Global ETD Search

Search theses and dissertations gathered from participating repositories worldwide. Every result links back to the library that holds it. No account is needed.

Results 1 to 20 of 74 for “"Failure envelope"”

  1. Measurement of the through-thickness strength of composites

    … field at the test section. A two dimensional failure envelope is defined for each laminate configuration using the experimentally obtained data. All three independent laminate configurations exhibited almost identical failure envelopes. The woven laminate exhibited superior interlaminar shear …

    oxford Repository record for Measurement of the through-thickness strength of composites (opens in a new tab)

  2. Error-in-variables for failure criteria applied to the near -wellbore region

    … to improve the parametric representation of the failure criteria used to characterize rock strength of a reservoir rock in the near-wellbore region is the focus of this study. We adopted a statistical method, so-called error-in-variables (EIV), to take into account experimental errors in all of …

    tamu Repository record for Error-in-variables for failure criteria applied to the near -wellbore region (opens in a new tab)

  3. Flexural Strength of Steel Beams with Holes in the Tension Flange

    … uses finite element analysis to simulate the failure mode of tension flange fracture caused from flexure in W-shapes with holes in the tension flange. Using a material failure envelope previously developed for aluminum extrusions through the IDS (instability, ductile, and shear) criterion and …

    ohiolink Repository record for Flexural Strength of Steel Beams with Holes in the Tension Flange (opens in a new tab)

  4. Response and Failure of Adhesively Bonded Automotive Composite Structures under Impact Loads

    … system and used to create a fracture failure envelope. Because load measurements become erratic and unreliable at higher test rates, displacement-based relationships were used to quantify these energy release rates. Displacement data was collected with an imaging system that utilized …

    vt Repository record for Response and Failure of Adhesively Bonded Automotive Composite Structures under Impact Loads (opens in a new tab)

  5. FIELD INSTRUMENTATIONS AND NUMERICAL ANALYSIS OF GEOSYNTHETIC REINFORCED SOIL – INTEGRATED BRIDGE SYSTEM (GRS-IBS)

    … demonstrated that the possible potential failure envelope of the GRS-IBS abutment was found to be a combination of a punching shear failure at the top and Rankine failure surface at the bottom, in which the failure envelope is developed under the inner edge of the footing and extending …

    lsu-thes Repository record for FIELD INSTRUMENTATIONS AND NUMERICAL ANALYSIS OF GEOSYNTHETIC REINFORCED SOIL – INTEGRATED BRIDGE SYSTEM (GRS-IBS) (opens in a new tab)

  6. Sampling and strength testing an unbonded locked sand

    … 100kPa these were suppressed and a bilinear failure envelope formed. Normal loads of 10MPa and above produced more rock like behaviour; peak strength was not suppressed and plumose structures were formed.</p><p>The triaxial tests did not produce a bilinear failure envelope, although changes …

    soton Repository record for Sampling and strength testing an unbonded locked sand (opens in a new tab)

  7. Formulation and Application of a New Critical State Model for Clays

    … (OC) clays and clays under cyclic loading. A failure envelope based on the experimental findings enters into the model formulation. The peak strength of heavily OC clay can be predicted satisfactorily. Comprehensive comparisons of model predictions with test data are conducted on various clays …

    nus Repository record for Formulation and Application of a New Critical State Model for Clays (opens in a new tab)

  8. A Model for Prediction of Fracture Initiation in Finite Element Analysis of Bolted Steel Connections

    … connections using damage mechanics. A material failure envelope has previously been developed for aluminum extrusions using the IDS (instability, ductile, and shear) criterion. The IDS criterion is a damage mechanics based model for defining failure envelopes. These failure envelopes are …

    ohiolink Repository record for A Model for Prediction of Fracture Initiation in Finite Element Analysis of Bolted Steel Connections (opens in a new tab)

  9. Damage Development in Static and Dynamic Deformations of Fiber-Reinforced Composite Plates

    … variables and the delamination by postulating a failure envelope in terms of the transverse stresses; the damage degrades elastic moduli. The delamination of adjoining layers is simulated by the nodal release technique. Coupled nonlinear partial differential equations governing deformations of a …

    vt Repository record for Damage Development in Static and Dynamic Deformations of Fiber-Reinforced Composite Plates (opens in a new tab)

