Global ETD Search
Search theses and dissertations gathered from participating repositories worldwide. Every result links back to the library that holds it. No account is needed.
Results 1 to 20 of 29 for “"FIB-TEM"”
-
Valutazione dell'emostasi mediante tromboelastometria (ROTEM®) durante la rianimazione fluida con amido idrossietilico 130/0,4 (VOLUVEN®) o soluzione salina ipertonica 7,5% in cani con dilatazione/torsione gastrica
… per analisi mediante tromboelastometria (ROTEM) e test coagulativi di routine (PT, aPTT, fibrinogeno). Lo studio ha incluso 13 cani nel gruppo HES e 10 cani nel gruppo HS. All’ammissione tutti i cani hanno presentato tracciati ROTEM classificati come normali, tranne 1/13 cani che è risultato …
-
Mechanism of Corrosion by Naphthenic Acids and Organosulfur Compounds at High Temperatures
… the corrosive property of crudes at high temperatures, the mechanism of corrosion by acids (naphthenic acids) in the presence of organosulfur compounds, and methods to mitigate its corrosive effect.In 2004, an industrial project was initiated at the Institute for Corrosion and Multiphase …
-
Iron-oxide and carbonate formation and transformations from banded iron formations 2.7 to 2.4 Ga
… à transmission à faisceau d’ions focalisé (FIB-TEM) révèle la présence de plaquettes de nano ferrihydrite dans les BIF dolomitiques (carbonate d’itabirite). La dolomite est interprétée comme étant une phase primaire précipitée à des températures plus élevées (~100°C) de fluides hydrothermaux …
-
On a novel technique for preparation and analysis of the implant surface and its interface to bone
… studies using focused ion beam microscopy (FIB) for transmission electron microscopy analysis have shown promising results. The general aim of the thesis was to evaluate FIB for TEM sample preparation using different lift-out techniques and protection modes applied on the implant surface and …
-
Contribution à la compréhension des mécanismes de fluage de l’acier austénitique inoxydable 316L(N) pour 60 ans de durée de fonctionnement : lien évolution microstructurale (précipités, dislocations) et endommagement
… Echangeurs Intermédiaires, …) sont soumis à des températures allant de 400°C à 575°C pour une durée de fonctionnement pouvant atteindre 60 ans pour les composants non remplaçables. A ces températures, l'acier inoxydable austénitique 316L(N) retenu pour ces applications est soumis au …
-
Localized CO2 Corrosion in the Presence of Organic Acids
… on X65 carbon steel. This leads directly to a temporary increase in the corrosion rate. However, the final corrosion rate does not seem to be affected. This raises the possibility that there may be a different phase conferring protection on the steel surface. This phase (corrosion scale) was …
-
Spark plasma sintering de composites base titane renforcés par des carbures pour applications en tribocorrosion
… de particules. On s'est rendu compte qu'à une température de consigne de 800°C, la réaction avait commencé en raison des avantages du courant pulsé dans le SPS. L'analyse SEM / FIB / TEM sur le matériau fritté à 800°C a montré une phase grise continue, constituée d'amas de particules de B4C …
-
Grenzflächenreaktionen in refraktären Metall-Keramik-Verbundwerkstoffen
Feuerfeste Werkstoffe spielen für die erzielbaren Temperaturen in Hochtemperaturprozessen eine entscheidende Rolle, die eingesetzten Keramiken -- beispielsweise Al$_2$O$_3$ -- sind allerdings anfällig für ein Versagen durch Thermoschock. Die dafür verantwortlichen, prozessbedingt großen …
-
Impact du vieillissement de l'additif MoDTC sur ses propriétés tribologiques pour les contacts acier-acier et DLC-acier
… interne. La réduction des pertes par frottement et une plus faible consommation du carburant représentent différents aspects sur lesquels il est possible d’intervenir dans ce sens. Pour diminuer les pertes par frottement, plusieurs approches ont été utilisées, soit au niveau du design des …
-
Reduction of carbon dioxide into value added chemicals and fuel
Electrochemical CO2 reduction reaction (CO2RR) systems are a viable strategy to mitigate the rising CO2 level in the atmosphere. If powered by photovoltaic cells, these systems also shed light onto the storage as well as the distribution of the intermittent and diffusive solar energy. At present, …
