Global ETD Search
Search theses and dissertations gathered from participating repositories worldwide. Every result links back to the library that holds it. No account is needed.
Results
Showing 1 to 17 of 17 for “"Delayed Hydride Cracking"”.
-
Bulk Hydrides and Delayed Hydride Cracking in Zirconium Alloys
… associated with the precipitation of brittle hydride phases and a sub-critical crack growth mechanism known as Delayed Hydride Cracking (DHC) is required to provide the engineering justifications for safe reactor operation. The nature of bulk zirconium hydrides at low concentrations (< 100 wt. …
-
Initiation of delayed hydride cracking in zirconium-2.5 niobium.
Delayed Hydride Cracking (DHC) occurs in Zr-2.5Nb when certain requirements are met. The mechanism of DHC consists of diffusion of hydrogen to a stress concentrator, such as a crack-tip, precipitation then fracture of a hydride at the crack-tip, and repetition of the process; the crack advances in …
-
Characterization of hydrides and delayed hydride cracking in zirconium alloys
… of the missing gaps in the study of zirconium hydrides with state-of-art experiments, cutting edge tomographical technique, and a novel numerical algorithm. A new hydriding procedure is proposed. The new anode material and solution combination overcomes many drawbacks of the AECL hydriding …
-
Initiation of Delayed Hydride Cracking in Zr-2.5Nb Micro Pressure Tubes
… high hydrogen concentration can lead to hydride precipitation during reactor shutdown/repair at flaws, resulting in the potential for eventual rupture of the pressure tubes by a process called Delayed Hydride Cracking (DHC). The threshold stress intensity factor (KIH) below which the …
-
Mapping the Zirconium-Hydrogen Phase System
… of zirconium alloys are vulnerable to failure by Delayed Hydride Cracking, which limits the amount of hydrogen, stress, and temperature history permitted during operation. Recreating reactor end-of-life conditions for testing purposes requires a method of adding hydrogen quantitatively into …
-
Cracking of zirconium alloys at constant load with and without applied potentials
… of their resistance to stress corrosion cracking (SCC), delayed hydride cracking (DHC), and localized corrosion (pitting and crevice) in neutral and acidic environments at ambient temperature and 90°C. For SCC testing, constant load and slow-strain-rate techniques were used. Some SCC …
-
The Effect of Testing Direction on DHC Growth Rate Using Zr-2.5Nb Plate
Delayed Hydride Cracking (DHC) is a fracture mechanism responsible for several failures of Zr-2.5Nb CANDU pressure tubes. The crack velocity is directionally dependant. Disk-shaped hydrides preferentially form on certain crystallographic planes that are hypothesized to be responsible for the …
-
Advanced Techniques for the Characterization of Hydrided Zirconium Alloy
… precipitation of a secondary, brittle zirconium hydride phase. Hydrides tend to first form at flaws (stress concentrations), and when they fracture can initiate a time-controlled crack growth mechanism known as delayed hydride cracking (DHC). Since DHC is a known failure mechanism for pressure …
-
Development, Characterization and Testing of Traditonal and Advanced Nuclear Fuel Cladding Materials
… reactors suffers from the effects of zirconium hydride formation including delayed hydride cracking. Zirconium hydrides in samples of hydrogen charged zircaloy-4 were characterized using 4-dimensional scanning transmission electron microscopy (4D-STEM). With investigation on a novel scale, …
-
Advanced Characterization of Hydrides in Zirconium
… Solid Solubility of Precipitation, brittle hydrides can form. The precipitated hydride phase has been shown to degrade the bulk mechanical properties of zirconium cladding and introduce mechanisms for failure through delayed hydride cracking. The behavior of Zr-H system at low hydrogen …
-
Evaluating the Accuracy of Finite Element Models at Reduced Length Scales
… 3 considers the nucleation of delta-zirconium hydrides in a Zircaloy-2 matrix. Zirconium hydrides are an important topic in the nuclear industry as they form a brittle phase which leads to delayed hydride cracking during reactor start-up and shut-down. Several FE models are used to compare …
-
Texture Evolution and Variant Selection in Zr-2.5Nb During the α-β Phase Transformation
… including strength, dimensional stability, and delayed hydride cracking resistance, are largely dependent upon the crystallographic texture of the hcp α-phase, whose texture is predominantly developed during the extrusion stage of manufacturing. During extrusion and subsequent cooling, the …
-
Analysis of Hydride Effects in Zr-2.5Nb Micro Pressure Tubes
… will precipitate as a flake-like brittle hydride phase. The natural orientation of the hydride flakes is in the circumferential direction but under a tensile hoop stress the hydrides are able to reorientate themselves to the radial direction. This makes the pressure tubes susceptible to …
-
On the Overload Crack Initiation Behaviour of Flaw-tip Reoriented Hydrides in CANDU Zr-2.5Nb Pressure Tube Material
… reactor's lifespan can cause precipitation of hydrides after the alloy’s solubility limit is reached, lowering the alloy’s ductility and fracture toughness. In the case of CANDU reactors, one important component is the pressure tube, made of Zr-2.5Nb alloy and tailored to decrease the hydrogen …
-
Development of Probabilistic Finite Element Models for Assessment of Deformation in CANDU Fuel Channels
… The PT CT contact can lead to the formation of hydride blisters and the eventual delayed hydride cracking (DHC) of PTs. To ensure a reliable operation and to predict the future dimensional changes of the FC, a comprehensive understanding of the nature of in-reactor deformation and physically …
-
MODELS FOR ASSESSMENT OF FLAWS IN PRESSURE TUBES OF CANDU REACTORS
… flaws in a pressure tube makes it vulnerable to delayed hydride cracking (DHC), which may lead to rupture or break-before-leak situation. Therefore, assessment of flaws in the pressure tubes is considered an integral part of a reactor core assessment program. The main objective of the thesis is …
-
Investigation of the mechanical behavior of rim/blister structure hydride phases in Zircaloy-4 by utilizing high energy synchrotron X-ray diffraction
… is potentially problematic. One issue is the delayed hydride cracking (DHC) phenomenon which occurs during storage of used nuclear fuel (UNF). DHC is a time-dependent subcritical crack growth mechanism that can be induced by tensile stress hoop stress within the fuel cladding, even when this …