  1. Factors influencing the Nucleation and Morphology of Crystallographic Type Etch Pits in Pure Iron.

    <p> Etch pits can be produced in iron whose shape reflects the crystallography of the crystal. It is shown that pit morphology can be adequately predicted from an orientation dependent dissolution theory. The influence of an air-formed surface oxide film on pit nucleation and morphology is …

    mcmaster Repository record for Factors influencing the Nucleation and Morphology of Crystallographic Type Etch Pits in Pure Iron. (opens in a new tab)

  2. A model for initiation of aluminum etch tunnels

    In the past, tunnel etching of aluminum has been used primarily in the production of electrolytic capacitors. Research has therefore focussed on the parameters which will increase capacity. The increase in capacity obtained is in direct proportion to the increase in effective surface area. However, …

    iastate Repository record for A model for initiation of aluminum etch tunnels (opens in a new tab)

  3. Microbial diagnesis in terrestrial aquifer conditions : laboratory and field studies

    … quartz and microcline were in close proximity to etch pits, exhibiting a spatial correlation between bacteria location and etch pits. The etch pits, however, were not localized at the actual contact surface of the microbe, and the euhedral shape and extent of etching suggest the mineral surface …

    texas Repository record for Microbial diagnesis in terrestrial aquifer conditions : laboratory and field studies (opens in a new tab)

  4. A Study of Lithium Flouride Etch Morphologies using Silica Gel

    <p>Cleavage surfaces of lithium fluoride are etched on a silica hydrogel containing ferric ions as inhibitor. The gel eliminates turbulence in the system and retards the diffusion of ferric ions towards the dissolving interface. The dissolution etch pits and features are examined by interference …

    mcmaster Repository record for A Study of Lithium Flouride Etch Morphologies using Silica Gel (opens in a new tab)

  5. A Quantitative Study of Etch Morphology of (0001) Zinc Cleavages

    The (0001) plane of zinc monocrystals were etched over a range of HCl/95% ethyl alcohol solutions for different etch times to produce etch pits. The etched surface was examined on the Zeiss interference microscope and from the interferograms made pits slopes, depths and rate of deepening were …

    mcmaster Repository record for A Quantitative Study of Etch Morphology of (0001) Zinc Cleavages (opens in a new tab)

  6. Scanning Tunneling Microscopy of Homo-Epitaxial Chemical Vapor Deposited Diamond (100) Films

    … is based on an amorphous carbon layer that is etched or converted to diamond by atomic hydrogen. With further exposure to atomic hydrogen at 500° C, etch pits were observed in the shape of inverted pyramids with {111} oriented sides. The temperature dependence of atomic hydrogen etching of the …

    unt Repository record for Scanning Tunneling Microscopy of Homo-Epitaxial Chemical Vapor Deposited Diamond (100) Films (opens in a new tab)

  7. Impurities and the Evaporation Morphology of Zinc Single Crystals

    … zinc single crystals are presented. Dislocation etch pits developed on (0001) zinc cleavage surfaces. A mechanism is proposed to account for enhanced evaporation at decorated dislocations. The observation of macroledges on pit faces is reported and attributed to impurity-induced bunching of …

    mcmaster Repository record for Impurities and the Evaporation Morphology of Zinc Single Crystals (opens in a new tab)

  8. The effects of surface roughness and stress on lattice gas models using kinetic Monte Carlo modeling

    … was studied as the origin of the formation of etch-pits at dislocations. Atoms from a diamond cubic lattice were irreversibly removed with a probability which depends on an local surface configuration as well as on the local stress developed from its physical location with respect to a …

    arizona-thes Repository record for The effects of surface roughness and stress on lattice gas models using kinetic Monte Carlo modeling (opens in a new tab)

  9. Plastic deformation of gallium arsenide

    … samples obtained by counting dislocation etch pits indicate that the density of dislocations in deformed GaAs is directly related to the applied stress, the plastic strain rate, the test temperature while being inversely related to the applied strain rate.

    ubc Repository record for Plastic deformation of gallium arsenide (opens in a new tab) Download PDF for Plastic deformation of gallium arsenide (opens in a new tab)

  10. Streaking on Aluminium Alloy Extrusions

    … the evolution of streaking after different etch durations needed to be examined as this type of finding has not been reported in literature. The streaking observed therefore might not be the same for all levels of material removal. To conduct this research on streaking, samples were …

    auckland-tech Repository record for Streaking on Aluminium Alloy Extrusions (opens in a new tab)

