  1. Laboratory Evaluation of Hot-Mix Asphalt Concrete Fatigue Cracking Resistance

    … these mixture types are now more susceptible to fatigue cracking. The primary goal of this study was to evaluate fatigue cracking test methods and recommend that which is both simple and robust, especially in qualifying commonly used Texas mixture types. One way to minimize fatigue cracking is …

    tamu Repository record for Laboratory Evaluation of Hot-Mix Asphalt Concrete Fatigue Cracking Resistance (opens in a new tab)

  2. Wear and Fatigue Resistance: An In-Vitro Comparison of Three Materials for Vacuum-Formed Retainers

    AbstractAim: To test the wear and fatigue resistance of three materials for the fabrication of vacuum-formed retainers in a simulated oral environment. Methods: Three materials were tested: Essix ACE, Taglus, and Zendura. To test wear resistance, 21 maxillary retainers of each material (63 overall) …

    umn Repository record for Wear and Fatigue Resistance: An In-Vitro Comparison of Three Materials for Vacuum-Formed Retainers (opens in a new tab)

  3. Laboratory Investigation of Fatigue Resistance of Thin and Standard Thicknesses of Asphalt Surfaces Incorporating Fibre-Reinforced Mixes and Cape Seals Using Beam Testing

    … asphalt layer is reduced because of increased fatigue movement. This research investigates the specific application of thin asphalt surfaces typically constructed on bound and unbound granular layers. It also investigates the application of Cape Seal layers on thin asphalt surfaces. The …

    auckland-ms Repository record for Laboratory Investigation of Fatigue Resistance of Thin and Standard Thicknesses of Asphalt Surfaces Incorporating Fibre-Reinforced Mixes and Cape Seals Using Beam Testing (opens in a new tab)

  4. Efeito de diferentes protocolos de acabamento/polimento na resistência à fadiga e módulo de Weibull de diferentes tipos de zircônia

    … different finishing/polishing protocols on the fatigue strength of new generations of zirconia. Materials and Methods: Ninety (N=90) ceramic discs (Ø:12mm; 1.5mm-ISO 6872) were made, 45 of ultra-translucent zirconia (UT-VITA, Vita Zahnfabrik) and 45 of a hybrid zirconia ceramic 3Y-TZP and 5Y-PSZ …

    brazil-ufrn Repository record for Efeito de diferentes protocolos de acabamento/polimento na resistência à fadiga e módulo de Weibull de diferentes tipos de zircônia (opens in a new tab)

  5. Využití metody digitální korelace obrazu při zkouškách asfaltových směsí

    Dnešná doba ponúka inovatívnejšie metódy pre skúšky asfaltových zmesí oproti tým konvenčným. Metóda digitálnej korelácie obrazu sa čoraz viac používa ako doplnok, alebo aj ako náhrada niektorých postupov pri skúškach asfaltových zmesí. Cieľom tejto bakalárskej je overiť možné pozitívne využitie …

    brno-tech Repository record for Využití metody digitální korelace obrazu při zkouškách asfaltových směsí (opens in a new tab)