cr powders (such as Fe) as well as absence of Cr7C3 sub-layer leads to the wrinkling of alumina scale and its premature spallation. Although MoAlB has been proposed as good candidate material for high temperature applications because it forms stable and protective alumina oxide layer, its …
-
Cr2AlC-Phasenentstehung und Eigenspannungsentwicklung in Cr-Al-C-Dünnschichten unter thermischer Belastung
… Cr2AlC-Phasenentstehung primär aus Cr2AlC mit Cr7C3-Anteilen, die von der Elementzusammensetzung der Schichten im abgeschiedenen Zustand bestimmt wurden. So zeigten die HPPMS-Schichten und ehemaligen amorphen Bereiche erhöhte Cr7C3-Gehalte. Die Analyse der Eigenspannungen in den …
-
Physico-chimie du brasage du carbone vitreux : mouillage et réactivé interfaciale
Dans ce travail nous avons réalisé une étude expérimentale du mouillage réactif du carbone vitreux par des alliages réactifs dans l'objectif d’approfondir la compréhension des phénomènes de mouillage et de réactivité interfaciale pour des applications en brasage du carbone vitreux. Les systèmes …
-
Étude de la pré-oxydation d'alliages modèles en vue de leur protection contre la carburation
Le « metal dusting » est une carburation catastrophique des alliages à base de fer ou de nickel. Ce phénomène a lieu lorsque le mélange gazeux est sursaturé en carbone, à des températures supérieures à 900°C. L’objectif de ce travail consiste à former une couche protectrice d'oxyde sur la surface …