  11. Electrochemical and surface topographic studies of oxide film passivation of aluminum

    <p>Passivation of corroding surfaces in aluminum etch pits and tunnels was investigated by step reductions and cathodic pulses in applied etching current. Morphology study shows that, in the early stage of passivation, the corroding surface consisted of recessed patches, which are actively …

    iastate Repository record for Electrochemical and surface topographic studies of oxide film passivation of aluminum (opens in a new tab)

  12. Growth of hexagonal boron nitride on electrochemically prepared polycrystalline copper substrates

    … effects during electropolishing, such as etch pits, arise from the standard electropolishing recipe of concentrated H3PO4. These secondary effects, ascribed to oxygen bubbling at random nucleation sites on Cu surface, can be overcome by using additives, such as acetic acid and ethylene …

    maryland Repository record for Growth of hexagonal boron nitride on electrochemically prepared polycrystalline copper substrates (opens in a new tab)

  13. Chemical Weathering of the Mafic Minerals Serpentine and Olivine in Natural Environments

    … an arid environment at Black Rock Flow, Nevada. Etch pits, an apparent dissolution feature, were observed and used to measure a surface-area normalized rate of olivine dissolution (3.48×10-15mol forsterite/m2s). These findings help quantify the incipient processes affecting serpentine soil …

    unlv Repository record for Chemical Weathering of the Mafic Minerals Serpentine and Olivine in Natural Environments (opens in a new tab) Download PDF for Chemical Weathering of the Mafic Minerals Serpentine and Olivine in Natural Environments (opens in a new tab)

  14. A general kinetic model: Kinetics and atomic-scale mechanisms of feldspar dissolution

    … evolution of a (001) surface of barite etched in pure water. The generation of two sets of oppositely-oriented triangular etch pits in consecutive atomic layers validates the model's efficiency. It is the first stochastic treatment out of numerous studies concerning barite dissolution to …

    rice Repository record for A general kinetic model: Kinetics and atomic-scale mechanisms of feldspar dissolution (opens in a new tab)

  15. Characterization and fabrication of a (6H)-SiC as a piezoresistive pressure sensor for high temperature applications

    … photoconductive selectivity techniques to etch the piezoresistors were developed. Techniques to wet etch the cavities in a dark current mode were developed, resulting in 25 um diaphragms free of etch-pits and hillocks. Average etch-rates between 0.6 and 0.8 um/min were achieved. Ti/TiN/Pt …

    njit Repository record for Characterization and fabrication of a (6H)-SiC as a piezoresistive pressure sensor for high temperature applications (opens in a new tab)

  16. Dislocations in gallium arsenide deformed at high temperatures

    … was established by cathodoluminescence (CL). Etch pits produced by molten KOH on examined crystal surfaces coincided with the CL images. The test pieces were capped with Si₃N₄, heated to between 950 and 1050°C, and plastically deformed by bending. The dislocation configuration after bending …

    ubc Repository record for Dislocations in gallium arsenide deformed at high temperatures (opens in a new tab) Download PDF for Dislocations in gallium arsenide deformed at high temperatures (opens in a new tab)

  17. The Chemical And Physical Mechanisms Determining The Morphology Of Wet-Chemically Etched Si(100)

    … harsh cleaning processes roughen silicon wafers, etchants that can produce smooth Si(100) surfaces have been a long-standing goal of the microelectronics industry. In this work, scanning tunneling microscopy was used to investigate the morphologies of wet-chemically-etched Si(100) surfaces, …

    cornell Repository record for The Chemical And Physical Mechanisms Determining The Morphology Of Wet-Chemically Etched Si(100) (opens in a new tab)

  18. Assessing the Reactive Surface Area of Phlogopite during Acid Dissolution: An Atomic Force Microscopy, X-ray Photoelectron Spectroscopy, and Low Energy Electron Diffraction Study

    … by measuring the volume of material removed from etch pits, and normalizing to either the "reactive" surface area of {hk0} edges exposed at pit walls, or to a total "BET-equivalent" surface area. Rates normalized to total surface area are in the range of dissolution rates reported in the …

    vt Repository record for Assessing the Reactive Surface Area of Phlogopite during Acid Dissolution: An Atomic Force Microscopy, X-ray Photoelectron Spectroscopy, and Low Energy Electron Diffraction Study (opens in a new tab)