Global ETD Search

Search theses and dissertations gathered from participating repositories worldwide. Every result links back to the library that holds it. No account is needed.

Results 1 to 18 of 18 for “"Ductility Dip Cracking"”

  1. Quantification of the Susceptibility to Ductility-Dip Cracking in FCC Alloys

    Ductility-dip cracking (DDC) in face-centered cubic (FCC) alloys, such as nickel-based alloys and 300-series stainless steels, is a challenge faced by nuclear power generation. Aging reactors need to be repaired via multipass weld overlays to extend their lifetime. DDC often occurs in the first few …

    ohiolink Repository record for Quantification of the Susceptibility to Ductility-Dip Cracking in FCC Alloys (opens in a new tab)

  2. Development of the Strain-To-Fracture Test to Study Ductility-Dip Cracking in Austenitic Alloys

    … been developed as a robust testing technique for ductility-dip cracking (DDC) and other elevated temperature cracking phenomenon. Samples are tested over a range of temperature and strain, producing temperature-strain cracking envelopes. Threshold strain for fracture (Emin) and the ductility-dip …

    ohiolink Repository record for Development of the Strain-To-Fracture Test to Study Ductility-Dip Cracking in Austenitic Alloys (opens in a new tab)

  3. Development of a High Chromium Ni-Base Filler Metal Resistant to Ductility Dip Cracking and Solidification Cracking

    … been found to be susceptible to stress corrosion cracking. The nuclear power industry now uses high chromium (~30wt%) Ni-based filler metals to mitigate stress corrosion cracking. Current alloys are plagued with weldability issues, either solidification cracking or ductility dip cracking (DDC). …

    ohiolink Repository record for Development of a High Chromium Ni-Base Filler Metal Resistant to Ductility Dip Cracking and Solidification Cracking (opens in a new tab)

  4. Solidification Cracking and Ductility-Dip Cracking Resistance of Ni-Base Filler Metal 52XL with Tantalum and Molybdenum Additions

    … power industry to mitigate stress corrosion cracking in repair and new construction applications. Depending on the composition, current Nb-bearing filler metals face weldability challenges in the form of solidification cracking or ductility-dip cracking. Due to the nature of the eutectic that …

    ohiolink Repository record for Solidification Cracking and Ductility-Dip Cracking Resistance of Ni-Base Filler Metal 52XL with Tantalum and Molybdenum Additions (opens in a new tab)

  5. Optimization and Application of the Strain-To-Fracture Test for Studying Ductility-Dip Cracking in Ni-base Alloys

    … however, led to weldability concerns, such as ductility-dip cracking, that have challenged manufacturers and users of these consumables. Concerns with ductility-dip cracking in FCC materials has led to the development of the Strain-To-Fracture test at Ohio State, which is a weldability test …

    ohiolink Repository record for Optimization and Application of the Strain-To-Fracture Test for Studying Ductility-Dip Cracking in Ni-base Alloys (opens in a new tab)

  6. An investigation of the elevated temperature cracking susceptibility of alloy C-22 weld-metal

    … involving welding, both solidification cracking and ductility-dip cracking (DDC) cracking may occur in these alloys if proper precautions are not followed. One such nickel-base alloy is Alloy C-22, which has limited weldability data to date. Alloy C-22 is one of the most corrosion …

    ohiolink Repository record for An investigation of the elevated temperature cracking susceptibility of alloy C-22 weld-metal (opens in a new tab)

  7. Elemental Effects of Fe, Mo, C, and Hf (or Nb) on Solidification Behavior, Microstructure, and Weldability of High-Cr, Ni-base Filler Metals

    … mitigation of primary water stress corrosion and ductility-dip cracking in Ni-Cr-Fe base materials and filler metals has led to increased Cr, Nb, and Mo contents in these alloys, respectively. Nb additions however, have resulted in a significant increase in the solidification cracking …

    ohiolink Repository record for Elemental Effects of Fe, Mo, C, and Hf (or Nb) on Solidification Behavior, Microstructure, and Weldability of High-Cr, Ni-base Filler Metals (opens in a new tab)

