  1. Hydrogen Embrittlement in Hexagonal Close Packed (HCP) Alloys with Microstructural Hydrogen Traps

    Hydrogen embrittlement (HE) in hexagonal close packed (HCP) alloys, such as titanium and zirconium, is a life-limiting mechanical degradation phenomenon. Current literature attributes HE in these alloys to the formation and cleavage fracture of hydrides formed due to low hydrogen solubility at …

    unsw Repository record for Hydrogen Embrittlement in Hexagonal Close Packed (HCP) Alloys with Microstructural Hydrogen Traps (opens in a new tab)

  2. Barreiras à base de ligas de alumínio para a difusão do hidrogênio nos substratos ferrosos

    The hydrogen barrier performance of aluminium-based coatings (Fe-Al, Al-Zr) deposited on ferritic substrates by high velocity oxy-fuel and magnetron sputtering was studied. Hydrogen interaction at the chemical stability and morphological properties of the aluminium-alloy/ferrous substrate …

    brazil-uerj Repository record for Barreiras à base de ligas de alumínio para a difusão do hidrogênio nos substratos ferrosos (opens in a new tab)

  3. Multiscale Modeling of Hydrogen Embrittlement

    Hydrogen embrittlement is a long-standing issue in materials science and engineering with a multitude of competing hypotheses and theories. Despite advances in experimental and computational capabilities, common understanding of contributing phenomena has not yet been achieved. Hence, a more …

    gatech Repository record for Multiscale Modeling of Hydrogen Embrittlement (opens in a new tab)

  4. Mechanism of failure by hydrogen-induced cracking in pipeline steels

    … of failure: stress corrosion cracking (SCC) and hydrogen-induced cracking (HIC). The SCC has been studied extensively in the literature; however, HIC phenomenon in pipeline steels is less investigated by researchers. Nevertheless, HIC is recognized as the most important damage mode in sour …

    sask Repository record for Mechanism of failure by hydrogen-induced cracking in pipeline steels (opens in a new tab)

  5. Study of hydrogen atom diffusion and distribution at surface defects on existing pipelines for hydrogen transport

    Hydrogen is acknowledged as a critical player in energy transition and pipelines are the most efficient means to transport hydrogen in large volumes across vast distances. Repurposing the existing natural gas pipelines for hydrogen service will be able to accelerate realization of a full-scale …

    calgary Repository record for Study of hydrogen atom diffusion and distribution at surface defects on existing pipelines for hydrogen transport (opens in a new tab)

  6. Influence of Fine-scale Niobium Carbonitride Precipitates on Hydrogen-Induced Cracking of X70 Pipeline Steel

    … microstructure of steel is well known to affect hydrogen-induced cracking (HIC) susceptibility by having certain heterogeneities serving as effective hydrogen trap sites. A consensus on whether or not fine-scale niobium carbide (NbC), nitride (NbN) and carbonitride (Nb(C,N)) precipitates can …

    mcmaster Repository record for Influence of Fine-scale Niobium Carbonitride Precipitates on Hydrogen-Induced Cracking of X70 Pipeline Steel (opens in a new tab)

  7. Characterisation of hydrogen trapping in steel by atom probe tomography

    <p>Hydrogen embrittlement (HE), which results in an unpredictable failure of metals, has been a major limitation in the design of critical components for a wide range of engineering applications, given the near-ubiquitous presence of hydrogen in their service environments. However, the exact …

    oxford Repository record for Characterisation of hydrogen trapping in steel by atom probe tomography (opens in a new tab)

  8. Hydrogen Embrittlement Susceptibility of Ca-Treated Linepipe Steel Skelp

    … identify problematic microstructural features as hydrogen traps in linepipe steel that serve to increase the hydrogen embrittlement susceptibility. A comparison is made between the hydrogen trapping capacity and associated hydrogen embrittlement susceptibility of Ca-treated X60 grade steel skelp …

    mcmaster Repository record for Hydrogen Embrittlement Susceptibility of Ca-Treated Linepipe Steel Skelp (opens in a new tab)

