Global ETD Search
Search theses and dissertations gathered from participating repositories worldwide. Every result links back to the library that holds it. No account is needed.
Results
Showing 1 to 20 of 59 for “"E.max CAD"”.
-
IPS e.max CAD and IPS e.max Press : fracture mechanics characterization
… crack propagation (FCP) parameters for IPS e.max CAD and IPS e.max Press. Materials and methods: For KIC determinations, 20 (6x6x6x12mm) notchless triangular prism (NTP) specimens of IPS e.max CAD and IPS e.max Press were prepared. IPS e.max CAD blocks were cut, ground and then crystallized, …
-
Surface preparation effect on bonding to e.max cad : a fracture mechanics approach
… interfacial fracture toughness (KIC) of IPS e.max CAD and an adhesive resin luting cement. Material and Methods: The materials selected for this study were from Ivoclar-Vivadent, Liechtenstein: e.max CAD blocks, Multilink implant, Mono Bond Plus, and IPS Ceramic Etching Gel. Eighty (4x4x4x4 mm) …
-
Effect of porcelain thickness and translucency on the final shade of IPS e.max CAD overlaying a dark substrate.
IPS e.max is a very esthetic lithium disilicate used in dental ceramics. Unfortunately, it can unintentionally change color after cementation with resin cements. The purpose of this study is to better understand how combining thickness and translucency affects the post-cementation shade of IPS …
-
Überlebensanalyse und klinische Nachuntersuchung einer maschinenbearbeitbaren Lithiumdisilikatkeramik (IPS e.max CAD LT) von Einzelzahnrestaurationen im Seitenzahngebiet im chairside-Verfahren: 10-Jahres-Ergebnisse
… Material im chairside-Verfahren mit Hilfe von CAD/CAM-Technik herzustellen, gewährt der modernen Zahnmedizin ökonomische Vorteile, wie beispielsweise die Präparationsanalyse in Echtzeit, selektive Wiederholbarkeit des Abdruckes, digitales Archivieren, Versorgung in einer Sitzung, die damit …
-
Failure load of monolithic and veneered Y-TZP and glass ceramic subjected to aging and fatigue
… materials were used: Vita In-Ceram YZ and IPS e. max CAD. Each material was designed into 60 veneered copings and 30 monolithic crowns (180 specimens). 10 specimens per group were loaded under compression using an Instron universal testing machine at a rate of 0.5 mm/minute until fracture. Another …
-
Effects of etching duration on the surface roughness, surface loss, flexural strength, and shear bond strength to a resin cement of e.max cad glass ceramic
… deleterious effects on ceramic strength while maximizing the bond strength to tooth structure. Objectives: To evaluate the effects of HF acid etching duration on the surface roughness, surface loss, flexural strength, and shear bond strength of IPS e.max CAD (Ivoclar Vivadent) lithium …
-
Edge-Chipping and Translucency Comparison Among Lithium Silicate-Based Ceramics
… glass-ceramic materials, IPS e.max CAD and GC Initial LiSi blocks, and two zirconia-lithium silicate glass-ceramic materials, Vita Suprinity and Celtra Duo, were prepared and tested (n=20 specimens/group). Specimens (14 x 12 x 1.5 mm) were sectioned from commercially available …
-
Effect of firing cycle and etching condition on resin cement tensile bond strength of Li2O-SiO2 system glass ceramics
… on the tensile bonding strength (TBS) of IPS e.max-CAD and CeltraDUO. METHODS: Lithium-disilicate (IPS e.max-CAD) ceramic blocks and zirconia reinforced lithium-disilicate (CeltraDUO) were sectioned into rectangular tiles. The tiles were randomly assigned to various treatment groups and heat …
-
The Effect Of Crystallization Temperature On The Flexural Strength Of Lithium Disilicate Glass-Ceramics
… protocols on the flexural strength of Amber Mill CAD glass-ceramics. Materials and Methods: Amber Mill CAD ceramic blocks (HASSBIO America Inc., Fairfax, VA) of a known Vita Classic shade (A1) shade were selected for testing against control lithium disilicate CAD blocks (IPS e.max CAD, Ivoclar …
-
Failure load of CAD/CAM-generated all ceramic posterior endocrowns