  8. Influence of microstructural features on the hot workability of Ni-based superalloys

    … to 1200°C. This causes severe intergranular cracking during subsequent deformation. During sub-solvus compression < 1100°C, variants with high γ′ fractions are susceptible to ductility dip cracking resulting from strain localisations at grain boundaries due to their high-strength matrix. …

    unsw Repository record for Influence of microstructural features on the hot workability of Ni-based superalloys (opens in a new tab)

  9. Effect of oxygen on the gas tungsten arc weldability of laser-powder bed fusion fabricated 304L stainless steel, The

    … via laser-powder bed fusion would affect the cracking response during gas tungsten arc welding. Weldability and solidification studies were performed on 304L stainless steel material produced via the laser-powder bed fusion process and compared with the behavior of wrought material. It was …

    colo-mines Repository record for Effect of oxygen on the gas tungsten arc weldability of laser-powder bed fusion fabricated 304L stainless steel, The (opens in a new tab)

  10. Intermediate temperature grain boundary embrittlement in nickel-base weld metals

    The ductility-dip cracking (DDC) susceptibility of NiCrFe filler metals was evaluated using the strain-to-fracture (STF) Gleeble(R)-based testing technique. These high chromium Ni-base filler metals are frequently used in nuclear power plant applications for welding Ni-base Alloy 690 and included …

    ohiolink Repository record for Intermediate temperature grain boundary embrittlement in nickel-base weld metals (opens in a new tab)

  11. High temperature cracking of nickel chromium austenitic steels.

    … detailed classification of high temperature weld cracking is proposed. Two major types of cracking are recognised: Type 1 - separations along boundaries decorated with liquated second phase resulting from microsegregation, (solidification cracking in the weld metal and liquation cracking in the …

    sheffield-hallam Repository record for High temperature cracking of nickel chromium austenitic steels. (opens in a new tab)

  12. Development of a Controlled Laboratory Test for Evaluation of DDC Susceptibility in Austenitic Alloys

    Ductility dip cracking (DDC) is a solid-state cracking phenomenon which affects high-Cr Ni-based alloys and welding filler metals. These alloys are utilized in multipass weld overlays in the nuclear industry, where DDC must be avoided due to stringent defect size tolerances imposed by relevant …

    ohiolink Repository record for Development of a Controlled Laboratory Test for Evaluation of DDC Susceptibility in Austenitic Alloys (opens in a new tab)

  13. Induction Bending of Internally Clad Steel Pipes: Failure Mechanisms & Processing Parameter Optimization in Ni-base Alloy Weld Overlays

    Cracking in corrosion resistant clad overlays on low alloy carbon steel pipes made with Alloy 825 has been experienced in the industry in an effort to reduce production costs by changing the cladding material from the more costly Alloy 625. A detailed metallurgical investigation was carried out to …

    ohiolink Repository record for Induction Bending of Internally Clad Steel Pipes: Failure Mechanisms & Processing Parameter Optimization in Ni-base Alloy Weld Overlays (opens in a new tab)

  14. Development of a chromium-free consumable for joining stainless steel

    … stainless steel based on tensile testing. Hot ductility testing revealed a narrow crack susceptible region (33 to 54°C) indicating a low susceptibility to weld metal liquation cracking. A low ductility region was found at intermediate temperatures in the range of 800 to 1100°C. This ductility …

    ohiolink Repository record for Development of a chromium-free consumable for joining stainless steel (opens in a new tab)

  15. Investigation of Weldability in High-Cr Ni-base Filler Metals

    … been affected by primary water stress corrosion cracking. During welding, defects may result from super-solidus and sub-solidus cracking phenomena. The ability to evaluate and quantify the degree to which a given alloy is susceptible to each cracking mechanism is of great importance in alloy …

    ohiolink Repository record for Investigation of Weldability in High-Cr Ni-base Filler Metals (opens in a new tab)

  16. Weldability Evaluation of High-Cr Ni-Base Filler Metals using the Cast Pin Tear Test

    … (DMW) affected by primary water stress corrosion cracking (PWSCC). These alloys provide optimum resistance to PWSCC in nuclear power plant cooling systems. However some of these nickel alloys present weldability challenges including susceptibility to solidification cracking and ductility dip …

    ohiolink Repository record for Weldability Evaluation of High-Cr Ni-Base Filler Metals using the Cast Pin Tear Test (opens in a new tab)