Global ETD Search

Search theses and dissertations gathered from participating repositories worldwide. Every result links back to the library that holds it. No account is needed.

Results

Showing 1 to 20 of 39 for “"Hatch Spacing"”.

  1. Microstructural and Mechanical Integrity of 3D Printed 316L Stainless Steel

    … a higher laser power in combination with large hatch spacing, or a combination of low power with a small hatch spacing is going to yield a better microstructure. The scan speed is the most sensitive parameter of the three individual parameters even though how sensitive the scan speed depends on …

    york Repository record for Microstructural and Mechanical Integrity of 3D Printed 316L Stainless Steel (opens in a new tab)

  2. 3-D Printing, Characterizing and Evaluating the Mechanical Properties of 316L Stainless Steel Materials with Gradient Microstructure

    … created by tailoring the processing parameters (hatch spacing, scanning speed, and laser power and scanning speed) of the Selective Laser Melting (SLM). The Materials with Graded Microstructure (MGMs) are characterized by optical and scanning electron microscopy (SEM). Image processing framework …

    vt Repository record for 3-D Printing, Characterizing and Evaluating the Mechanical Properties of 316L Stainless Steel Materials with Gradient Microstructure (opens in a new tab)

  3. Characterization of high deposition rate wire arc directed energy deposition of 316L stainless steel for pressure boundary components

    … models to make predictions of dendrite spacing and growth morphology showing good agreement with experimental measurements. Further work was undertaken to understand the role of hatch spacing on lack of fusion porosity in WA-DED builds. By increasing the ratio of hatch spacing to weld …

    colo-mines Repository record for Characterization of high deposition rate wire arc directed energy deposition of 316L stainless steel for pressure boundary components (opens in a new tab)

  4. Laser Powder Bed Fusion of H13 Tool Steel: Experiments, Process Optimization and Microstructural Characterization

    … range of 500-1000 mm/s. layer thickness (l) and hatch spacing (h) were kept constant. Volumetric energy density (γ) was calculated using the above process parameters. In order to find a relation between the recorded density and top surface roughness with changing process parameters, set of …

    unt Repository record for Laser Powder Bed Fusion of H13 Tool Steel: Experiments, Process Optimization and Microstructural Characterization (opens in a new tab)

  5. Parameter optimization for curl distortion in building parts using 3-D laser stereolithography

    … study were layer thickness, border overcure, hatch overcure, fill cure depth, fill spacing, and hatch spacing. The material used to build the part was Ciba-Geigy Resin SL 5170 and the apparatus was a 3D Systems Corporation SLA-250 rapid prototyping system. Experimental measurements confirm …

    njit Repository record for Parameter optimization for curl distortion in building parts using 3-D laser stereolithography (opens in a new tab)

  6. High Cycle Fatigue of Additively Manufactured Inconel 625

    … the influence of variations in laser scan speed, hatch spacing, and L-PBF machine system. Visual and SEM inspection of fractures was carried out to understand the nucleation mechanisms behind failure of these specimens. Finally, roughness tests were used to measure average roughness of specimens …

    gatech Repository record for High Cycle Fatigue of Additively Manufactured Inconel 625 (opens in a new tab)

  7. Viability and Reproducibility of Additively Manufactured Shape Memory Alloys and High Temperature Shape Memory Alloys

    … cases, the specimens fabricated with a shorter hatch spacing exhibited higher transformation temperatures, lower actuation strain, and lower irrecoverable strain compared to the specimens fabricated with wider hatch spacing. The actuation strain of the L-PBF samples was lower than that of …

    tamu Repository record for Viability and Reproducibility of Additively Manufactured Shape Memory Alloys and High Temperature Shape Memory Alloys (opens in a new tab)

  8. A Process Optimization Framework for Direct Energy Deposition: Densification, Microstructure, and Mechanical Properties of an Iron-Chromium Alloy

    … laser power, scan speed, mass flow rate, hatch spacing, and layer height. The framework utilizes single laser scans and geometric criteria to propose a range of process parameters likely to result in high-density parts. The proposed framework is validated by printing Fe-9wt.%Cr as a …

    tamu Repository record for A Process Optimization Framework for Direct Energy Deposition: Densification, Microstructure, and Mechanical Properties of an Iron-Chromium Alloy (opens in a new tab)

  9. Reducing Porosity in LPBF TI-6AL-4V by Parameter Optimization and Low Temperature Hot Isostatic Pressing Cycle

    … at varied levels of laser power, travel speed, hatch spacing, and layer thickness to obtain a variety of initial defect populations. The specimens were then subjected to a hot isostatic pressure (HIP) at 850 °C and 200 MPa to evaluate the low temperature high pressure (LTHP) cycle’s ability to …

    marquette Repository record for Reducing Porosity in LPBF TI-6AL-4V by Parameter Optimization and Low Temperature Hot Isostatic Pressing Cycle (opens in a new tab)

  10. On prediction of residual stresses for additive manufacturing of Ti-6Al-4V

    … laser speed of approximately 800 mm/s, while the hatch spacing has minimal influence. Additional considerations and the experimental characterisation of the martensitic phase, a by-product of the process, are also discussed. The numerical results are validated using the Carlsson-Larsson theory, …

    birmingham Download PDF for On prediction of residual stresses for additive manufacturing of Ti-6Al-4V (opens in a new tab)

