Global ETD Search

Search theses and dissertations gathered from participating repositories worldwide. Every result links back to the library that holds it. No account is needed.

Results 1 to 18 of 18 for “"Edge fracture"”

  1. Prediction and Prevention of Edge Fracture in Forming of AHSS

    Edge fracture, defined simply as fracture originated from the edge, is a common problem in sheet metal forming, especially when forming Advanced High Strength Steels (AHSS). The increase of AHSS in the automotive industry has derived into substantial efforts in order to predict and prevent the edge …

    ohiolink Repository record for Prediction and Prevention of Edge Fracture in Forming of AHSS (opens in a new tab)

  2. Edge Fracture Prediction Of Dual Phase Steels With Consideration Of Microstructures

    … This class of sheet metals are prone to edge fracture during stamping production, and the fracture often occurs at much lower strain than that predicted based on the forming limit curves. The uncertainty in predicting edge fracture represents a great challenge in the application of AHSS. …

    wayne-thes Repository record for Edge Fracture Prediction Of Dual Phase Steels With Consideration Of Microstructures (opens in a new tab)

  3. Influence of Anisotropy on Edge Fracture of Advanced High-strength Steels

    … deformed local area. AHSS is more susceptible to edge fracture compared to traditional mild steels, due not only to reduced ductility but also to distinct local fracture behavior. To deepen the knowledge of the edge fracture behavior of AHSS, it is necessary to find a characterization method that …

    aalto Repository record for Influence of Anisotropy on Edge Fracture of Advanced High-strength Steels (opens in a new tab)

  4. Evaluation of Edge Fracture in Flanging Advanced High Strength Steel (AHSS) Using the Double Bending Test

    Different type of shearing methods is used in the edge trimming operation. For example, conventional shearing, water jet or laser cutting. Even though water jet and laser cutting yields better edge quality, for mass production, conventional shearing is the preferred method due to the time and cost …

    ohiolink Repository record for Evaluation of Edge Fracture in Flanging Advanced High Strength Steel (AHSS) Using the Double Bending Test (opens in a new tab)

  5. Influence of Boundary Conditions on the Sheared Edge Fracture Limits of a 3rd Generation Advanced High Strength Steel.

    … strength steels (AHSS), particularly for sheared edge splitting in automotive forming operations. The widely used ISO16630 conical hole expansion test for edge stretchability is known to be a poor representation of the in-plane deformation modes that are the primary source of edge splitting in …

    waterloo Repository record for Influence of Boundary Conditions on the Sheared Edge Fracture Limits of a 3rd Generation Advanced High Strength Steel. (opens in a new tab)

  6. A Numerical and Practical Investigation for the Edge Fracture of Advanced High Strength Steels (AHSS) Using the Half Dome Test

    In edge trimming process, shearing and water-jet (or laser-cut) are two commonly used methods in industry for Advanced High Strength Steel (AHSS). Water-jet (or laser-cut) is commonly used during prototyping since it does not need conventional cutting tools and it can cut virtually any materials. …

    ohiolink Repository record for A Numerical and Practical Investigation for the Edge Fracture of Advanced High Strength Steels (AHSS) Using the Half Dome Test (opens in a new tab)

  7. Aplicação de curvas limite de conformação na previsão de rupturas em bordas de peças estampadas

    … limitation comes from the work hardening and the edge defects generated during the cutting operation which decreases the materials ductility in this region, causing premature fractures. The hole expansion test is used to evaluating the ability of deformed edges. However, the major concern with …

    brazil-ufmg Repository record for Aplicação de curvas limite de conformação na previsão de rupturas em bordas de peças estampadas (opens in a new tab)

  8. Graman revisited : an analysis of stone artefact and site function at Graman sites GB1 and GB4

    … particularly those dealing with variations in fracture damage rates and transverse snapping. Both of these areas of research require further investigation b u t it appears that edge fracture rates are linked both to intensity and duration of use and to the mechanical properties of the stone raw …

    anu Repository record for Graman revisited : an analysis of stone artefact and site function at Graman sites GB1 and GB4 (opens in a new tab)

  9. Shear banding in polymeric fluids under large amplitude oscillatory shear flow

    … discuss the possible importance of considering edge fracture as a mechanism for shear banding.

    durham Repository record for Shear banding in polymeric fluids under large amplitude oscillatory shear flow (opens in a new tab)

  10. Nonlinear Flow Behavior of Entangled DNA Fluids

    … Because of experimental difficulties such as edge fracture during shearing, it is challenging to achieve reliable steady state in synthetic entangled polymeric liquids. In this work, we choose DNA solutions as model entangled systems. Since the required DNA concentration is rather low, between …

    ohiolink Repository record for Nonlinear Flow Behavior of Entangled DNA Fluids (opens in a new tab)

