Global ETD Search

Search theses and dissertations gathered from participating repositories worldwide. Every result links back to the library that holds it. No account is needed.

Results 1 to 20 of 22 for “"Environmental stress cracking"”

  1. IMPROVING THE UNDERSTANDING OF ENVIRONMENTAL STRESS CRACKING IN POLYETHYLENES

    … most common failures of plastics while in use is environmental stress cracking (ESC). Studies were conducted in this thesis to improve our understanding of ESC, through experimentation to modify the existing and most-used standardized test for ESC, namely the Bell Test (ASTM D-1693). Given the …

    mcmaster Repository record for IMPROVING THE UNDERSTANDING OF ENVIRONMENTAL STRESS CRACKING IN POLYETHYLENES (opens in a new tab)

  2. Methodologies for Obtaining Reliable Indicators for the Environmental Stress Cracking Resistance of Polyethylene

    Environmental stress cracking (ESC) is one of the main, and probably the most common, failure mechanisms involved in polymer fractures. This type of failure is critically important as it occurs suddenly, without any visible pre-fracture deformation. Such failure can be catastrophic and costly in …

    waterloo Repository record for Methodologies for Obtaining Reliable Indicators for the Environmental Stress Cracking Resistance of Polyethylene (opens in a new tab)

  3. Effects of Microcrystallinity on Physical Aging and Environmental Stress Cracking of Poly (ethylene terephthalate) (PET)

    … of microcrystallinity to physical aging and environmental stress cracking was systematically evaluated.</p><p>It is found that physical aging occurs in both amorphous and semi-crystalline PET stored above room temperature, but below the glass transition. Some physical property changes …

    ohiolink Repository record for Effects of Microcrystallinity on Physical Aging and Environmental Stress Cracking of Poly (ethylene terephthalate) (PET) (opens in a new tab)

  4. Studies of Environmental Stress Cracking of High Density Polyethylene Liner in Alkaline Surfactant Polymer Enhanced Oil Recovery Floods

    … polyethylene (HDPE) pipes in EOR process, environmental stress cracking (ESC) poses a threat to the integrity of the pipe in ASP floods. In this research, the ESC behaviour of HDPE pipes was studied in ASP floods under conditions that simulated the EOR reality. Particularly, tensile tests …

    calgary Repository record for Studies of Environmental Stress Cracking of High Density Polyethylene Liner in Alkaline Surfactant Polymer Enhanced Oil Recovery Floods (opens in a new tab)

  5. Investigating Alternative Testing Techniques for Evaluating the Environmental Stress Cracking Resistance of Polyethylenes in Contact with Ageing Fluids

    Environmental stress cracking (ESC) is a significant problem that has plagued the plastics industry since its discovery nearly 70 years ago. The accelerated brittle failure brought about when a stressed polymer comes in contact with an aggressive environment can happen suddenly with destructive …

    mcmaster Repository record for Investigating Alternative Testing Techniques for Evaluating the Environmental Stress Cracking Resistance of Polyethylenes in Contact with Ageing Fluids (opens in a new tab)

  6. Vliv detergentů na urychlení testů životnosti u PE trubkových materiálů.

    … ISO (ISO 16770: Plastics - Determination of environmental stress cracking (ESC) of Polyethylene (PE) - Full Notch Creep Test (FNCT)). Jako detergent byl použit vzduch, destilovaná voda, Arkopal N 090 a Arkopal N 110.

    brno-tech Repository record for Vliv detergentů na urychlení testů životnosti u PE trubkových materiálů. (opens in a new tab)

  7. The crosslinking of polyethylene by ultraviolet radiation

    … improved, especially the flow properties and the environmental stress cracking resistance (ESCR). Other properties such as Tensile strength, Glass transition temperature (Tg) and melting temperature (Tm) were not greatly affected. The significant improvement in the flow properties was due to the …

    strathclyde Repository record for The crosslinking of polyethylene by ultraviolet radiation (opens in a new tab)

  8. INVESTIGATING THE COMPATIBILITY OF BIODIESEL ON POLYETHYLENE THROUGH NONDESTRUCTIVE AND TRADITIONAL METHODS

    … of unexpected brittle failures of polymers, environmental stress cracking (ESC) is a major issue for the plastics industry, accounting for approximately 15-40% of all plastic part failures in service. ESC is an intriguing phenomenon that is not yet well understood, which relates to the …

    mcmaster Repository record for INVESTIGATING THE COMPATIBILITY OF BIODIESEL ON POLYETHYLENE THROUGH NONDESTRUCTIVE AND TRADITIONAL METHODS (opens in a new tab)

  9. Mechanical and Chemical Properties of High Density Polyethylene: Effects of Microstructure on Creep Characteristics

    Environmental stress cracking (ESC) can result in catastrophic failure of polyethylene (PE) structures without any visible warning. The use of PE in more demanding applications, such as trenchless piping, can accelerate ESC failure of the material. Besides public safety issues, the replacement and …

    waterloo Repository record for Mechanical and Chemical Properties of High Density Polyethylene: Effects of Microstructure on Creep Characteristics (opens in a new tab)

