Global ETD Search

Search theses and dissertations gathered from participating repositories worldwide. Every result links back to the library that holds it. No account is needed.

Results 1 to 20 of 42 for “"Enamic"”

  1. Effect of cyclic fatigue on the failure load of screw and cement-retained CAD/CAM implant crowns

    … with screw access holes sealed with composite or Enamic inlay. MATERIALS AND METHODS: For the screw-retained implant crowns, Ivoclar e.max and Vita Enamic CAD/CAM (n=44 for each material) and Enamic inlays (n=44) were designed using Sirona in-Lab software system (SW4 4.2.5) and milled using CEREC …

    bu Repository record for Effect of cyclic fatigue on the failure load of screw and cement-retained CAD/CAM implant crowns (opens in a new tab)

  2. Mechanical properties of dental resin composite CAD/CAM blocks

    … composite CAD/CAM blocks (Lava Ultimate and Enamic) and compare them to those of a widely-used ceramic CAD/CAM block (IPS e.max), that served as a control, in order to evaluate the clinical suitability of the former. Materials and Methods: Fifty bars of Lava Ultimate and Enamic and …

    ubc Repository record for Mechanical properties of dental resin composite CAD/CAM blocks (opens in a new tab)

  3. Enhanced Ceramic-based Interpenetrating Phase Composites via Pre-ceramic Chemical Necking

    … materials. One commercial IPC material, 1.8 g/cc Enamic (Vita Zahnfabrik, Germany), consists of an approximately 86% porous feldspathic porcelain matrix by weight and a copolymer of triethylene glycol dimethacrylate and urethane dimethacrylate. Although this IPC has comparable strength and …

    uconn-diss Repository record for Enhanced Ceramic-based Interpenetrating Phase Composites via Pre-ceramic Chemical Necking (opens in a new tab)

  4. Comparison of adherence of self-cured adhesive resin cement to lithium disilicate ceramics and ceramic resin composites using fracture mechanics

    … resin composites (Lava Ultimate – 3M ESPE and Enamic – Vita-Zahnfabrik) and a ceramic (IPS e.max – Ivoclar-Vivadent). Materials and Methods : Sixty specimens were prepared from each e.max and Enamic, and 120 specimens were prepared for Lava Ultimate. Ceramic resin composite blocks samples were …

    ubc Repository record for Comparison of adherence of self-cured adhesive resin cement to lithium disilicate ceramics and ceramic resin composites using fracture mechanics (opens in a new tab)

  5. Failure load of CAD/CAM-generated all ceramic posterior endocrowns

    … load of milled and bonded IPS e.max CAD and VITA ENAMIC endocrowns used in the restoration of endodontically molar teeth. MATERIALS AND METHODS: Typodont tooth # 30 was prepared with a central cavity to support the endocrowns. Fifty-eight epoxy resin dies were made from a physical impression of …

    bu Repository record for Failure load of CAD/CAM-generated all ceramic posterior endocrowns (opens in a new tab)

  6. Comparison Of Vickers Hardness Between Dental Ceramics And Hybrid Materials

    … Duo CAD), dual polymer hybrid ceramic (Vita Enamic) and resin ceramic hybrid (VarseoSmile Crown Plus). Vickers indenter (Wilson VH3100, Buehler) was used to create 6 pyramid-shaped indentations on each specimen and surface hardness was then measured. Results: A statistically significant …

    umn Repository record for Comparison Of Vickers Hardness Between Dental Ceramics And Hybrid Materials (opens in a new tab)

  7. In- vitro Wear of Four CAD-CAM Materials in the UAB Wear Simulating Device

    … ceramic/polymer hybrid materials (LAVA Ultimate, Enamic, and Cerasmart), 2 reference glass ceramics (IPS e.max and Celtra Duo), and 1 reference composite material (Paradigm MZ100). Methods: Flexural strength specimens (n=10) (2.5 × 2.5 × 16 mm) were prepared using a sectioning saw. After 24 …

    uab Repository record for In- vitro Wear of Four CAD-CAM Materials in the UAB Wear Simulating Device (opens in a new tab)

  8. Effect of surface finish on wear of ceramics

    … specimens (2×12×14 mm) were prepared using Vita Enamic, Vita Mark II, IPS e.max, and InCoris Zirconia TZI (n=48 for each material). Each material was divided into four main groups (n=12) according to their surface treatment (polished, machined, polished, then glazed, and machined, then glazed). …

    bu Repository record for Effect of surface finish on wear of ceramics (opens in a new tab)

  9. Flexural strength and marginal fit of two types of lithium disilicate ceramics for crowns

    … strength included: E.max press, E.maxCAD, ENAMIC, Experimental press, and Experimental-CAD. Each group (N= 10) was tested using the Instron 5566A using the piston-on-three-balls test. For the crown fit experiment an Ivorine tooth was prepared with a chamfer finish and used as the master …

    bu Repository record for Flexural strength and marginal fit of two types of lithium disilicate ceramics for crowns (opens in a new tab)

  10. The effects of machining on the flexural strength of CAD-CAM materials

    … CAD-CAM materials were used: VITA MARKII, VITA Enamic (VITA Zahnfabrik), Empress CAD, and e.max CAD (Ivoclar Vivadent). Rectangular bars for each material (except e.max CAD) were made by three procedures: saw cut, normal mill and fast mill. Each subgroup had a sample size of 5. Saw cut bars were …

    bu Repository record for The effects of machining on the flexural strength of CAD-CAM materials (opens in a new tab)

