Global ETD Search
Search theses and dissertations gathered from participating repositories worldwide. Every result links back to the library that holds it. No account is needed.
Results 1 to 15 of 15 for “"Intergranular oxidation"”
-
Preferential Intergranular Oxidation and Stress Corrosion Cracking of Alloy X-750 in CO-CO2 Gas Mixtures
… pressure tubes that house fuel bundles. Brittle intergranular fracture was observed on Alloy X-750 ex-service spacers, instigating materials research to identify the responsible mechanisms. Alloy X-750 is a precipitation-hardened variant of Alloy 600 (72Ni-16Cr-9Fe) with the addition of Al and …
-
Ultrasonic nondestructive evaluation techniques and the effects of fiber architecture on mechanical performance in multi-directionally reinforced textile composites
… effect of modifying surface residual stresses on intergranular oxidation and cracking was examined using constant strain C-ring tests;The mechanism for high temperature intergranular fracture in alloy 908 is stress assisted intergranular oxidation cracking. A direct correlation between percent …
-
OXIDATION STUDIES ON Ag-In AND Ni-BASED ALLOYS AT LOW HOMOLOGOUS TEMPERATURE
Internal and intergranular oxidation can result in embrittlement, degradation of mechanical properties and possible premature mechanical failure or stress corrosion cracking. Internal oxidation of Ag-In alloys was studied in an air atmosphere at a relatively low homologous temperature (240 °C) (∼ …
-
Stress Corrosion Cracking of Ni-Fe-Cr Alloys Relevant to Nuclear Power Plants
… 82 dissimilar metal welds using the internal oxidation model as a guide. Initial experiments were carried out in a 480 °C hydrogenated steam environment considered to simulate high temperature reducing primary water. Ni alloys underwent classical internal oxidation intragranularly resulting in …
-
A study of internal oxidation in carburising steels
<p>The phenomena known as `internal oxidation' can play a major detrimental role in the failure of carburised components such as bearings and gears. Internal oxidation leads to a degradation of the surface layer often leading to surface break up and fatigue. This work is concerned with a detailed …
-
Oxidation kinetics of 316l stainless steel in the pressurised water reactor environment
… reactor (PWR). It is generally accepted that intergranular oxidation at the surface of a metal forms a preferential site for stress corrosion crack (SCC) initiation; therefore the kinetics of both surface and intergranular oxidation were measured. The influence of temperature, within the range …
-
Understanding the Effect of Oxygen on the Degradation of 316L in Liquid Sodium
… present at all oxygen levels with increased intergranular oxidation observed at higher concentrations. Carbides transitioned from Cr23C6 under purified conditions to (Fe, Mo)6C at intermediate oxygen concentration. Redeposited ferrite particles were observed to increase in size with increased …
-
Phase-field study of diffusion controlled phenomena: reorientation of zirconium hydrides and oxidation of metals
… zirconium hydrides in nuclear fuel claddings and oxidation induced stresses in steels, which are among two critical problems in materials used in water-cooled nuclear reactors. For this purpose, we developed micro-scale computational frameworks based on the phase-field method.We investigated the …
-
Induction hardening response of a carburized 4121 steel
… transformation products near surface intergranular oxidation. Mechanical property characterization techniques include post-heat treatment dimensional analysis of the fatigue specimens, radial hardness profiles, carbon gradient analysis, torsional fatigue testing, and residual stress vs …
-
Towards highly fatigue resistant additively manufactured metals
… and 0.1 Hz loading, all materials exhibited intergranular oxidation crack growth. However, compared to wrought and HIP LPBF materials, the highly elongated S+DA LPBF grain structure nearly halted crack growth perpendicular to the build direction and gave much higher fatigue resistance for …
-
Understanding the mechanisms controlling stress corrosion cracking through high-resolution characterization
… <p>Several SCC precursors have been identified: intergranular oxidation zone (IOZ) ahead of the crack tip, Cr-Fe depletion ahead of the IOZ, grain boundary migration along the crack and ahead of the crack tip, and localized deformation around the crack tip. The first objective of this thesis was …
-
Effect of molybdenum on niobium, titanium carbonitride precipitate evolution and grain refinement in high-temperature vacuum carburizing alloys, The
… vacuum carburizing due to the suppression of intergranular oxidation. To provide resistance to undesired grain coarsening at these elevated temperatures and associated reduction in fatigue performance, microalloyed steel variants have been developed which employ fine Ti- and Nb-carbonitrides …
-
Oxydation et corrosion à haute température de superalliages à base de nickel issus de la fabrication additive
La résistance à l’oxydation isotherme et cyclique de l’alliage 718 produit par le procédé de fusion sélective par faisceau laser (LBM) et par faisceau d’électrons (EBM) a été comparée à celle de l’alliage 718 forgé (AMS5662). Les essais d’oxydation isotherme à 850 °C sous air ont montré des tenues …
-
Oxydation intergranulaire des superalliages à base de nickel et de l'acier inoxydable austénitique 316L
L'oxydation intergranulaire est un phénomène de dégradation observé dans les alliages polycristallins exposés à des environnements oxydants, où les joints de grains agissent comme des chemins de diffusion rapide et subissent une oxydation préférentielle. Cela peut entraîner une diminution des …
-
Modélisation de l'amorçage de la corrosion sous contrainte dans les alliages base nickel 182 et 82 en milieu primaire des réacteurs à eau sous pression
Les métaux déposés base nickel sont utilisés pour assembler des composants du circuit primaire des centrales nucléaires à Réacteurs à Eau sous Pression (REP). Un nombre croissant de cas de fissuration par Corrosion Sous Contrainte (CSC) des soudures en alliages base nickel 182 et 82 est rapporté …