Global ETD Search
Search theses and dissertations gathered from participating repositories worldwide. Every result links back to the library that holds it. No account is needed.
Results 1 to 20 of 25 for “"IGSCC"”
-
Inhibition of Corrosion and Stress Corrosion Cracking of Sensitized AA5083
… and intergranular stress corrosion cracking (IGSCC). This is due to a highly anodic ß phase (Mg2Al3) relative to the matrix that forms along the grain boundary and decreases corrosion resistance of 5XXX aluminum alloys. The purpose of this study is to develop the proper method to test …
-
Effects of stress on intergranular corrosion and intergranular stress corrosion cracking in AA2024-T3
… and intergranular stress corrosion cracking (IGSCC), which seriously limits the lifetime as engineering materials. Conventional investigation methods constrained a single crack per specimen can not characterize and evaluate multiple IGC cracks exist in real structures. In this study, a number …
-
The Effect of Laser Shock Peening on Dislocation Morphology and Microstructural Evolution of AA5083-H116
… for intergranular stress corrosion cracking (IGSCC) in AA5083-H116 significantly increases under thermal exposure. The effects of laser-shock peening (LSP) on the kinetics of β-phase were studied via accelerated sensitization heat treatments between 70-175℃ for times between 5-3,600 hours. …
-
Experimental validation of intergranular stress corrosion cracking predictive models
<p>Intergranular Stress Corrosion Cracking (IGSCC) has been one of the most important challenges to nuclear power plant operation worldwide. The degradation of alloy 600 (Ni-based alloy) and its susceptibility to Stress Corrosion Cracking (SCC) when exposed to primary water environment in …
-
A Study of the Effects of Mechanical Surface Treatments on Residual Stresses, Microstructure and Stress Corrosion Cracking Behavior of Alloy 600
… Localized corrosion and intergranular SCC (IGSCC) have been observed in Alloy 600 in the high temperature (288-340 °C) pure water environment of LWRs. Additionally, IGSCC of Alloy 600 has been reported even at room temperature under certain conditions in thiosulfate and tetrathionate …
-
Experimental and modeling studies of formation of self-organized porous anodic oxide layers and intergranular corrosion of steel
… intergranular stress corrosion cracking (IGSCC) on high strength X70 pipeline steels was studied. In high-pH solution (pH 8 - 10.5), pipeline steels are susceptible to both intergranular cracking (IGC) and IGSCC in the same active-passive potential range, suggesting that IGC leads to …
-
Nonlinear ultrasonic measurement on cold rolled and sensitized 304 austenitic stainless steel
… to intergranular stress corrosion cracking (IGSCC). Sensitization preferably tends to occur in the heat affected zone (HAZ) of welds where heat is induced for a certain amount of time during welding. IGSCC is a main cause of the cracking in boiling water reactor piping systems and therefore …
-
TEM crack tip investigations of SCC
… of intergranular stress corrosion cracking (IGSCC) has been investigated in Alloy 600 subjected to constant load and slow strain rate tests in simulated primary circuit pressurized water reactor conditions. Cracks were observed to nucleate at high-angle grain boundaries and propagate to …
-
Stress corrosion crack detection in alloy 600 in high temperature caustic.
… Intergranular stress corrosion cracking (IGSCC) attacks the tubes in areas of high residual stress, and in crevice regions. No method has been successfully developed to monitor steam generator tubing in-situ for crack initiation and growth. Essentially all available published IGSCC crack …
-
Measurements of acoustic nonlinearity in cold-rolled and heat-treated 304 austenitic stainless steel using nonleaner ultrasound
… to intergranular stress corrosion cracking (IGSCC). The heat affected zone (HAZ) of weld in 304 SS structures is usually the most probable locations for sensitization. The IGSCC is of great interest because most cracking in high temperature pipes, such as water reactor pipes, initiates in HAZ …
-
The Effect of Sensitization on the Stress Corrosion Cracking of Aluminum Alloy 5456
… to intergranular stress corrosion cracking (IGSCC). Aluminum alloy 5456-H116 (also identified as Al-Mg5.1) samples were sensitized at 175C for varying durations of time and then mechanically tested in salt water. Mass loss tests quantified the degree of sensitization (DOS) as a function of …
-
Oxidation kinetics of 316l stainless steel in the pressurised water reactor environment
… of intergranular stress corrosion cracking (IGSCC) in the primary water environment has been observed within the same temperature range, it is proposed that the above explanation, observed in the absence of applied stress, extends to explain the behaviour of IGSCC kinetics in austenitic …
-
Micromechanical testing of oxidized grain boundaries
… de France (EDF) to build a predictive model for IGSCC based on localized/microscopic information, one of the main objectives was the extraction of the stress at failure of individual oxidized GBs. Supported by finite element simulations, microcantilever fracture tests revealed that surface oxides …
-
The Effect of Sensitization on Corrosion Fatigue and Threshold Stress Intensity of AA5083-H131 Used for Marine Applications
… and intergranular stress corrosion cracking (IGSCC) due to the formation of the active Al3Mg2-ß phase on grain boundaries. ß phase is metallurgically undesirable and forms on grain boundaries when slightly elevated in-service temperatures are experienced for prolonged periods of time, a …
-
Micromechanics of stress corrosion cracking in 304 stainless steel and Ni Alloy 600
… the intergranular stress corrosion cracking (IGSCC) by applying a relatively new micro-mechanical technique to look at the crack growth rate of individual grain boundaries in 304 stainless steel (SS) and to measure fracture toughness for different grain boundaries in Ni Alloy 600. In addition, …
-
Studies of Microscopic Scale Strains in Nickel Alloys Resulting from Mechanical and Chemical Forces
… in the stress axis direction. Intergranular SCC (IGSCC) was observed in Alloy 600 C-ring specimens electrochemically corroded in a high temperature caustic solution. Tensile strains with respect to the stress axis and plastic strain could be identified in regions ahead of the crack tip. These …
-
Influence of heat treatment condition on the stress corrosion cracking properties of low pressure turbine blade steel FV520B
… intergranular stress corrosion cracking (IGSCC) as the dominant cracking mechanism.
-
Comportement en corrosion et en corrosion sous contrainte en milieu primaire REP d'un acier inoxydable 316L élaboré par fabrication additive WAAM et WLAM
… la résistance à la fissuration intergranulaire (IGSCC) des matériaux WAAM et WLAM lors d'essais à déplacement imposé (U-bends). Parallèlement, des essais de traction lente ont permis d'étudier les premiers stades de l'amorçage des fissures de CSC. Des amorces de fissures intergranulaires ont été …
-
Study of 316L Stainless Steel Passivation under PWR Primary Water by Electrochemical Noise Analysis
… à la corrosion sous contrainte intergranulaire (IGSCC). Toutefois, peu de méthodes existent pour un suivi in situ de l'oxydation ou la détection précoce de l'apparition de fissures. La technique du bruit électrochimique pourrait répondre à cette ambition. Dans ce contexte, cette thèse s'intéresse …
Page 1 of 2