  11. Static and cyclic loading effects on fracture toughness of contemporary CAD/CAM restorative materials

    … (3M ESPE), IPS Empress® CAD (Ivoclar Vivadent), Enamic® (VITA), IPS e.max® CAD (Ivoclar Vivadent), and CERASMART™ (GC Dental). Polished rectangular bars 4×2×14 mm (n=30) were prepared from mill blocks for each material. Single notch of 0.5-1 mm in depth was made on the center of one length edge. …

    bu Repository record for Static and cyclic loading effects on fracture toughness of contemporary CAD/CAM restorative materials (opens in a new tab)

  12. Retention strength, failure load, and fatigue of various ceramics and cement combinations to titanium

    … using four crown materials (Ivoclar e.max, Vita Enamic, Vitablocs Mark II, and Sirona inCoris zirconia). Pins were held in a CNC machine to reproducibly sandblast each pin at the same speed and pressure (100 psi, Prepstar) using 125 micron alumina and then cleaned in an ultrasonic bath. The …

    bu Repository record for Retention strength, failure load, and fatigue of various ceramics and cement combinations to titanium (opens in a new tab)

  13. Prüfung der Zughaftfestigkeit von Komposit an Oberflächen neuer CAD/CAM- Hybridkeramiken nach künstlicher Alterung

    … Mann-Whitney-Test) signifikant beeinflusst. Bei Enamic zeigte sich kein statistisch signifikanter Unterschied zwischen den beiden Vorbehandlungswegen [17 (12,75; 23,00) und 20 (15,25; 22,00) MPa] [Med (Q 25; Q 75) MPa] und bei Suprinity lieferte die Vorbehandlung durch Sandstrahlen [29 (22,25; …

    fu-berlin Repository record for Prüfung der Zughaftfestigkeit von Komposit an Oberflächen neuer CAD/CAM- Hybridkeramiken nach künstlicher Alterung (opens in a new tab)

  14. Step-Stress Fatigue, Fracture Toughness and Load to Failure of an Additively Manufactured Ceramic Filled Hybrid Crown Material

    … between Varseosmile Crown Plus and Vita Enamic. Methods: Two materials were assessed in three tests. Six bars of both materials were utilized to assess fracture toughness following the ISO6872:2015[3] standard. The fracture toughness was assessed utilizing the single edge v-notch beam …

    iupui Repository record for Step-Stress Fatigue, Fracture Toughness and Load to Failure of an Additively Manufactured Ceramic Filled Hybrid Crown Material (opens in a new tab)

  15. Introduction of novel CAD/CAM fabricated esthetic interprenetrating phase ceramic orthodontic brackets; fracture and frictional resistance evaluation

    … brackets with a 0.018"×0.025" slot from Vita-Enamic interpenetrating phase ceramic (Vita Zahnfabrik) and Cerasmart (GC America) composite resin block. The brackets were subjected to separate tests (torque, tipping and sliding) using a universal testing machine. The average moments necessary to …

    bu Repository record for Introduction of novel CAD/CAM fabricated esthetic interprenetrating phase ceramic orthodontic brackets; fracture and frictional resistance evaluation (opens in a new tab)

  16. The fabrication of CaF₂-containing bioactive glass polymer-infiltrated ceramic network restorative material

    … block (Lava Ultimate) and RIPC block (Vita Enamic), were evaluated for biaxial flexural strength and Vickers hardness according to ISO standards (n=10, 10 mm diameter, and 2 mm thickness). Scanning electron microscopy (SEM) was employed to assess the microstructure of each material while …

    bu Repository record for The fabrication of CaF₂-containing bioactive glass polymer-infiltrated ceramic network restorative material (opens in a new tab)

  17. Propriedades mecânicas de resinas compostas diretas e de blocos de CAD/CAM de resina: revisão sistemática

    … de cerâmica híbrida, Amber Mill Hybrid, Vita Enamic, Katana Avencia, um à base de resina composta, Lava Ultimate e uma vitro cerâmica, Amber Mill. O estudo de Lauvahutanon et al (2014) foram testados quatro blocos CAD/CAM, um à base de resina composta, Block HC, Cerasmart e Gradia Block e Lava …

    coimbro Repository record for Propriedades mecânicas de resinas compostas diretas e de blocos de CAD/CAM de resina: revisão sistemática (opens in a new tab)

  18. Chipping, failure load and fatigue resistance of anterior veneers manufactured with CAD/CAM technology

    … were used; IPS Empress CAD, IPS e.max CAD, VITA ENAMIC and Lava Ultimate. Veneers were milled using a Sirona InLab MCXL at three different thicknesses, 0.4mm, 0.7mm and 1.0mm, n=10 for each group. Veneers were inspected under the light microscope to calculate the chipping factor (CF). All veneers …

    bu Repository record for Chipping, failure load and fatigue resistance of anterior veneers manufactured with CAD/CAM technology (opens in a new tab)

  19. Strain and load-to-fracture comparison of CAD-CAM dental implant crown materials under loading

    … containing a resin-reinforced glass network (Enamic). The screw access channel technique is frequently utilized to help clinicians retrieve cement-retained implant crowns when needed. One concern with screw access holes is the fracture resistance of the crown material after creating the access …

    ohiolink Repository record for Strain and load-to-fracture comparison of CAD-CAM dental implant crown materials under loading (opens in a new tab)

  20. Adherence of polyetheretherketone (PEEK) to different veneering materials and evaluation of the mechanical properties

    … from four materials; PEEK (Juvora), Vita Enamic, MarkII, and InCoris (Sirona). 144 specimens were divided into 12 groups and sectioned into plates (frameworks) and rods (veneers) for the shear bond strength test. The final dimension of each plate was about 18mm in length, 2mm thick, and …

    bu Repository record for Adherence of polyetheretherketone (PEEK) to different veneering materials and evaluation of the mechanical properties (opens in a new tab)

Page 1 of 3