Global ETD Search
Search theses and dissertations gathered from participating repositories worldwide. Every result links back to the library that holds it. No account is needed.
Results 1 to 20 of 20 for “"Glaze Layer"”
-
Tribology and glaze layer formation of Stellite 6 composite coatings produced by thermal spray
Cette recherche se concentre sur l'amélioration de l'usure à haute température par l'évaluation de quatre revêtements composites à matrice métallique de Stellite 6 produits par projection thermique HVOF (high-velocity oxygen-fuel) : 1) Un revêtement métallique sans carbure ; 2) Un revêtement …
-
Wear Rate and Mechanism Maps for Stainless Steel at High Temperature
… that a compacted and sintered wear protective layer, namely “glaze layer” can be formed in many Co, Ni and Fe alloys under certain circumstances, and it is possible to take advantage of glaze layer formation to reduce friction and wear at high temperature. The dissertation is aimed for better …
-
Troisième corps à l'interface céramique métal sous chargement de fretting usure à hautes températures
… observés sont associés à la formation d’une glaze layer. La glaze layer est un troisième corps formé à partir des débris d’usure qui apparaît dans des contacts frottant à haute température. Traditionnellement observée pour des contacts métal/métal, sa formation pour un contact métal/céramique …
-
Etude en fretting usure sous hautes températures d'un contact Waspaloy/René125 : formation et stabilité des "glaze layers"
… de 400°C, l’interface génère la formation d’une glaze layer lubrifiante qui réduit considérablement la cinétique de l’usure. En fixant la température à 700°C (température de l’application industrielle), nous avons étudié la stabilité de ces couches protectrices vis-à-vis de la pression de …
-
Wear and Erosion Behaviours of FeCoCrNi-based Medium- and High-Entropy Alloys
… and Cr. FeCoNi rapidly developed a Co3O4-based glaze layer that improved wear resistance at moderate temperatures but failed at 1000 °C due to layer deformation. The development of a Cr2O3-rich glaze layer was delayed in CoCrNi, but the layer remained resistant to wear at 1000 °C. Alloying both …
-
Formalisation des mécanismes de tribo-oxydation d'un alliage de cobalt soumis à des sollicitations de fretting-usure : effet de la température
… tribocouche. La tribocouche, également appelée glaze layer, possède une structure multi-couches, où les propriétés d’oxydation et de diffusion des éléments d’alliage jouent un rôle prépondérant dans les modalités de sa formation. À la lumière de ces résultats, sont finalement discutés les …
-
An Investigation of Molybdenum Disulphide Dry Film Lubricant Coatings used in Aero-Engine Fan Disc Applications
… retained in the contact, a durable, low friction glaze layer was observed to form on the surface. This layer occurred as a consequence of compaction and sintering of wear debris, generated during the initial interaction between the two surfaces. With time, this layer was observed to lose …
-
Development and Tribological Performance of Thermally Sprayed Coatings Inspired by Glaze Layers
Ceramic coatings inspired by the glaze layers naturally formed on Co-Cr-W superalloys (e.g., Haynes 25) were developed to meet the demands of next-generation gas turbine engines operating at elevated temperatures. Four distinct chemical compositions were investigated: CoO, CoO-21Cr₂O₃, CoO-42Cr₂O₃, …
-
Mechanisms of Nickel-Based Coatings for Fretting Wear Mitigation of Ti6Al4V Interfaces
… due to the formation of what is often called a Glaze oxide layer. The current state of literature describes the composition of the glaze layer as NiO. The focus of this dissertation was to provide experimentation and analysis of temperature effects on the lubricious tribofilm formation that …
-
Effect of surface finish on wear of ceramics
… treatment (polished, machined, polished, then glazed, and machined, then glazed). Ceramics were subjected to 200,000 cycles against Vita Mark II using the two-body pin-on-plate linear wear tester under dead weight a load of 1 Newton. The wear performance of ceramic was determined using volume …
