An experimental measuring instrument for internal stress in contrete
Thesis (M.S.)--Michigan State College of Agriculture and Applied Science. Dept. of Civil Engineering, 1950
-
Thermal Expansion, Internal Stress, and Strength of Glass-Crystal Composites
Made available in DSpace on 2014-12-10T17:32:38Z (GMT). No. of bitstreams: 1 6915410.pdf: 3084944 bytes, checksum: b7bc29b46702c51d414feb4a93759bc3 (MD5) Previous issue date: 1969
-
The role of internal stress in strengthening heavily codeformed two-phase materials
… properties. This thesis examines the role of internal stresses on the strengthening of heavily codeformed two-phase materials. The magnitude of these stresses and the effects of annealing on them are studied in various types of copper-niobium composites: bundle drawn and in-situ drawn wire …
-
Modeling Slip Gradients and Internal Stresses in Crystalline Microstructures with Distributed Defects
… effects in the presence of heterogeneities and internal stresses in continuum crystal plasticity. A three-dimensional constitutive theory accounting for length-scale dependent internal residual stresses is developed. The resulting internal stress is discussed in terms of the long-range …
-
Multilayer graphene-based capacitive micromachined ultrasonic transducer design, manufacturing, and characterization
… silicon-based MEMS due to relatively high internal stress and thickness. Chemical vapor deposition (CVD)-grown, multi-layer graphene (MLG) is a promising alternative to silicon because it can be made very thin and has low internal stress, which results in higher compliance membranes. Before …
-
Microcreep of molybdenum crystals
… a very sensitive capacitance extensometer. Flow stress was measured on an Instron machine. Microcreep of the crystals was studied at stresses below half the macroscopic flow stress in the temperature range 200° to 300°K. at resolved shear strains of below 5%. The creep following addition of a …
-
The Influence of Interfaces on Dislocation Mobility
… method was developed to calculate the passing stress of pile-ups in a general internal stress field. This method was used to calculate the passing stress for a pile-up of like edge dislocations for a sinusoidal internal stress field, a simple tilt wall, and a Van der Merwe net of misfit …
-
Investigating the Relation Between Stress and Marital Satisfaction: The Interaction Effects of Dyadic Coping and Communication
… and coping skills play in the relation between stress and marital satisfaction in a community sample of 119 married, heterosexual couples in Italy. Hierarchical regression models were used to test for communication or coping skills as a moderator of the relation between an external or internal …
-
A new vibrational technique for measurement of stress variations in thin films
… physical deposition, etc.) shows that internal stress is a common problem, particularly in industrial applications. The presence of stress influences the properties of the film and when severe may cause the film to buckle or crack. There is a significant technological and industrial …
-
Experimental Assessment and Implementation of Photoelastic Tomography
… is a destructive and time-consuming experimental stress analysis technique that assesses internal stress by the construction of a stress frozen polymeric prototype that is sliced and analysed section by section by 2-D photoelasticity. Non-destructive 3-D internal stress reconstruction, such as …
-
Structure, Mechanical and Tribological Properties of Hydrogen-free Amorphous Carbon Films Deposited by Dual-Frequency Mode Pulsed-DC Magnetron Sputtering
… (to increase the deposition rate and reduce the internal stress) on the mechanical and tribological properties obtained in non-hydrogenated a-C films by such deposition techniques. Four a-C films were deposited at different substrate negative bias voltages (50 V - 170 V), which have a …
-
Fatigue Behavior of Hardened Fe-.3C-4Ni-1Al Medium Carbon Alloy Steel
… fatigue tests, and x-ray line broadening and stress relaxation measurements. The three different heat treatments produced the following structures: (I) a conventional quenched and tempered microstructure with a high density of dislocations and elongated carbides, (II) a microstructure) of high …
-
Cooperative Manipulation Strategies for Multi-Robot Collaboration
… approach, I will focus on the concept of applied internal stress, on the jointly manipulated object, and how internal stress can be leveraged as a compensation mechanism for disturbance on a cooperative manipulation setup. I will present an impedance-based strategy that is used to determine how …
-
Effect of minor phase additions on the microstructure and dielectric properties of barium titanate ceramics
… samples were accompanied by an increase in the internal stress level with decreasing grain size and increasing concentration of core-shell grains. The core-shell grains are comprised of a core of unmodified BaTiO$\sb3$ and a shell of Zr modified BaTiO$\sb3$, Ba(Zr$\sb{\rm x}$Ti$\sb{\rm …
-
Characterization of a lithium niobate piezoelectric transformer
… for such beam loads. PT characteristics such as internal stress, electric field, and electric potential can provide insight into the optimal operating conditions for a given application. Measurement of internal stress can be used to ensure that the single-crystal lithium niobate (LiNbO3) PT does …
-
Produção e caracterização de recobrimentos de carbono-flúor via técnica rf-PECVD a partir do gás tetrafluoretano
… 10 – 40 GPa elastic modulus, 0,55 GPa mean internal stress and 0,35 ± 0,11 dynamic friction coefficient were produced in the cathode electrode. Activated growth model associated with plasma polymerization in continuous mode took part in anode deposition. A plasma polymer, probably the …
-
Control of electrodeposit properties of nickel and nickel alloy by pulse plating.
… The mechanical properties of micro-hardness and internal stress obtained using the EFCO stress-meter and X-ray diffraction were measured as a function of bath composition, on/off cycles,current density, types of plating and solution pH. The structure and composition of alloys deposited have been …