… the failure load of milled and bonded IPS e.max CAD and VITA ENAMIC endocrowns used in the restoration of endodontically molar teeth. MATERIALS AND METHODS: Typodont tooth # 30 was prepared with a central cavity to support the endocrowns. Fifty-eight epoxy resin dies were made from a physical …
-
Mechanical and physical properties of three CAD/CAM glass-ceramics
… and physical properties of three glass-ceramic CAD/CAM systems; Vita Suprinity PC (Vita ZahnFabrik), Cerrec Tessera (Dentsply-Sirona), and IPS e.max CAD (Ivoclar Vivadent). MATERIALS AND METHODS: For each material, CAD/CAM blocks were sectioned into a total of N=108 (n=12 per group) test discs …
-
Fatigue behaviour and failure modes of monolithic CAD/CAM hybrid-ceramic and all-ceramic posterior crown restorations
… behaviour and failure modes of a novel CAD/CAM experimental hybrid-ceramic material and to compare it with two monolithic all-ceramic CAD/CAM materials (Vita Mark II and IPS e.max CAD) in a standardized molar crown model. The correlation between fracture load, cement thickness, crack …
-
Effect of real time aging and cyclic fatigue on fused and cemented machined veneers to Y-TZP zirconia
… The veneering material was either milled IPS e.max CAD (glass-ceramic) or milled VITABLOCS Triluxe Forte (feldspathic porcelain). The types of linking material between the substructures and veneering material were either fusing or cementation. Observations were compared between aged and non-aged …
-
The effects of machining on the flexural strength of CAD-CAM materials
… machining modes on the flexural strength CAD-CAM restorative materials. MATERIALS AND METHODS: Four different CAD-CAM materials were used: VITA MARKII, VITA Enamic (VITA Zahnfabrik), Empress CAD, and e.max CAD (Ivoclar Vivadent). Rectangular bars for each material (except e.max CAD) were …
-
Mechanical and optical properties of machinable and pressable glass ceramic
… Four glass-ceramics were investigated; IPS e.max CAD, IPS e.max Press, Celtra Duo, and Celtra Press. For each material 87 disc-shaped specimens, 2 mm in thickness and 12 mm in diameter were fabricated. Specimens were divided into 3 groups (n=29) as no treatment, polishing, and glazing group. …
-
Static and cyclic loading effects on fracture toughness of contemporary CAD/CAM restorative materials
… (K1C) and microhardness of dental restorative CAD/CAM materials. MATERIAL AND METHODS: Five commercially available CAD/CAM restorative materials were included in this study: Lava™ Ultimate Restorative (3M ESPE), IPS Empress® CAD (Ivoclar Vivadent), Enamic® (VITA), IPS e.max® CAD (Ivoclar …
-
Chipping, failure load and fatigue resistance of anterior veneers manufactured with CAD/CAM technology
… marginal chipping of anterior veneers made with CAD/CAM by calculating the chipping factor, to evaluate the failure load of different veneering materials and thicknesses under static loading and cyclic loading. MATERIALS AND METHODS: An ivorine central incisor was prepared to receive a …
-
Fracture Strength of Translucent Zirconia Crowns
… crown preparations were designed with AutoCAD software with a 0.8mm shoulder margin and 1 mm incisal-cervical marginal curvature. A stylized crown with a 1mm thickness and 0.8mm minimum thickness in the central pit was designed in 3shape software. Tooth dies were milled out of a resin …
-
Machinability of ceramic blanks for dental CAD/CAM restorations
… focused on evaluating the damage of various CAD/CAM materials arising from machine type, CAM setup, machining parameters, and tool quality. MATERIALS & METHODS: The tested materials were VITA Mark II (feldspathic block), Ivoclar e.max CAD (un-crystallized lithium disilicate), and VITA Enamic …
-
Crown Fatigue Resistance And Enamel Wear Of 3D Printed Resin Compared To Lithium Disilicate
… Crown, a 3D-printed resin material, and IPS™ e.Max CAD, a lithium disilicate material. Methods: This study evaluates wear and fatigue characteristics of dental crowns made from Ceramic Crown (SprintRay) and IPS e.max CAD LT (Ivoclar). For fatigue testing, custom fatigue devices were utilized to …
Page 1 of 3