Global ETD Search

Search theses and dissertations gathered from participating repositories worldwide. Every result links back to the library that holds it. No account is needed.

Results

Showing 1 to 11 of 11 for “"Delayed Hydride Cracking (DHC)"”.

  1. Cracking of zirconium alloys at constant load with and without applied potentials

    … of their resistance to stress corrosion cracking (SCC), delayed hydride cracking (DHC), and localized corrosion (pitting and crevice) in neutral and acidic environments at ambient temperature and 90°C. For SCC testing, constant load and slow-strain-rate techniques were used. Some SCC …

    unlv Repository record for Cracking of zirconium alloys at constant load with and without applied potentials (opens in a new tab) Download PDF for Cracking of zirconium alloys at constant load with and without applied potentials (opens in a new tab)

  2. Initiation of delayed hydride cracking in zirconium-2.5 niobium.

    Delayed Hydride Cracking (DHC) occurs in Zr-2.5Nb when certain requirements are met. The mechanism of DHC consists of diffusion of hydrogen to a stress concentrator, such as a crack-tip, precipitation then fracture of a hydride at the crack-tip, and repetition of the process; the crack advances in …

    ottawa-retro Repository record for Initiation of delayed hydride cracking in zirconium-2.5 niobium. (opens in a new tab)

  3. The Effect of Testing Direction on DHC Growth Rate Using Zr-2.5Nb Plate

    Delayed Hydride Cracking (DHC) is a fracture mechanism responsible for several failures of Zr-2.5Nb CANDU pressure tubes. The crack velocity is directionally dependant. Disk-shaped hydrides preferentially form on certain crystallographic planes that are hypothesized to be responsible for the …

    carleton Repository record for The Effect of Testing Direction on DHC Growth Rate Using Zr-2.5Nb Plate (opens in a new tab)

  4. Advanced Techniques for the Characterization of Hydrided Zirconium Alloy

    … precipitation of a secondary, brittle zirconium hydride phase. Hydrides tend to first form at flaws (stress concentrations), and when they fracture can initiate a time-controlled crack growth mechanism known as delayed hydride cracking (DHC). Since DHC is a known failure mechanism for pressure …

    queens Repository record for Advanced Techniques for the Characterization of Hydrided Zirconium Alloy (opens in a new tab)

  5. Initiation of Delayed Hydride Cracking in Zr-2.5Nb Micro Pressure Tubes

    … high hydrogen concentration can lead to hydride precipitation during reactor shutdown/repair at flaws, resulting in the potential for eventual rupture of the pressure tubes by a process called Delayed Hydride Cracking (DHC). The threshold stress intensity factor (KIH) below which the …

    queens Repository record for Initiation of Delayed Hydride Cracking in Zr-2.5Nb Micro Pressure Tubes (opens in a new tab)

  6. Bulk Hydrides and Delayed Hydride Cracking in Zirconium Alloys

    … associated with the precipitation of brittle hydride phases and a sub-critical crack growth mechanism known as Delayed Hydride Cracking (DHC) is required to provide the engineering justifications for safe reactor operation. The nature of bulk zirconium hydrides at low concentrations (< 100 wt. …

    queens Repository record for Bulk Hydrides and Delayed Hydride Cracking in Zirconium Alloys (opens in a new tab)

  7. Analysis of Hydride Effects in Zr-2.5Nb Micro Pressure Tubes

    … will precipitate as a flake-like brittle hydride phase. The natural orientation of the hydride flakes is in the circumferential direction but under a tensile hoop stress the hydrides are able to reorientate themselves to the radial direction. This makes the pressure tubes susceptible to …

    queens Repository record for Analysis of Hydride Effects in Zr-2.5Nb Micro Pressure Tubes (opens in a new tab)

  8. On the Overload Crack Initiation Behaviour of Flaw-tip Reoriented Hydrides in CANDU Zr-2.5Nb Pressure Tube Material

    … reactor's lifespan can cause precipitation of hydrides after the alloy’s solubility limit is reached, lowering the alloy’s ductility and fracture toughness. In the case of CANDU reactors, one important component is the pressure tube, made of Zr-2.5Nb alloy and tailored to decrease the hydrogen …

    queens Repository record for On the Overload Crack Initiation Behaviour of Flaw-tip Reoriented Hydrides in CANDU Zr-2.5Nb Pressure Tube Material (opens in a new tab)

  9. Development of Probabilistic Finite Element Models for Assessment of Deformation in CANDU Fuel Channels

    … The PT CT contact can lead to the formation of hydride blisters and the eventual delayed hydride cracking (DHC) of PTs. To ensure a reliable operation and to predict the future dimensional changes of the FC, a comprehensive understanding of the nature of in-reactor deformation and physically …

    waterloo Repository record for Development of Probabilistic Finite Element Models for Assessment of Deformation in CANDU Fuel Channels (opens in a new tab)

  10. MODELS FOR ASSESSMENT OF FLAWS IN PRESSURE TUBES OF CANDU REACTORS

    … flaws in a pressure tube makes it vulnerable to delayed hydride cracking (DHC), which may lead to rupture or break-before-leak situation. Therefore, assessment of flaws in the pressure tubes is considered an integral part of a reactor core assessment program. The main objective of the thesis is …

    waterloo Repository record for MODELS FOR ASSESSMENT OF FLAWS IN PRESSURE TUBES OF CANDU REACTORS (opens in a new tab)

  11. Investigation of the mechanical behavior of rim/blister structure hydride phases in Zircaloy-4 by utilizing high energy synchrotron X-ray diffraction

    … is potentially problematic. One issue is the delayed hydride cracking (DHC) phenomenon which occurs during storage of used nuclear fuel (UNF). DHC is a time-dependent subcritical crack growth mechanism that can be induced by tensile stress hoop stress within the fuel cladding, even when this …

    uiuc Repository record for Investigation of the mechanical behavior of rim/blister structure hydride phases in Zircaloy-4 by utilizing high energy synchrotron X-ray diffraction (opens in a new tab)