Global ETD Search

Search theses and dissertations gathered from participating repositories worldwide. Every result links back to the library that holds it. No account is needed.

Results

Showing 1 to 20 of 112 for “"E.max"”.

  1. IPS e.max CAD and IPS e.max Press : fracture mechanics characterization

    … crack propagation (FCP) parameters for IPS e.max CAD and IPS e.max Press. Materials and methods: For KIC determinations, 20 (6x6x6x12mm) notchless triangular prism (NTP) specimens of IPS e.max CAD and IPS e.max Press were prepared. IPS e.max CAD blocks were cut, ground and then crystallized, …

    ubc Repository record for IPS e.max CAD and IPS e.max Press : fracture mechanics characterization (opens in a new tab) Download PDF for IPS e.max CAD and IPS e.max Press : fracture mechanics characterization (opens in a new tab)

  2. Marginal gap and internal fit of CEREC e.max and Celtra Duo crowns

    … internal fit as well as marginal chipping of e.max (EM) and Celtra Duo (CD) all-ceramic crowns fabricated using chairside economical restoration of esthetic ceramics (CEREC) system. Material and Methods: Tooth # 15 was prepared for an all-ceramic crown on an ivorine typodont. A total of 15 CD …

    ubc Repository record for Marginal gap and internal fit of CEREC e.max and Celtra Duo crowns (opens in a new tab) Download PDF for Marginal gap and internal fit of CEREC e.max and Celtra Duo crowns (opens in a new tab)

  3. Surface preparation effect on bonding to e.max cad : a fracture mechanics approach

    … interfacial fracture toughness (KIC) of IPS e.max CAD and an adhesive resin luting cement. Material and Methods: The materials selected for this study were from Ivoclar-Vivadent, Liechtenstein: e.max CAD blocks, Multilink implant, Mono Bond Plus, and IPS Ceramic Etching Gel. Eighty (4x4x4x4 mm) …

    ubc Repository record for Surface preparation effect on bonding to e.max cad : a fracture mechanics approach (opens in a new tab) Download PDF for Surface preparation effect on bonding to e.max cad : a fracture mechanics approach (opens in a new tab)

  4. Color stability of pressed IPS e.max lithium disilicate ceramics after repeated firing cycles

    … difference CIEDE2000 (ΔE00) of pressed IPS E.max lithium disilicate ceramic material after repeated firing cycles. To determine and evaluate correlation of CIELAB and CIEDE2000 values analyzed by X-Rite Color i5 Spectrophotometer, VITA EasyShade® Advance 4.0 (VITA Zahnfabrik) and Adobe …

    bu Repository record for Color stability of pressed IPS e.max lithium disilicate ceramics after repeated firing cycles (opens in a new tab)

  5. Effect of porcelain thickness and translucency on the final shade of IPS e.max CAD overlaying a dark substrate.

    IPS e.max is a very esthetic lithium disilicate used in dental ceramics. Unfortunately, it can unintentionally change color after cementation with resin cements. The purpose of this study is to better understand how combining thickness and translucency affects the post-cementation shade of IPS …

    louisville Repository record for Effect of porcelain thickness and translucency on the final shade of IPS e.max CAD overlaying a dark substrate. (opens in a new tab)

  6. Überlebensanalyse und klinische Nachuntersuchung einer maschinenbearbeitbaren Lithiumdisilikatkeramik (IPS e.max CAD LT) von Einzelzahnrestaurationen im Seitenzahngebiet im chairside-Verfahren: 10-Jahres-Ergebnisse

    … im Durchschnitt 46,6 Jahre (±13,1; min. 26, max. 72; davon 62% weiblich). Die statistische Auswertung (IBM SPSS Statistics 22, IBM Ehningen, Deutschland) der Daten erfolgte mittels Kaplan-Meier-Analyse, Log-Rank-Test und Wilcoxon-Vorzeichenrangtest bei einem Signifikanzniveau von p=0,05. Nach …

    qucosa-diss

  7. Failure load of monolithic and veneered Y-TZP and glass ceramic subjected to aging and fatigue

    … materials were used: Vita In-Ceram YZ and IPS e. max CAD. Each material was designed into 60 veneered copings and 30 monolithic crowns (180 specimens). 10 specimens per group were loaded under compression using an Instron universal testing machine at a rate of 0.5 mm/minute until fracture. Another …

    bu Repository record for Failure load of monolithic and veneered Y-TZP and glass ceramic subjected to aging and fatigue (opens in a new tab)

  8. Flexural strength and marginal fit of two types of lithium disilicate ceramics for crowns

    … compare the marginal fit of crowns made with e.max press and a new experimental (EXP) press ceramic. MATERIALS AND METHODS: The materials tested for flexural strength included: E.max press, E.maxCAD, ENAMIC, Experimental press, and Experimental-CAD. Each group (N= 10) was tested using the …

    bu Repository record for Flexural strength and marginal fit of two types of lithium disilicate ceramics for crowns (opens in a new tab)

  9. Failure load of CAD/CAM-generated all ceramic posterior endocrowns

    … the failure load of milled and bonded IPS e.max CAD and VITA ENAMIC endocrowns used in the restoration of endodontically molar teeth. MATERIALS AND METHODS: Typodont tooth # 30 was prepared with a central cavity to support the endocrowns. Fifty-eight epoxy resin dies were made from a physical …

    bu Repository record for Failure load of CAD/CAM-generated all ceramic posterior endocrowns (opens in a new tab)

  10. Comparison of adherence of self-cured adhesive resin cement to lithium disilicate ceramics and ceramic resin composites using fracture mechanics

