  1. Evaluation and Prediction of Hydrogen Assisted Cracking of Dissimilar Metal Welds

    … work builds upon the previous research regarding hydrogen assisted cracking (HAC) of low alloy steel to nickel-base filler dissimilar metal welds (DMWs). In particular, this work is focused on DMWs commonly experienced in offshore oil and gas production systems in subsea use. The HAC tendency of …

    ohiolink Repository record for Evaluation and Prediction of Hydrogen Assisted Cracking of Dissimilar Metal Welds (opens in a new tab)

  2. Evaluation of the Susceptibility of Duplex Stainless Steel 2205 to Hydrogen Assisted Cracking in REAC System

    … crevice/pitting corrosion and stress corrosion cracking. Given the condition of hydrogen-rich environment, high-pressure process fluid, and service temperature, this type of cracking is most likely a form of hydrogen assisted cracking (HAC). It is highly influenced by phase balance …

    ohiolink Repository record for Evaluation of the Susceptibility of Duplex Stainless Steel 2205 to Hydrogen Assisted Cracking in REAC System (opens in a new tab)

  3. Quantification of the Local Mechanical Behavior in Dissimilar Metal Welds and its Effect on Hydrogen Assisted Cracking

    … is a continuation of previous works related to hydrogen assisted cracking susceptibility testing using the delayed hydrogen cracking test (DHCT). DHCT was developed in house within the welding engineering program to study fusion boundary failure of Alloy 625 filler metal to steel Dissimilar …

    ohiolink Repository record for Quantification of the Local Mechanical Behavior in Dissimilar Metal Welds and its Effect on Hydrogen Assisted Cracking (opens in a new tab)

  4. Effect of microstructure and alloying elements on the resistance of fastener grade steels to hydrogen assisted cracking

    … employed to measure changes in resistance to hydrogen assisted cracking. The testing procedure compared notched tension specimens fractured in air to threshold stress values obtained during hydrogen charging, utilizing a rising step load procedure. Bainitic structures improved resistance by …

    mtu Repository record for Effect of microstructure and alloying elements on the resistance of fastener grade steels to hydrogen assisted cracking (opens in a new tab)

  5. Effect of Microstructure on Hydrogen Assisted Cracking in Dissimilar Welds of Low Alloy Steel Pipes Joined with Nickel Based Filler Metals

    … protection. These failures were attributed to hydrogen assisted cracking (HAC) along brittle carbides that precipitate in the nickel alloy during onshore PWHT. In response to the field failures, the oil and gas industry began using low alloy steel (LAS) or C-Mn steel overlays in place of nickel …

    ohiolink Repository record for Effect of Microstructure on Hydrogen Assisted Cracking in Dissimilar Welds of Low Alloy Steel Pipes Joined with Nickel Based Filler Metals (opens in a new tab)

  6. Study of Structure, Hydrogen Diffusion and Trapping, Plasticity and Fracture towards the Comprehension of Hydrogen-Assisted Cracking of High-Strength Low-Alloy Martensitic Steels

    … une résistance suffisante au sulfide stress cracking (SSC) motive cette recherche vers une meilleure compréhension de la fragilisation par l'hydrogène des aciers martensitiques revenus faiblement alliés. La caractérisation structurale est réalisée par de multiples techniques,notamment le …

    star-france Repository record for Study of Structure, Hydrogen Diffusion and Trapping, Plasticity and Fracture towards the Comprehension of Hydrogen-Assisted Cracking of High-Strength Low-Alloy Martensitic Steels (opens in a new tab)

  7. Hydrogen embrittlement of L-PBF 316L stainless steel

    Hydrogen embrittlement poses a major challenge for the application of metallic materials in hydrogen-related environments. Although 316L austenitic stainless steel is generally considered hydrogen resistant, laser powder bed fusion (L-PBF) additive manufacturing introduces a complex microstructure …

    soton Repository record for Hydrogen embrittlement of L-PBF 316L stainless steel (opens in a new tab)

  8. Use of implant testing to evaluate the susceptibility of HY-130 steel weldments to hydrogen embrittlement.

    The cracking that may occur near the fusion zone of a steel weldment can often be attributed to the embrittlement of the microstructure by hydrogen induced during the welding process. The modified implant test was used in this case to evaluate the hydrogen-assisted cracking susceptibility of three …

    nps Repository record for Use of implant testing to evaluate the susceptibility of HY-130 steel weldments to hydrogen embrittlement. (opens in a new tab)

  9. Feasibility of underwater friction stir welding of HY-80 steel

    … temper low carbon steels that are susceptible to hydrogen-assisted cracking (HAC). The specific benefits of underwater FSW would be weld repairs of ship and submarine control surfaces and hulls without the need for drydocking and extensive environmental control procedures. A single tool of …

    nps Repository record for Feasibility of underwater friction stir welding of HY-80 steel (opens in a new tab)