-
Copper and Silicon: Implications for the Long-term Stability of Plated Contacts for Silicon Solar Cells
… using advanced lifetime spectroscopy of temperature and injection-dependent lifetime curves, with two defect levels identified at Et-Ei = −(0.14-0.16) eV and Et-Ei = (0.08-0.11) eV. Different capture cross-section ratios were obtained for Cu precipitates formed under illumination (k = 1.4 …
-
Designing synergetic chemical modifications to substrate coating and lubricant additives: a novel strategy to reduce friction and wear
… environmental sustainability in mechanical systems, innovations in surface coating technologies and a re-evaluation of conventional lubricant additives have gained significant attention. Diamond-like carbon (DLC) coatings are widely used for wear protection due to their excellent hardness and …
-
Correlated SEM, FIB, and TEM Studies of Material Collected by the NASA Stardust Spacecraft
… Electron Microscopy (SEM), Focused Ion Beam (FIB) sample preparation, and Transmission Electron Microscopy (TEM). Investigations of the Stardust aerogels are conducted with plasma ashing sample preparation followed by detailed characterization of the material with TEM. Additional studies of …
-
Aerogels catalítics de Co-Si sobre monòlits ceràmics per a produir hidrogen mitjançant la reformació d'etanol
… this reaction with high selectivity at low temperature. Cobalt talc dispersed in silica aerogelscoating ceramic honeycombs and Co talc-coated ceramic honeycombs were selected as catalysts for ESR at 300-500 °C. The addition of small amounts of Fe and K to the aerogel-dispersed catalyst was …
-
Study of ultrashort laser-pulse induced ripples formed at the interface of silicon-dioxide on silicon
… interface of SiO2 and Si were studied in a systematic fashion by irradiating the SiO2-Si samples with ultrashort laser pulses under a broad variety of experimental conditions. They consist of di↵erent irradiating laser wavelengths, incident laser energies, translation speeds, translation …
-
Investigation into the surface modification of Ti-6Al-4V to facilitate antimicrobial ionic silver integration for use in implantable orthopaedic devices
… directly in contact with bacteria, with no attempt to measure silver release rate profiles. The research in this dissertation aimed to investigate methodologies for the incorporation of silver into a modified surface of Ti-6Al-4V in order to facilitate an antimicrobial effect for use in …
-
Causes for slow weathering and erosion in the steep, warm, monsoon-subjected Highlands of Sri Lanka
… chemical, and electron-microscopic (SEM, FIB, TEM) analyses to identify the factors limiting the rate of weathering front advance in the profile, the sequence of weathering reactions, and the underlying mechanisms. The first mineral attacked by weathering was found to be pyroxene initiated …
-
GEOCHEMICAL FACTORS AFFECTING THE TRANSPORT AND REACTIVITY OF METALS AND PYRITE COLLOIDS IN COAL MINE SPOILS
… analyzed by transmission electron microscopy (FIB-TEM), X-ray diffraction (XRD), and synchrotron-based X-ray Microprobe (XMP) analyses was conducted to determine the morphology elemental, and mineral composition and oxidation state of the colloids. Chapter 1 includes the historical background …
-
Insights into Fluid-Rock Interactions on the CV3 Carbonaceous Chondrite Asteroid: The Complex Record in the Allende-like CV3 Chondrite, NWA 2364.
… oxidized and reduced, contain primitive solar system materials that provide many insights into early solar system processes. Both subgroups record significant evidence of secondary alteration that has modified their primary characteristics. In this work, we have studied the petrography, …
-
Initiation and Propagation of Localized Corrosion of Mild Steel in Marginally Sour Environments
A systematic investigation of pitting failure of mild steel in marginally sour environments was performed with the objective of understanding and predicting the occurrence of localized corrosion. While localized corrosion can happen due to a variety of reasons, recent work has shown that mild steel …
Page 1 of 2