  9. Fatigue and corrosion fatigue crack growth resistance of RQT501 steel.

    … to evaluate the role of these elements, as hydrogen traps, on the resistance to corrosion fatigue crack growth. In order to evaluate these effects, tests have been carried out under freely corroding conditions and applied cathodic polarisation (-9 . SO mV/SCE). Metallographic examination has …

    whiterose Download PDF for Fatigue and corrosion fatigue crack growth resistance of RQT501 steel. (opens in a new tab)

  10. Investigation of hydrogen diffusion and accumulation in X70 pipeline steel

    … and financial losses. Pipeline cracking by hydrogen embrittlement is the main cause of pipeline failure. The main focus of this research was on the effect of grain size and misorientation on hydrogen diffusion and accumulation in X70 pipeline steel. In this investigation, the hydrogen …

    sask Repository record for Investigation of hydrogen diffusion and accumulation in X70 pipeline steel (opens in a new tab)

  11. On mitigation of hydrogen embrittlement and theoretical modeling of hydrogen accelerated fatigue crack growth

    Hydrogen embrittlement and fatigue are two modes of structural materials failure for which mechanistic understanding is still lacking. In addition, it has been found experimentally that concurrent cyclic loading and hydrogen gas exposure can lead to enhanced fatigue crack growth rates. This work …

    uiuc Repository record for On mitigation of hydrogen embrittlement and theoretical modeling of hydrogen accelerated fatigue crack growth (opens in a new tab)

  12. Sulfide stress cracking resistance of API-X100 high strength low alloy steel in H2S environments

    … "A" solution. The NACE TM0177 "A" solution is a hydrogen sulfide (H2S) saturated solution containing 5.0 wt.% sodium chloride (NaC1) and 0.5 wt.% acetic acid (CH3COOH). The aim of this thesis was to study the effect of microstructure, non-metallic inclusions and alloying elements of the X100 on …

    ubc Repository record for Sulfide stress cracking resistance of API-X100 high strength low alloy steel in H2S environments (opens in a new tab) Download PDF for Sulfide stress cracking resistance of API-X100 high strength low alloy steel in H2S environments (opens in a new tab)

  13. Application of hydrogen-as-a-probe to detect early microstructural imperfections in a power plant’s steel

    … and reliability of a novel probing framework, hydrogen-as-a-probe implemented via thermal desorption spectroscopy (TDS), for detecting early small-scale damage. The main objectives include: assessing, through a literature review, the sensitivity limits of state-ofthe-art NDT techniques for …

    aalto Repository record for Application of hydrogen-as-a-probe to detect early microstructural imperfections in a power plant’s steel (opens in a new tab)

  14. Experimental study of hydrogen trapping by carbides in low alloyed steels using Atom Probe Tomography

    Hydrogen embrittlement (HE) of high-strength low-alloy (HSLA) steels is a big problem. Several options are known to prevent/delay the embrittlement of the steels. One option is to trap the hydrogen at or inside the carbides. This could be interpreted as an energetic interaction, as the nano-sized …

    chalmers Repository record for Experimental study of hydrogen trapping by carbides in low alloyed steels using Atom Probe Tomography (opens in a new tab)

  15. Vliv elektrolytického vodíkování na mechanické vlastnosti a lomové chování slitiny EN AW-2618-T6

    Práca sa zaoberá vplyvom elektrolytického vodíkovania na mechanické vlastnosti a lomové správanie hliníkovej zliatiny EN AW 2618-T6. Cieľom práce bolo posúdiť vplyv vodíka a parametrov elektrolytického vodíkovania na degradáciu mechanických vlastností zliatiny a vysvetliť jej správanie z hľadiska …

    brno-tech Repository record for Vliv elektrolytického vodíkování na mechanické vlastnosti a lomové chování slitiny EN AW-2618-T6 (opens in a new tab)