  10. Stress corrosion cracking and hydrogen embrittlement of thick section high strength low alloy steel.

    … ship structural applications. Stress corrosion CRACKING(SCC) and hydrogen embrittlement(HEM) were investigated by conducting 42 Wedge-Opening load(WOL) tests as a function of stress intensity and corrosion potential and 33 Slow Strain Rate(SSR) tests as a function of strain rate and corrosion …

    nps Repository record for Stress corrosion cracking and hydrogen embrittlement of thick section high strength low alloy steel. (opens in a new tab)

  11. Feasibility of underwater friction stir welding of hardenable alloy steel

    … in order to assess the potential for inducing hydrogen assisted cracking (HAC) during FSW of susceptible alloys. All traverses were visually defect-free. The FSW nuggets (stir zone) exhibited refined microstructures and increased hardness relative to the base plate. Based on preliminary …

    nps Repository record for Feasibility of underwater friction stir welding of hardenable alloy steel (opens in a new tab)

  12. Hydrogen Assisted Crack in Dissimilar Metal Welds for Subsea Service under Cathodic Protection

    … at the weld fusion boundary region. This type of cracking is known as hydrogen assisted cracking (HAC) and it is influenced by base/filler metal combination, and welding and PWHT procedures.DMWs of two material combinations (8630 steel – Alloy 625 and F22 steel – Alloy 625), produced with two …

    ohiolink Repository record for Hydrogen Assisted Crack in Dissimilar Metal Welds for Subsea Service under Cathodic Protection (opens in a new tab)

  13. Phase Transformation Behavior and Hydrogen Cracking Susceptibility in Grade T23 and T24 Steel Welds

    Cracking in water walls of newly built fossil power plants using Grade T23 and T24 steels has halted service. The cause for this cracking is still undetermined, and one possible mechanism is hydrogen assisted cracking (HAC). The goal of this research was to compare the susceptibility to HAC in …

    ohiolink Repository record for Phase Transformation Behavior and Hydrogen Cracking Susceptibility in Grade T23 and T24 Steel Welds (opens in a new tab)

  14. Evaluation of Friction Stir Processing of HY-80 Steel Under Wet and Dry Conditions

    … tempered condition and is highly susceptible to hydrogen assisted cracking associated with conventional fusion welding. FSW/P (400 RPM/ 2 IPM) was conducted using a polycrystalline cubic boron nitride tool having a pin length of 6.35 mm. Two sets of processing runs were completed on HY-80 plates, …

    nps Repository record for Evaluation of Friction Stir Processing of HY-80 Steel Under Wet and Dry Conditions (opens in a new tab)

  15. Near Field Electrospinning of Nanofibers for Multi-Modal Hydrogen Sensing

    Hydrogen gas is a common byproduct in industrial processes. It is also frequently used in practical applications such as fuel cell vehicles. It has no smell and no taste, but it may pose immediate safety risks because it is combustible in air. It is also un wanted in manufacturing processes as it …

    calgary Repository record for Near Field Electrospinning of Nanofibers for Multi-Modal Hydrogen Sensing (opens in a new tab)

  16. Illuminating The Chemo-Mechanics Of Environment Assisted Fatigue In Aluminum

    … atomistic-scale mechanisms governing environment assisted fatigue crack growth in aluminum. All studies focus on the application of concurrent atomistic-continuum multiscale modeling, utilizing the coupled atomistic and discrete dislocation (CADD) methodology. First, an ab-initio prediction of …

    cornell Repository record for Illuminating The Chemo-Mechanics Of Environment Assisted Fatigue In Aluminum (opens in a new tab)

  17. Permeation and Thermal Desorption Studies of Deuterium Diffusion and Trapping in Ion-Implanted Nickel

    <p>The interaction between hydrogen isotopes and irradiation defects in nickel is studied using Gas-phase Permeation and Thermal Desorption Analysis techniques. The work was motivated by the need for the understanding and control of tritium diffusion and trapping in structural materials of the …

    mcmaster Repository record for Permeation and Thermal Desorption Studies of Deuterium Diffusion and Trapping in Ion-Implanted Nickel (opens in a new tab)

  18. Investigation of hydrogen induced cracking susceptibility of API 5L X65 pipeline steels

    … mechanisms such as corrosion, embrittlement and cracking. The hydrogen induced cracking (HIC) phenomenon often affects pipelines exposed to sour and acidic environments. It involves the ingress of hydrogen atoms into the steel, which leads to the degradation of its mechanical properties such as, …

    sask Repository record for Investigation of hydrogen induced cracking susceptibility of API 5L X65 pipeline steels (opens in a new tab)