  10. An assessment of the performance of high density polyethylene copolymers for natural gas distribution pipes

    … the major influences being in the long-term hoop stress resistance and the environmental stress cracking resistance. Minor amounts of hexene-1 are more effective than comonomers lower in the homologous series, although there is some sacrifice of density related properties. A synergistic …

    aston Repository record for An assessment of the performance of high density polyethylene copolymers for natural gas distribution pipes (opens in a new tab)

  11. Estudo do efeito combinado da degradação por radiação gama e fratura sob tensão ambiental (ESC) nas propriedades de polímeros vítreos

    … a degradação por fratura sob tensão ambiental (environmental stress cracking ou ESC) de alguns polímeros vítreos, o poli(metacrilato de metila), o poliestireno e o poli (metacrilato de metila) tenacificado (PMMA-t), após esses polímeros terem sido submetidos a diferentes doses de radiação gama. …

    brazil-ufpe Repository record for Estudo do efeito combinado da degradação por radiação gama e fratura sob tensão ambiental (ESC) nas propriedades de polímeros vítreos (opens in a new tab)

  12. Estudo do tensofissuramento em geomembranas de polietileno de alta densidade utilizadas em aterros de resíduos

    … ambiental de corpo de prova dobrado (Bent Strip Environmental Stress Cracking). Neste ensaio algumas amostras foram banhadas em solução tensoativa, conforme preconiza a norma, enquanto outras foram ensaiadas banhadas em chorume, numa adaptação à metodologia normalizada. No segundo ensaio, corpos …

    brazil-ufrgs Repository record for Estudo do tensofissuramento em geomembranas de polietileno de alta densidade utilizadas em aterros de resíduos (opens in a new tab)

  13. Effects of liquid environments on the mechanical fatigue behavior of polyethylene

    Environmental stress cracking (ESC) of polyethylene (PE) in the presence of active liquid environments results in fracture under applied stress conditions much lower than for failure in the absence of the ESC agent. However, recent studies have shown that the fatigue lifetime of high density …

    ohiolink Repository record for Effects of liquid environments on the mechanical fatigue behavior of polyethylene (opens in a new tab)

  14. Effect of intermediate solvents on poly(ether ether ketone)

    … microtensile tests, and tensile test in the environmental scanning electron microscope (ESEM)), which were first verified with another semi-crystalline thermoplastic polymer, isotactic polypropylene. PEEK specimens were stressed in the inside of glass cones and immersed in a series of …

    vt Repository record for Effect of intermediate solvents on poly(ether ether ketone) (opens in a new tab)

  15. Role of Crystallinity on Failure Variability in ASTM D1693 Bell Test

    … from the ASTM D1693 ‘Standard Test Method for Environmental Stress-Cracking of Ethylene Plastics’ (aka Bell Test) for high-density polyethylene (HDPE) was hypothesized in this project to be primarily caused by variation in crystallinity within molded test plaques. The broad molecular weight …

    mcmaster Repository record for Role of Crystallinity on Failure Variability in ASTM D1693 Bell Test (opens in a new tab)

  16. Solvent induced microcracking in high performance polymeric composites

    The first paper, “Dye Penetrant Induced Microcracking in High-Performance Thermoplastic Polyimide Composites”, studied the possibility of spurious microcracking in three high-performance thermoplastic polyimide composite materials due to zinc iodine dye penetrant. The material systems were …

    vt Repository record for Solvent induced microcracking in high performance polymeric composites (opens in a new tab)

  17. Biostability and Biocompatibility of Modified Polyurethane Elastomers

    … the degraded surface layer buckled with applied stress as opposed to the cracking observed in PEU. Environmental stress cracking has been reported as the primary failure mechanism of poly(ether urethanes) in medical devices. Therefore, the clinical relevance of these findings to poly(carbonate …

    ohiolink Repository record for Biostability and Biocompatibility of Modified Polyurethane Elastomers (opens in a new tab)

  18. Strukturbezogene Betrachtung zum Zeitstandverhalten geschweißter Polyolefinhalbzeuge

    Die Kunststoffschweißverfahren Infrarot- und Vibrationsschweißen sind in der Serienfertigung etablierte Fügetechnologien. Sie sind durch eine wirtschaftliche und effiziente Prozessführung gekennzeichnet und sind verfahrenstechnisch prinzipiell zum Einsatz im Apparate-, Behälter- und Rohrleitungsbau …

    qucosa-diss Repository record for Strukturbezogene Betrachtung zum Zeitstandverhalten geschweißter Polyolefinhalbzeuge (opens in a new tab)

  19. The effect of environmental aging/exposure on the durability of high performance polymeric composites

    … However, the long-term durability and environmental stability of these materials continue to be under question. Continued application of these composites in aerospace structures is contingent upon the long-term durability of these material systems. Polymeric materials have been known to …

    vt Repository record for The effect of environmental aging/exposure on the durability of high performance polymeric composites (opens in a new tab)

Page 1 of 2