  11. Rheology of Filled and Unfilled Polyurethanes for Reactive Extrusion-Based Applications

    … shear testing environments (e.g. sample loss/edge fracture, slip, and large sample size requirements). A literature review in Chapter 2 outlines the most recent advances in highly filled polyurethane processing for DIW, with a particular focus on how interparticle network recovery – in the …

    vt Repository record for Rheology of Filled and Unfilled Polyurethanes for Reactive Extrusion-Based Applications (opens in a new tab)

  12. Methoden zur Charakterisierung des nichtlinear viskoelastischen Verhaltens von Polymerschmelzen

    … zum Auftreten eines Schmelzebruch-Phänomens („edge fracture“). Der Schmelzebruch verändert die Probengeometrie und stellt somit einen limitierenden Faktor für die FTR-Methode darf. Die detailliertere Untersuchung dieses Bruchvorgangs hat gezeigt, dass es sich dabei um ein Phänomen handelt, dass …

    freiburg-diss Repository record for Methoden zur Charakterisierung des nichtlinear viskoelastischen Verhaltens von Polymerschmelzen (opens in a new tab)

  13. On the measurement of fracture toughness to understand the cracking resistance of advanced high strength steel sheets

    … cracking resistance. Premature cracking during edge forming operations (edge cracking) or the occurrence and propagation of cracks under impact loading are some of the common cracking related issues in processing and implementation of AHSS. To face these problems, the development of new …

    barcelona Repository record for On the measurement of fracture toughness to understand the cracking resistance of advanced high strength steel sheets (opens in a new tab)

  14. Untersuchung und Bestimmung der rheologischen Eigenschaften von Polyethylenschmelzen im konventionellen, kHz und MHz Frequenzbereich

    … ablaufen, können durch das Auftreten des sog. Edge Fracture Phänomens massive Messfehler auftreten. Der experimentell zugängliche Frequenz- und Deformationsbereich wird dadurch in einen stabilen und instabilen Bereich unterteilt. Die Richtigkeit einer Gleichung, die im Rahmen dieser und einer …

    freiburg-diss Repository record for Untersuchung und Bestimmung der rheologischen Eigenschaften von Polyethylenschmelzen im konventionellen, kHz und MHz Frequenzbereich (opens in a new tab)

  15. Nonlinear viscoelastic properties of branched polymers and flow instability of entangled polymers in the cone and plate geometry

    Rheological properties of long chain branched polymers, including commercial low density polyethylenes (LDPEs) and well-characterized hyperbranched polyiosbutylenes (PIBs) were studied here. The effects of chain architecture on viscoelastic properties are investigated from three perspectives. …

    ttu Repository record for Nonlinear viscoelastic properties of branched polymers and flow instability of entangled polymers in the cone and plate geometry (opens in a new tab)

  16. Ultra-broad molecular weight distributed multimodal blends of linear polyethylene: its linear and nonlinear viscoelastic properties and flow-induced crystallization ability

    … by the MWD of the polymers. Therefore, the knowledge of the MWD is indispensable. Knowing that the most used high-temperature size-exclusion chromatography often results in systematic errors in the UHMW region, linear viscoelastic analyses were carried out to overcome these problems. With the …

    freiburg-diss Repository record for Ultra-broad molecular weight distributed multimodal blends of linear polyethylene: its linear and nonlinear viscoelastic properties and flow-induced crystallization ability (opens in a new tab)

  17. Applied Rheology for Extrusion-Based Processing of Highly Filled Polymer Composites

    … materials (e.g. slippage, sample ejection, edge fracture, jamming, liquid phase migration). Capillary rheology is a widely applied tool to measure high shear rate behavior of fluids, however it suffers from a practical limitation of requiring large sample quantities for testing (tens of …

    vt Repository record for Applied Rheology for Extrusion-Based Processing of Highly Filled Polymer Composites (opens in a new tab)

  18. Étude expérimentale et numérique des mécanismes d'endommagement ductile et rupture des bords découpés des aciers avancés pour l'automobile

    La performance mécanique des pièces de structures automobiles fabriquées à partir de tôles d'acier à très haute résistance (THR) est souvent réduite à cause des bords découpés. Ce phénomène a été étudié pour deux nuances d'aciers ferrite-bainite (FB600) et ferrite-martensite (DP600), ce dernier …

    star-france Repository record for Étude expérimentale et numérique des mécanismes d'endommagement ductile et rupture des bords découpés des aciers avancés pour l'automobile (opens in a new tab)