    … Enamic – Vita-Zahnfabrik) and a ceramic (IPS e.max – Ivoclar-Vivadent). Materials and Methods : Sixty specimens were prepared from each e.max and Enamic, and 120 specimens were prepared for Lava Ultimate. Ceramic resin composite blocks samples were prepared by wet cutting and grinding. Ceramic …

    ubc Repository record for Comparison of adherence of self-cured adhesive resin cement to lithium disilicate ceramics and ceramic resin composites using fracture mechanics (opens in a new tab) Download PDF for Comparison of adherence of self-cured adhesive resin cement to lithium disilicate ceramics and ceramic resin composites using fracture mechanics (opens in a new tab)

  11. Mechanical and optical properties of machinable and pressable glass ceramic

    … Four glass-ceramics were investigated; IPS e.max CAD, IPS e.max Press, Celtra Duo, and Celtra Press. For each material 87 disc-shaped specimens, 2 mm in thickness and 12 mm in diameter were fabricated. Specimens were divided into 3 groups (n=29) as no treatment, polishing, and glazing group. …

    bu Repository record for Mechanical and optical properties of machinable and pressable glass ceramic (opens in a new tab)

  12. Effects of etching duration on the surface roughness, surface loss, flexural strength, and shear bond strength to a resin cement of e.max cad glass ceramic

    … deleterious effects on ceramic strength while maximizing the bond strength to tooth structure. Objectives: To evaluate the effects of HF acid etching duration on the surface roughness, surface loss, flexural strength, and shear bond strength of IPS e.max CAD (Ivoclar Vivadent) lithium …

    iupui Repository record for Effects of etching duration on the surface roughness, surface loss, flexural strength, and shear bond strength to a resin cement of e.max cad glass ceramic (opens in a new tab)

  13. The effect of repetitive firing cycles on physical and optical properties of zirconia reinforced lithium silicate ceramics

    … showed that repetitive firing cycles reduced e.max® and Vita Suprinity’s® translucency, but not that of Celtra® Duo, which showed no significant difference. All materials of greater thickness exhibited less translucency, and e.max® CAD had the highest mean light transmission; however, it was not …

    bu Repository record for The effect of repetitive firing cycles on physical and optical properties of zirconia reinforced lithium silicate ceramics (opens in a new tab)

  14. Die mechanische und thermische Belastbarkeit von Zirkonoxidgerüst-Kronen und Brücken in Abhängigkeit vom Verblendmaterial

    … Es wurden die Verblendkeramiken e.max (Firma Ivoclar) und Cercon ceram S (Firma DeguDent) gegenübergestellt. Der zweite Teil der Arbeit untersucht die Auswirkung künstlicher Alterung auf die Festigkeitseigenschaften von physiologisch gelagerten vollkeramischen …

    lmu-germany Repository record for Die mechanische und thermische Belastbarkeit von Zirkonoxidgerüst-Kronen und Brücken in Abhängigkeit vom Verblendmaterial (opens in a new tab)

  15. Edge-Chipping and Translucency Comparison Among Lithium Silicate-Based Ceramics

    … glass-ceramic materials, IPS e.max CAD and GC Initial LiSi blocks, and two zirconia-lithium silicate glass-ceramic materials, Vita Suprinity and Celtra Duo, were prepared and tested (n=20 specimens/group). Specimens (14 x 12 x 1.5 mm) were sectioned from commercially available …

    marquette Repository record for Edge-Chipping and Translucency Comparison Among Lithium Silicate-Based Ceramics (opens in a new tab)

  16. Effect of firing cycle and etching condition on resin cement tensile bond strength of Li2O-SiO2 system glass ceramics

    … on the tensile bonding strength (TBS) of IPS e.max-CAD and CeltraDUO. METHODS: Lithium-disilicate (IPS e.max-CAD) ceramic blocks and zirconia reinforced lithium-disilicate (CeltraDUO) were sectioned into rectangular tiles. The tiles were randomly assigned to various treatment groups and heat …

    bu Repository record for Effect of firing cycle and etching condition on resin cement tensile bond strength of Li2O-SiO2 system glass ceramics (opens in a new tab)

  17. The Effect Of Crystallization Temperature On The Flexural Strength Of Lithium Disilicate Glass-Ceramics

    … control lithium disilicate CAD blocks (IPS e.max CAD, Ivoclar Vivadent, Amherst, NY) of the same shade. Four different translucencies were selected for Amber Mill CAD blocks and were as follows: HT, MT, LT, and MO. Two different translucencies were selected for IPS e.max CAD blocks and were as …

    umn Repository record for The Effect Of Crystallization Temperature On The Flexural Strength Of Lithium Disilicate Glass-Ceramics (opens in a new tab)

  18. Retention Of Cad/Cam Crowns Luted With Resin Cements And Rmgi

    … measure retention of lithium disilicate (IPS e.max CAD, Ivoclar Viva-dent) and zirconia reinforced lithium disilicate (CELTRATM DUO, Dentsply) copings luted using resin cements and resin-modified glass ionomer cement. Methods: 110 Extracted human, non-carious mandibular 2nd premolars (n=10) were …

    uab Repository record for Retention Of Cad/Cam Crowns Luted With Resin Cements And Rmgi (opens in a new tab)

  19. Fracture Resistance of Lithium Disilicate Restorations Following Endodontic Access Preparation; An In Vitro Study

    … restorations. Twenty monolithic milled (IPS e.max Press) and twenty monolithic milled (IPS e.max CAD) lithium disilicate restorations were fabricated and adhesively bonded to forty identical epoxy resin dies. Ten of the pressed and ten of the milled crowns were accessed for a simulated …

    tamu Repository record for Fracture Resistance of Lithium Disilicate Restorations Following Endodontic Access Preparation; An In Vitro Study (opens in a new tab)

Page 1 of 6