Global ETD Search

Search theses and dissertations gathered from participating repositories worldwide. Every result links back to the library that holds it. No account is needed.

Results

Showing 1 to 20 of 32 for “"Creep and Recovery"”.

  1. Influence of the recovery duration on the cyclic creep response of carbon fibre reinforced polymer composites

    … exhibit time-dependent degradation in modulus and strength. The former is exhibited as time-dependent increase in strain under constant loading, known as creep. Upon unloading, this viscoelastic strain will recover completely if enough time is allowed. During cyclic loading the time for …

    manitoba Repository record for Influence of the recovery duration on the cyclic creep response of carbon fibre reinforced polymer composites (opens in a new tab)

  2. Long-term creep modeling of wood using time temperature superposition principle

    Long-term creep and recovery models (master curves) were developed from short-term data using the time temperature superposition principle (TTSP) for kiln-dried southern pine loaded in compression parallel-to-grain and exposed to constant environmental conditions (~70°F, ~9%EMC). Short-term …

    vt Repository record for Long-term creep modeling of wood using time temperature superposition principle (opens in a new tab)

  3. Fundamental Mechanism of Time Dependent Failure in Shale

    … state of in-situ stresses. The induced and in-situ stresses deform the rockmass surrounding the mine openings. Primary roof supports impede the deformation of the rockmass overlying the entries. However, failure can occur in the bolted rockmass, causing fatalities and injuries. The …

    wvu Repository record for Fundamental Mechanism of Time Dependent Failure in Shale (opens in a new tab)

  4. Factors affecting creep in gold on silicon bi-layer MEMS cantilevered beams

    … research identifies factors that contribute to creep in bi-layer gold on polysilicon MEMS beams. Beams used in this research were manufactured using the Multi-User MEMS Process (MUMPs). Their thicknesses were 2(micrometer) or 4(micrometers) (O.5(micrometers) gold on either 1.5(micrometers) or …

    nps Repository record for Factors affecting creep in gold on silicon bi-layer MEMS cantilevered beams (opens in a new tab)

  5. Effects of canola pretreatments on sorption hysteresis and rheological behavior of single kernels

    Equilibrium moisture content (EMC) and creep and recovery tests were conducted for canola seeds (Brassica napus L., cv. Westar). The effects of sample age, origin and pretreatment (rewetting/drying cycles, irradiation and long-term stress) on EMC properties and viscoelasto-plastic behaviour were …

    manitoba Repository record for Effects of canola pretreatments on sorption hysteresis and rheological behavior of single kernels (opens in a new tab)

  6. Development of an Experimentally Validated Non-linear Viscoelastic Viscoplastic Model for a Novel Fuel Cell Membrane Material

    … exchange membrane fuel cells (PEMFCs). During standard fuel cell operation, the PEM degrades due to cyclic hygrothermal loads, resulting in performance loss or total failure. Improvement of current PEM materials and development of cheaper, more durable materials is essential to the …

    vt Repository record for Development of an Experimentally Validated Non-linear Viscoelastic Viscoplastic Model for a Novel Fuel Cell Membrane Material (opens in a new tab)

  7. Deformation of wood under load

    Creep and recovery tests in compression parallel to the grain were conducted on 2 in. by 2 in. Douglas-fir specimens 4 in. long at four different levels of moisture. Specimens were loaded in stages up to a predetermined load. Instantaneous axial and lateral deformation as well as creep measurements …

    ubc Repository record for Deformation of wood under load (opens in a new tab) Download PDF for Deformation of wood under load (opens in a new tab)

  8. Effect of nonionic surfactant (X-100) on the rheological properties of aqueous polyacrylamide solutions

    … as thickening agent, for turbulent reduction and many other uses. They have been extensively used in enhanced oil recovery. In many cases, polyacrylamide comes into contact with surfactants which lead to a change in its rheological properties. In this study, an experimental work was carried …

    concordia Download PDF for Effect of nonionic surfactant (X-100) on the rheological properties of aqueous polyacrylamide solutions (opens in a new tab)

  9. A Viscoelastoplastic Continuum Damage Model for the Compressive Behavior of Asphalt Concrete

    … illustrates the development, calibration and validation of a comprehensive constitutive material model for asphalt concrete in unconfined and confined compression. A continuum damage-based viscoelastic model is extended with viscoplasticity. Thermodynamic principles, an …

    maryland Repository record for A Viscoelastoplastic Continuum Damage Model for the Compressive Behavior of Asphalt Concrete (opens in a new tab)