  10. PROGRESSIVE MICROSCOPIC DAMAGE AND THE DEVELOPMENT OF MACROSCOPIC FRACTURE IN POROUS SANDSTONES

    … damage induced dilatancy precedes macroscopic failure of a rock. However, the quantitative relationship between microstructural damage and fault development is not clearly understood. To better understand the mechanics of brittle faulting of rock and the association of precursory phenomena with …

    maryland Repository record for PROGRESSIVE MICROSCOPIC DAMAGE AND THE DEVELOPMENT OF MACROSCOPIC FRACTURE IN POROUS SANDSTONES (opens in a new tab)

  11. The triaxial load response of grain

    … does not. The tests also show that the Mohr failure envelopes are not linear, as normally assumed, but are concave downwards. General expressions for the compression loading tangent modulus and the Mohr failure envelope are developed, and the parameters for the four grains, each at three bulk …

    iastate Repository record for The triaxial load response of grain (opens in a new tab)

  12. Compressive behavior of laminated composite structures

    … seem to be possible reasons for the premature failure. However, since many of the failures are characterized by delamination of the structures, the cause of the failure may be due to local buckling of the composite plies. In this dissertation, a ply buckling model is studied to assist in the …

    nebraska Repository record for Compressive behavior of laminated composite structures (opens in a new tab)

  13. Development of Improved Methods for Quantifying the Multiaxial Failure of Soft Materials.

    … materials. Developing criteria that map the failure of materials under multiaxial stress states is therefore essential for material selection. Although such analyses have long been applied to quantify the yielding behavior of stiff materials such as metals and glassy polymers, limited …

    ohiolink Repository record for Development of Improved Methods for Quantifying the Multiaxial Failure of Soft Materials. (opens in a new tab)

  14. Effect of CEC, Salinity, Sand Content, and Particle Size Distribution on Mud Rock Properties

    … testing is commonly used to determine the failure envelope for mudrocks. The most common application of this technique requires multiple identical samples. In heterogeneous formation identical samples are often difficult to obtain. The twinning problem is overcome by performing ‘multistage’ …

    houston Repository record for Effect of CEC, Salinity, Sand Content, and Particle Size Distribution on Mud Rock Properties (opens in a new tab)

  15. Early age and durability study of the bond strength on the interface between UHPC – HSC

    … Carol’s approaches were adopted to construct the failure envelope and the experimental results were subsequently used to estimate the cohesion and friction coefficients at the bond interface. The overall interface bond performance of the small-scale specimens was satisfactory. The direct tensile …

    manitoba Repository record for Early age and durability study of the bond strength on the interface between UHPC – HSC (opens in a new tab)

  16. The failure of graphite arc-furnace electrodes

    … to contribute to particular types of electrode failure. In this computer-aided analysis of the stresses induced by the above effects, a commercial finite element program is used in conjunction with a purpose-written finite difference program. Mechanical loads due to electrode self-weight and …

    durham Repository record for The failure of graphite arc-furnace electrodes (opens in a new tab)

  17. Dependency on the strain rate, temperature, and moisture content of the uniaxial and multiaxial mechanical behaviour of syntactic foams

    … strain rate, and temperature on the multiaxial failure envelope of a polyamide syntactic foam is assessed experimentally. The multiaxial failure stress loci of the material at different temperature and strain rates are analysed, discussed, and interpreted using the pressure-dependent …

    oxford Repository record for Dependency on the strain rate, temperature, and moisture content of the uniaxial and multiaxial mechanical behaviour of syntactic foams (opens in a new tab) Restricted access

  18. Observations on non-linear rock mass strength from the Nantlle Valley, Gwynedd, Wales

    … of slopes and underground excavations. Two failure criteria are discussed: The Generalised Hoek-Brown criterion defined in terms of maximum and minimum principal stress, and Barton’s criterion in terms of normal and shear stress. The Generalised Hoek-Brown criterion defines non-linearity and …

    birmingham Repository record for Observations on non-linear rock mass strength from the Nantlle Valley, Gwynedd, Wales (opens in a new tab)

  19. A comprehensive experimental study of the fracture behavior of granite under three dimensional loading, at ambient temperature and 300 F /

    … These results are compared with the classical failure theories of Coulomb-Mohr and Drucker and Prager. It is observed that none of the above criteria are able to predict the failure over the entire range of stresses, and at different temperatures. A new failure criterion based on the strain …

    oklahoma-thes Repository record for A comprehensive experimental study of the fracture behavior of granite under three dimensional loading, at ambient temperature and 300 F / (opens in a new tab)

Page 1 of 4