-
Toothbrush Resistance Of Resin-Based Stain And Glaze Materials Applied To 3D-Printed Denture Resins
… resin, after which surface stain and glaze coatings are applied to reproduce gingival coloration, enhance the esthetic appearance and improve clinical longevity of characterized prostheses. However, daily oral hygiene procedures such as toothbrushing degrade surface coatings, leading …
-
The application of non-invasive analytical techniques for the investigation of vitreous materials in museum collections
… are objects such as glass, enamel, and ceramic glazes, with differences in the manufacture, structure, composition and use. This study focuses on forty-four Limoges enamel objects including plaques, bowls and tazzas, and thirty-seven Egyptian faience figurine and scarab objects. Limoges enamels …
-
Efeito de diferentes regimes de acabamento e polimento na resistência à flexão e topografia superficial de zircônias monolíticas
… + diamond polishers, PG- grinding with burs + glaze) and "Degradation" - 2 levels (WithD: autoclave at 127 ° C, 1,7 bar / 24h, without degradation). The miniflexion resistance test (3 points) was performed, with v: 1mm / min and 500N and 5000N load cells. Two samples from each group were …
-
An evaluation of the colours of base metal alloy oxide layers, and its effects on the shade of base metal alloy metal-ceramic restorations
… different metalceramic base metal alloy oxide layers, and the effects of each oxide layer on the shade of the porcelain applied to its surface. The increase in the cost of gold alloys in the dental industry has influenced manufacturers to provide alloys which are cost effective and have …
-
Studies of the high temperature tribological behaviour of some superalloys
… certain wearing conditions compacted debris layers known as 'glaze' layers which are highly resistant to further wear are formed. The principal aim of this project was to understand the mechanisms of such layer/glaze formation particularly during sliding of unlike materials against unlike …
-
Μελέτη της βυζαντινής κυπριακής εφυαλωμένης κεραμικής: διερεύνηση της τεχνολογίας κατασκευής και της προέλευσης με φυσικοχημικές μεθόδους
… present PhD thesis, samples of Cypriot Byzantine glazed ceramics and tripod stilts were studied by means of micro X-Ray Fluorescence Spectrometry (μ-XRF), Powder X-Ray Diffraction (PXRD), Scanning Electron Microscopy with Energy Dispersion Spectrometry (SEM - EDS) and Atomic Emission Spectroscopy …
-
The effect of full-contour Y-TZP ceramic surface roughness on the wear of bovine enamel and synthetic hydroxyapatite : an in-vitro study
… procedure: G1-as-machined (n = 8), G2- glazed (n = 16), G3-diamond bur-finishing (Brasseler, USA) (n = 8) and G4- G3+OptraFine polishing kit (Ivoclar-Vivadent) (n = 16). Thirty-two sintered HA disks (diameter = 11 mm × 2.9 mm in height) and 16 bovine enamel samples with a minimum surface …
-
Investigation of Glaze Formation in Reciprocating Wear of Superalloys
… avoid metal-to-metal contact is to have an oxide layer on the surface. As sliding begins, the transient oxide layers on the surface break down due to adhesive wear. This exposes fresh metal, which then oxidises, generating wear debris in the contact area and resulting in abrasive wear. These …
-
Brake performance and emission behaviors of brake materials on a sub-scale dynamometer
… processes are high enough to form a thick glaze layer on the surfaces. The glaze layers were correlated to a lubricating effect, or fade effect, at disc temperatures above 400 °C, especially when their extension covered the steel fibers. The cermet-coated disc displayed the same fade …
-
Etude expérimentale du comportement sous chargement de fretting simple à haute température de superalliages à base nickel MC2 et CMSX-4. : Application aux aubes de turbine pour moteur d'hélicoptère
Ce travail porte sur l'étude du comportement sous sollicitation de fretting sirnple à haute température de superalliages monocristallins à base de nickel MC2 et CMSX-4. Il trouve son application dans le domaine aéronautique, plus précisément au niveau de la turbine haute pression des moteurs …