  10. Short-Term Creep Properties of Commercial Dentin Bonding Resins

    The compressive creep and recovery of five dentin adhesive resins. (All-Bond 2, Amalgambond Plus. ProBOND. Pertac Universal Bond. Scotchbond 2) chosen from commercial dentin bonding systems were examined in this study. Cylindrical specimens. 8.0 ± 0.1 mm in height and 8.0 ± 0.1 mm in diameter, were …

    marquette Repository record for Short-Term Creep Properties of Commercial Dentin Bonding Resins (opens in a new tab)

  11. Effects of Elevated Temperature on the Physical Aging of a High Temperature Thermoplastic Resin and Composite

    … polymeric composites for both the primary and secondary structures and the predictive methodology necessary for assessment of long term durability. While polymeric composites offer an excellent strength to weight ratio a key disadvantage is the time dependent properties exhibited by the …

    odu Repository record for Effects of Elevated Temperature on the Physical Aging of a High Temperature Thermoplastic Resin and Composite (opens in a new tab)

  12. Characterization of asphalt concrete using anisotropic damage viscoelastic-viscoplastic model

    … of capturing hot mix asphalt (HMA) response and performance under a wide range of temperatures, loading rates, and stress states. The damage viscoelasticity model developed by Schapery (1969) is employed to present the recoverable response, and the viscoplasticity model developed at the Texas …

    tamu Repository record for Characterization of asphalt concrete using anisotropic damage viscoelastic-viscoplastic model (opens in a new tab)

  13. Studies of Mechanical Behavior of HFPE-II-52 Polyimide in Extreme Environments

    Motivated by demanding applications of polyimides and polyimide matrix composites, this study aims to understand the mechanical behavior of HFPE-II-52 polyimide at high temperature. First, a temperature dependent constitutive model combining linear viscoelasticity with viscoplasticity was …

    cornell Repository record for Studies of Mechanical Behavior of HFPE-II-52 Polyimide in Extreme Environments (opens in a new tab)

  14. Prediction of Permanent Deformation in Asphalt Concrete

    … important for preventive maintenance programs and design of rehabilitation strategies. Rutting by definition is the accumulated permanent deformation that remains after removal of the load. Rigorous modeling of permanent deformations using nonlinear finite element analysis based on the correct …

    maryland Repository record for Prediction of Permanent Deformation in Asphalt Concrete (opens in a new tab)

  15. Evaluation of recycled waste plastics as modifiers for performance-graded asphalt binders

    … (RPE) using the Superpave Performance Grading and the Multiple Stress Creep and Recovery (MSCR) Tests. The study will also focus on the influence of the chemical modifiers Elvaloy and Polyphosphoric Acid (PPA) on the performance of the RPE-modified binders. Two different types of RPE pellets …

    manitoba Repository record for Evaluation of recycled waste plastics as modifiers for performance-graded asphalt binders (opens in a new tab)

  16. Long Term Property Prediction of Polyethylene Nanocomposites

    … been thought to be a significant contributor to creep deformation. In polyethylene (PE) nanocomposites, the semicrystalline nature of the maleated PE compatibilizer leads to a limited ability to separate the role of the PE in the nanocomposite properties. This dissertation investigates blown …

    unt Repository record for Long Term Property Prediction of Polyethylene Nanocomposites (opens in a new tab)

  17. Characterization of Rutting in Asphalt Pavements using Laboratory Testing

    … aggregate gradation, air voids, traffic loading, and temperature. Base and sub-base layers and subgrade soil conditions also influence rutting. Excessive rutting can result in structural failure, loss of control while driving, and hydroplaning in the presence of water. The present study aims to …

    oklahoma-thes Repository record for Characterization of Rutting in Asphalt Pavements using Laboratory Testing (opens in a new tab) Restricted access

  18. The Mechanism of Modification and Properties of Polymer Modified Asphalts

    … of asphalt modification with polymers and/or PPA were investigated. The impact of modifying materials on the rheological properties of conventional asphalt was studied in both linear (dynamic mechanical analysis, multiple stress creep and recovery, steady shear viscosity) and non-linear …

    calgary Repository record for The Mechanism of Modification and Properties of Polymer Modified Asphalts (opens in a new tab)

  19. Optimization and characterization of asphalts modified with isocyanate modifier

    … increase of traffic volumes, higher axle loads and harsh climate conditions, the paving industry relies on the use of polymer modified asphalts. With the progress of polymer science and technology, new polymer modified asphalt technologies have emerged. Among the most innovative modification …

    calgary Repository record for Optimization and characterization of asphalts modified with isocyanate modifier (opens in a new tab)

  20. Development of phosphate glass-polymer blends

    … (w/w)%] tin-based polyphosphate glass (Pglass) and organic thermoplastic polymers in conventional plastics processing equipment. The melt rheology of the pure Pglass and of the polymer hybrids was studied under oscillatory shear flow and deformation to understand the behavior of these materials …

    iastate Repository record for Development of phosphate glass-polymer blends (opens in a new tab)