  11. Microstructural Development of Inconel 625 Nickel-Based Superalloy as Function of Laser Powder Bed Fusion Parameters

    … 275W, and 350W) while holding a constant 0.12 mm hatch spacing, 0.03 mm layer thickness, and 16-degree scan rotation angle. Archimedes' method and optical image analysis were carried out to determine relative density of the samples. All laser powers evaluated yielded at least one sample with …

    ucf Repository record for Microstructural Development of Inconel 625 Nickel-Based Superalloy as Function of Laser Powder Bed Fusion Parameters (opens in a new tab)

  12. Parametric Optimization and Performance of Additively Manufactured Refractory and Shock Sensitive Alloys

    … by varying the scanning speed, laser power, hatch spacing, layer height, and resulting energy density. Powder was characterized and tested to meet flowability and composition standards required for LPBF. Detailed microstructural characterization was performed on the printed samples using …

    unt Repository record for Parametric Optimization and Performance of Additively Manufactured Refractory and Shock Sensitive Alloys (opens in a new tab)

  13. Characterisation of mechanically alloyed feedstock for laser-powder bed fusion: titanium silicon carbide metal matrix composite

    … parameters including laser power, scan speed and hatch spacing are presented. A new and novel experimental route is discussed. Detailed findings are presented with a robust methodology for producing elemental feedstock in small batch sizes, and process parameter characterisation for in-situ …

    wlv Repository record for Characterisation of mechanically alloyed feedstock for laser-powder bed fusion: titanium silicon carbide metal matrix composite (opens in a new tab) Download file for Characterisation of mechanically alloyed feedstock for laser-powder bed fusion: titanium silicon carbide metal matrix composite (opens in a new tab)

  14. Additive Manufacturing of Tungsten via Selective Laser Melting and Electron Beam Melting

    … on defects within parts. Specifically, hatch spacing, beam current, and beam speed were investigated and shown to all have a significant effect on porosity and geometric accuracy. Second order models were generated to fit the experiential data, representing the response well (R^2 = 99% …

    whiterose Download PDF for Additive Manufacturing of Tungsten via Selective Laser Melting and Electron Beam Melting (opens in a new tab)

  15. Real-Time Thermography for In Operando Additive Manufacturing Defect Mitigation using a Machine Learning Approach

    … steel (316L) investigated the impact of variable hatch spacing and its correlation with lack-of-fusion defects, illustrating the role of insufficient thermal overlap. Overall, this study introduces a low-cost, in-situ thermal monitoring and predictive framework that establishes a connection …

    houston Repository record for Real-Time Thermography for In Operando Additive Manufacturing Defect Mitigation using a Machine Learning Approach (opens in a new tab) Embargoed until 2027-12-01

  16. Additive Manufacturing of Copper-based Alloy by Laser Powder Bed Fusion

    … melt pool dimension, and dendrite arm spacings dimension, determined by optical microscopy, X-ray diffraction and Scanning electron microscope. LPBF, also known as selective laser melting, was carried out for the Cu-10Sn alloy with varying parameters of laser power from 200W to 350W, …

    ucf Repository record for Additive Manufacturing of Copper-based Alloy by Laser Powder Bed Fusion (opens in a new tab)

  17. On the Fabrication of Shape Memory Alloys by Laser Powder Bed Fusion

    … employed to map laser power, scanning speed, and hatch spacing to processing regimes leading to lack of fusion, keyholing, and balling defects. The effects of these processing parameters on the microstructure variation and phase transformation characteristics are systematically investigated. For …

    tamu Repository record for On the Fabrication of Shape Memory Alloys by Laser Powder Bed Fusion (opens in a new tab)

  18. Laser Powder Bed Fusion of Nickel-based Superalloys

    … RS is affected by scan speed, laser power, and hatch spacing, respectively. Third, the optimum set of parameters was used to manufacture and test as-built and shot-peened samples to investigate the fatigue life without costly heat treatment processes. It was found that shot peening resulted in a …

    mcmaster Repository record for Laser Powder Bed Fusion of Nickel-based Superalloys (opens in a new tab)

  19. Powder Bed Fusion of Difficult-to-Print Ni-Based Superalloys: Microstructural Evolution and Cracking Behavior

    … ratio governing crack susceptibility. Reducing hatch spacing or increasing laser power resulted in grain coarsening, with the effect being more pronounced for hatch spacing reduction. Nevertheless, crack density was significantly reduced with decreasing hatch spacing, which is attributed to …

    waterloo Repository record for Powder Bed Fusion of Difficult-to-Print Ni-Based Superalloys: Microstructural Evolution and Cracking Behavior (opens in a new tab)

  20. An investigation of defects in the nickel-based superalloy IN738LC fabricated by laser powder bed fusion

    … single variable method of 3 parameters (hatch spacing, scan speed and laser power) in LPBF is applied to understand how processing parameters influence defect formation. It is found that pores can be eliminated using the parameter optimisation method but cracks cannot. Single-track …

    birmingham Download PDF for An investigation of defects in the nickel-based superalloy IN738LC fabricated by laser powder bed fusion (opens in a new tab)

Page 1 of 2