Global ETD Search

Search theses and dissertations gathered from participating repositories worldwide. Every result links back to the library that holds it. No account is needed.

Results

Showing 1 to 15 of 15 for “"Edge delamination"”.

  1. Application of finite fracture mechanics for predicting free edge delamination in multi-layered materials under various loading conditions

    This thesis investigates the free edge effect in multi-layered composites, where stress concentrations at dissimilar interfaces induce delamination. A novel 3D Finite Fracture Mechanics (FFM) criterion is introduced to predict delamination under quasi-static, thermal, and fatigue loading …

    qu-belfast Repository record for Application of finite fracture mechanics for predicting free edge delamination in multi-layered materials under various loading conditions (opens in a new tab) Download PDF for Application of finite fracture mechanics for predicting free edge delamination in multi-layered materials under various loading conditions (opens in a new tab)

  2. Fracture of advanced polymer composites with nanofiber reinforced interfaces

    … study is performed to explore the novel delamination suppression concept based on nanofiber reinforcement of interfaces between plies in advanced polymer composites (Dzenis and Reneker: US patents awarded and pending). Edge delamination was studied on graphite/epoxy composites reinforced …

    nebraska Repository record for Fracture of advanced polymer composites with nanofiber reinforced interfaces (opens in a new tab)

  3. Additive layers to suppress delamination in composite laminates

    Delamination originating from the free edges is a common failure mechanism of composite laminates, as the free edges in composite laminates are high-stress concentration areas. This thesis has studied a solution that could suppress delamination starting from the free edges in composite laminates in …

    strathclyde Repository record for Additive layers to suppress delamination in composite laminates (opens in a new tab)

  4. In-situ corrosion health monitoring and prediction in miltary vehicles.

    … i.e. micro-cracks effects, blistering and edge delamination. These models can be used for the analysis of coating failure initiation and propagation, especially useful for coating life assessment. The models follow multidisciplinary approach coupling the concepts of thermodynamics, fracture …

    bournemouth Download PDF for In-situ corrosion health monitoring and prediction in miltary vehicles. (opens in a new tab) Embargoed until 2099-12-31

  5. Variable complexity modeling of postbuckled stiffeners for delamination initiation

    Delamination at the free edge is analyzed as a mode of failure for uniaxial compression of postbuckled structural components. Analyses are performed for I-section stiffeners and for a dropped-ply laminate, all of which failed due to free edge delamination in earlier experimental studies. These …

    vt Repository record for Variable complexity modeling of postbuckled stiffeners for delamination initiation (opens in a new tab)

  6. Co-cured composite joint strength investigation based on behavior characterization of [0/±θ/90]s family

    … co-cured composite joints through minimized free-edge delamination was investigated for quasi-isotropic [0/±45/90]s lay-up based on the quantitative assessments of the quasi-static and fatigue strength and qualitative understanding of the fatigue damage initiation and propagation for the …

    gatech Repository record for Co-cured composite joint strength investigation based on behavior characterization of [0/±θ/90]s family (opens in a new tab)

  7. Considerations of the Impedance Method, Wave Propagation, and Wireless Systems for Structural Health Monitoring

    … are examined: transverse matrix cracking and edge delamination. With both composite defects, a sample is interrogated with the impedance method before and after damage is introduced. The exact amount of damage in each specimen is found using radiography and compared with the health monitoring …

    vt Repository record for Considerations of the Impedance Method, Wave Propagation, and Wireless Systems for Structural Health Monitoring (opens in a new tab)

  8. Instability-related delamination growth of embedded and edge delaminations

    … in composite laminates that have a near-surface delamination. This buckling causes load redistribution and secondary loads, which in turn cause interlaminer stresses and delamination growth. The goal of this research effort was to enhance the understanding of this instability-related delamination …

    vt Repository record for Instability-related delamination growth of embedded and edge delaminations (opens in a new tab)

  9. EXPERIMENTAL CHARACTERIZATION OF ELASTIC STIFFNESS AND DELAMINATION TOUGHNESS IN THERMAL BARRIER COATING SYSTEMS

    … material systems requires detailed knowledge of the constitutive behavior of each layer and the adhesion between layers. The focus of this study is to measure the properties relevant to thermal barrier coatings and elucidate how variations in the processing affect the mechanical response. …

    jhu Repository record for EXPERIMENTAL CHARACTERIZATION OF ELASTIC STIFFNESS AND DELAMINATION TOUGHNESS IN THERMAL BARRIER COATING SYSTEMS (opens in a new tab)

  10. Experimental measurements of thermal barrier coating interfacial fracture toughness as a function of mode-mix

    … for gas turbine engines rely on accurate knowledge of the experimentally measured interfacial fracture toughness over a range of mode mix and especially at mode-II. Previously no reliable test method had been employed to evaluate these properties under pure mode-II conditions, which are most …

    jhu Repository record for Experimental measurements of thermal barrier coating interfacial fracture toughness as a function of mode-mix (opens in a new tab)

  11. Understanding the Formation Mechanism of Plasma-sprayed Ni and Ni20Cr Splats through Experimental and Numerical Study

    … microstructure, contact quality and edge delamination, were carefully characterised by FIB and TEM microscopes. Combined with the simulation results of energy conversion and fluid dynamics during droplet spreading, solidification was found to be crucial in generating splashing in the …

    auckland-ms Repository record for Understanding the Formation Mechanism of Plasma-sprayed Ni and Ni20Cr Splats through Experimental and Numerical Study (opens in a new tab)

  12. Trans-laminar-reinforced (TLR) composites

    … restricted size and growth of impact damage and edge delamination. TLR has also been used to eliminate catastrophic stiffener disbonding in stiffened structures. as little as one percent volume of TLR significantly alters the mechanical response of laminates.;The objective of this work was to …

    wm-mary Repository record for Trans-laminar-reinforced (TLR) composites (opens in a new tab)

  13. Development of Damage Detection Techniques Using Guided Waves for Engineering Materials

    … contain structural features like weld joints and edges, where defects commonly occur due to high stress concentration. These structural features have complex cross-sections, adding complexity to wave analysis and making damage detection a challenging task. The second challenge arises from …

    adelaide Repository record for Development of Damage Detection Techniques Using Guided Waves for Engineering Materials (opens in a new tab)

  14. Mechanics of bubbles and tents formed by 2D materials

    … conditions that prohibit any motions of their edges. In striking contrast, experimental observations have revealed subtle wrinkling instabilities near the edge of 2D material bubbles and tents (even at small deflections before further edge delamination occurs). This gives concrete evidence for …

    texas Repository record for Mechanics of bubbles and tents formed by 2D materials (opens in a new tab)

  15. Scale effects in buckling, postbuckling and crippling of graphite-epoxy Z-section stiffeners

    … The crippling mechanisms included flange free edge delamination at both nodal and anti-nodal axial positions, material crushing in the flange-to-web corner at nodal axial positions, and ply splitting in the flange-to-web corner at anti-nodal axial locations. The constraint of the potted end …

    vt Repository record for Scale effects in buckling, postbuckling and crippling of graphite-epoxy Z-section stiffeners (opens in a new tab)