Global ETD Search
Search theses and dissertations gathered from participating repositories worldwide. Every result links back to the library that holds it. No account is needed.
Results
Showing 1 to 20 of 83 for “"Early Strength"”.
-
Compressive tests of high early strength cements
Thesis (M.S.)--Michigan State College of Agriculture and Applied Science, 1930
-
Early Strength Development of Cement Mixed Singapore Marine Clay
… This research was set out to devise an effective early QC technique for the cement mixed clay fill in land reclamation. The early strength behaviour of cement mixed Singapore marine clay was first investigated. In this investigation, the effect of curing temperature on the early strength behaviour …
-
Optimization of very early strength concrete mixes using maturity method
… fast track was concerned only with rapid strength gain and workability but little concern was paid to cost and durability of the concrete. The purpose of this research study is to develop a current improved very early strength (VES) concrete mix, which was accepted by NJDOT in 1996. More …
-
REHABILITATION AND MAINTENANCE OF ROAD PAVEMENTS USING HIGH EARLY STRENGTH CONCRETE.
… maintenance purposes. The application of early strength concrete in pavement maintenance measures will lead to a substantial reduction in the user costs involved with the road closures caused by such maintenance. These costs involve both the actual costs of the delays in terms of time and …
-
Very Early Strength Latex-Modified Concrete Used For Bridge Deck Repairs
M.S. Thesis. University of Hawaiʻi at Mānoa 2018.
-
High-Early Strength Concrete for Rapid Bridge Deck Repair and Rehabilitation
… the same characteristic of fast-setting and high-early strength development to minimize traffic disruptions, however, current methods do not typically address rehabilitation at varying levels of deterioration or make use of expensive non-cementitious materials. This research investigated the use …
-
Towards performance engineered specifications for high early strength concrete pavement repair applications
… highway repair applications are required to gain strength at a much faster pace than regular concrete mixtures. By uniquely focusing on the strength requirements, other mixture properties such as durability are often neglected, so that many agencies have reported premature failure of the repaired …
-
Effects of supplementary cementing materials on the setting time and early strength of concrete
… frequently results in delayed setting and low early strength. When SCM containing concrete is placed during cold weather and/or contains certain chemical admixtures, these problems can intensify and can seriously impact the performance of a pavement. This project investigated the setting time, …
-
Robust Methods for UHPC Early-Strength Determination and Quality Control for Accelerated Bridge Construction
… of UHPC is that it can reach high compression strength of about 10-12 ksi after one day and about 21-23ksi after 28 days of casting. Such advantage is crucial for accelerated construction, especially bridges where the roads are fully closed when traditional construction methods are used. To …
-
Use Of Nano-Silica To Increase Early Strength And Reduce Setting Time Of Concretes With High Volumes Of Slag Or Fly Ash
… slag or fly ash concretes can develop good strengths over time if properly cured, exceeding those of similar concretes without slag or fly ash. However, early strengths of such concretes are often lower than Portland cement concrete without slag or fly ash which may affect construction …
-
Investigating Rapid Concrete Repair Materials and Admixtures
… to their present and future work. Current high early strength concrete mixtures have natural cracking and shrinkage problems due to the high content of cementitious material or their chemical components. Using IC allows for early strength, enhanced durability, reduced shrinkage and a better …
-
High performance concrete in Oklahoma designed for precast/prestressed bridge beams.
… applications. Cement selection is crucial to early strength gain while the choice of coarse aggregate is more important for ultimate strength development. The w/cm is a useful statistics for today's increasingly complex HPC mixtures. Heat curing was damaging to ultimate strength potential and, …
-
Explore Accelerated PCC Pavement Repairs Using Metakaolin-Based Geopolymer Concrete
… under different acid conditions on the bond strength of geopolymer with conventional concrete, and comparison of the metakaolin geopolymer with other pavement repair materials are analyzed. It was found curing time affects the interface bond strength greatly and the interface bond strength …
-
Concrete Mix Design for TxDOT CRCP Repair: Utilizing Rapid Set Cement (RSC) with Nano Calcium Carbonate
… the challenges of temperature sensitivity and early strength gain. Through the evaluation of nano CaCO3 with rapid set cement (RSC), the study investigates the effectiveness of enhancing early-age strength under low ambient temperatures. Findings suggest that careful consideration of fresh …
-
Examining compositions, hydration mechanisms and properties of supersulfated cement for use in concrete
… is currently under-utilized because of its slow early-strength development. The low-alumina content (
-
Cold In-Place Recycling with Expanded Asphalt Mix (CIREAM)
… (CIR) and other methods. Although CIREAM offers early strength advantages and extended paving periods among other benefits, late season CIREAM can be burdened by distresses such as ravelling, potholing and other moisture-induced damage. Limited information on the behaviour and failure mechanisms …
-
Development of High Performing, Commercially Relevant Concretes with High Levels of Clinker Replacement by Manipulating Microstructure and Controlling Crystal Growth
… carbon, blended cement formulations. The reduced strength development due to the addition of slag can be improved by the addition of chemical activators such as sodium sulfate (Na2SO4). The reactivity and early strength of cement:slag binders is significantly enhanced by the addition of Na2SO4 …
-
Use of Supplementary Cementitous Material in Concrete Effect on Fresh Concrete Properties
… the fresh state properties as well as long-term strength and durability. This study investigated six different SCMs, both natural and industrial, i.e. ground granulated blast furnace slag (GGBS), fly ash (FA), calcined (Nova) clay, volcanic pozzolan from Iceland (VPI), pumice (Yalite) from …
Page 1 of 5